Please wait a minute...
金属学报  2026, Vol. 62 Issue (6): 1059-1068    DOI: 10.11900/0412.1961.2024.00398
  研究论文 本期目录 | 过刊浏览 |
950 ℃下DZ411镍基高温合金NiCoCrAlY涂层热腐蚀行为
邓尕平1, 赵杰1, 高凯1, 王威2, 刘欢2, 曹铁山1, 程从前1()
1 大连理工大学 材料科学与工程学院 大连 116024
2 中国航发沈阳发动机研究所 沈阳 110015
Hot Corrosion Behavior of DZ411 Nickel-Based Superalloy NiCoCrAlY Coating at 950 oC
DENG Gaping1, ZHAO Jie1, GAO Kai1, WANG Wei2, LIU Huan2, CAO Tieshan1, CHENG Congqian1()
1 School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China
2 AECC Shenyang Engine Research Institute, Shenyang 110015, China
引用本文:

邓尕平, 赵杰, 高凯, 王威, 刘欢, 曹铁山, 程从前. 950 ℃下DZ411镍基高温合金NiCoCrAlY涂层热腐蚀行为[J]. 金属学报, 2026, 62(6): 1059-1068.
Gaping DENG, Jie ZHAO, Kai GAO, Wei WANG, Huan LIU, Tieshan CAO, Congqian CHENG. Hot Corrosion Behavior of DZ411 Nickel-Based Superalloy NiCoCrAlY Coating at 950 oC[J]. Acta Metall Sin, 2026, 62(6): 1059-1068.

全文: PDF(2674 KB)   HTML
摘要: 

为了揭示NiCoCrAlY涂层在900 ℃以上熔盐环境中的热腐蚀机制与失效行为,本工作在常规称重研究方法基础上,考虑熔盐挥发对涂盐样品质量的影响,研究了950 ℃下DZ411合金NiCoCrAlY涂层在Na2SO4盐膜及Na2SO4与NaCl组成的混合盐膜中的热腐蚀动力学行为、表/界面组织和成分特征。结果表明,经热盐挥发质量校准后,常规热腐蚀减重动力学曲线显示,试样热腐蚀后质量增加,且混合盐环境下的腐蚀增重速率大于纯硫盐环境;2种盐膜条件下的腐蚀产物层结构类似,外层为Al2O3氧化层,中间层为以Al2O3和Cr2O3为主的疏松氧化物,内层为互扩散区,且在基体界面前沿析出大量Al2S3和Cr2S3。此外,与纯硫盐环境相比,混合盐中的氯盐通过氯化反应促进了S、O元素的扩散,从而加速了涂层的劣化进程。

关键词 : NiCoCrAlY涂层,  DZ411合金,  热腐蚀,  扩散    
Abstract:

NiCoCrAlY coatings offer good resistance to high-temperature oxidation and corrosion, making them an effective protective layer for gas turbine blades. However, in marine environments, these coatings are susceptible to hot corrosion damage, considerably affecting service lifespan and safety. With the development of modern gas turbines with high efficiency and power, the service temperatures of their blades have increased. An in-depth understanding of the hot corrosion mechanisms of NiCoCrAlY coatings above 900 oC is crucial for developing advanced gas turbine blade materials suitable for marine applications. This study investigates the hot corrosion kinetics using conventional gravimetric analysis while considering the quality effect of molten salt volatilization. XRD, SEM, and EDS were used to analyze the surface and interface microstructures, as well as the compositional characteristics of the NiCoCrAlY coating on the DZ411 alloy. These analyses were performed after exposure at 950 oC under a Na2SO4 salt film and a mixed salt film comprising Na2SO4 and NaCl. Results demonstrated that after modifying conventional hot corrosion mass-loss kinetics to consider molten salt volatilization, the hot corrosion mass change becomes a mass gain. The mass gain rate was higher in mixed salt environments than in pure sulfate environments. The hot corrosion mass gain of the alloy is attributed to cyclic oxidation-sulfidation reactions in the coating. Cross-sectional analysis of the corrosion product layer revealed a similar structure under both salt conditions: an outer layer of Al2O3, a middle layer of porous oxides dominated by Al2O3 and Cr2O3, and an inner interdiffusion zone. In addition, Al2S3 and Cr2S3 precipitates were present at the coating-substrate interface. Furthermore, the presence of chloride salt in the mixed salt environment facilitated chlorination reactions, promoting the diffusion of sulfur and oxygen, and accelerating the degradation of the coating compared with the pure sulfate condition.

Key words: NiCoCrAlY coating    DZ411 alloy    hot corrosion    diffusion
收稿日期: 2024-11-21     
ZTFLH:  TG178  
基金资助:船用燃气轮机基础研究项目(MGT2023001)
通讯作者: 程从前,cqcheng@dlut.edu.cn,主要从事高温腐蚀与寿命评价、表面电化学腐蚀检测新技术研究
Corresponding author: CHENG Congqian, professor, Tel: (0411)84709076, E-mail: cqcheng@dlut.edu.cn
作者简介: 邓尕平,男,2000年生,硕士
图1  热腐蚀后无盐及涂盐合金试样片以及涂盐陶瓷片试样的质量变化曲线
图2  热盐挥发校准后DZ411合金NiCoCrAlY涂层的热腐蚀动力学曲线
图3  热腐蚀200 h后试样表面的XRD谱
图4  不同盐膜条件下热腐蚀200 h后试样截面形貌和表面形貌的SEM像
图5  纯硫盐试样横截面形貌的高倍SEM像
PointOAlCrCoNiTiNSWSi
116.2937.5824.27--1.8917.402.57--
22.2850.0911.93---32.373.33--
3--9.26-2.4964.2816.25–3.983.74
表1  图5中各点的EDS结果 (mass fraction / %)
图6  混合盐试样横截面形貌的高倍SEM像
PointOAlCrCoTiNSTaNi
123.76-5.76-19.39--51.09-
226.2728.3527.29---18.39--
3--4.77-72.7219.023.49--
4--20.09-43.0120.9612.693.25-
5-0.686.710.4762.2523.27--6.62
6--41.95-19.8911.4126.75--
7----68.18-22.669.16-
表2  图6中各点的EDS结果 (mass fraction / %)
图7  热腐蚀200 h后纯硫盐和混合盐试样截面的EDS线扫描结果
图8  各腐蚀层厚度和硫化物扩散深度统计
图9  DZ411合金NiCoCrAlY涂层中可能形成腐蚀产物的Gibbs自由能
图10  DZ411合金在950 ℃下的熔盐腐蚀机理图
[1] Tang Q Y, Liu T J, Hu Y, et al. Research status of environmental spectrum acceleration techniques for typical life sensitive parts in engines[J]. Equip. Environ. Eng., 2023, 20(12): 1
[1] 唐庆云, 刘天娇, 胡 毅 等. 发动机典型寿命敏感件环境谱加速技术研究现状[J]. 装备环境工程, 2023, 20(12): 1
[2] Kosieniak E, Biesiada K, Kaczorowski J, et al. Corrosion failures in gas turbine hot components[J]. J. Fail. Anal. Prev., 2012, 12: 330
doi: 10.1007/s11668-012-9571-3
[3] Meisner K J, Opila E J. Hot corrosion of shipboard gas turbine blades[J]. Oxid. Met., 2020, 94: 301
doi: 10.1007/s11085-020-09990-7
[4] Liu D L, Mu R D, Lu F. High temperature oxidation and corrosion property test of NiCoCrAlYTa coating on turbine blade[J]. Equip. Environ. Eng., 2018, 15(11): 54
[4] 刘德林, 牟仁德, 陆 峰. 涡轮叶片NiCoCrAlYTa涂层抗高温氧化和腐蚀性能测试研究[J]. 装备环境工程, 2018, 15(11): 54
[5] Li F G, Yang L, Zhou Y C. Study advances of high temperature coating for aeroengine to resist marine atmospheric corrosion[J]. Therm. Spray Technol., 2019, 11(4): 1
[5] 李发国, 杨 丽, 周益春. 航空发动机高温涂层耐海洋大气腐蚀研究进展[J]. 热喷涂技术, 2019, 11(4): 1
[6] Gong S K, Liu Y, Geng L L, et al. Advances in the regulation and interfacial behavior of coatings/superalloys[J]. Acta Metall. Sin., 2023, 59: 1097
doi: 10.11900/0412.1961.2023.00257
[6] 宫声凯, 刘 原, 耿粒伦 等. 涂层/高温合金界面行为及调控研究进展[J]. 金属学报, 2023, 59: 1097
doi: 10.11900/0412.1961.2023.00257
[7] Lu X Y, Yu D Q, Jiang S M, et al. Hot corrosion behavior of a (NiCoCrAlYSiB + AlSiY) composite coating[J]. Acta Metall. Sin., 2012, 48: 461
doi: 10.3724/SP.J.1037.2012.00031
[7] 卢旭阳, 于大千, 姜肃猛 等. (NiCoCrAlYSiB + AlSiY)复合涂层热腐蚀行为的研究[J]. 金属学报, 2012, 48: 461
doi: 10.3724/SP.J.1037.2012.00031
[8] Yao Q W, Xu B M. Researches on hot corrosion resistance of thermal barrier coating for turbine blade[J]. Turbine Technol., 2014, 56: 237
[8] 姚青文, 徐佰明. 涡轮叶片热障涂层热腐蚀性能研究[J]. 汽轮机技术, 2014, 56: 237
[9] Syamkumar K, Babu N, Govindarajan S, et al. Hot corrosion behaviour of mullite thermal barrier coatings for marine diesel engines[J]. Ceram. Int., 2024, 50: 2808
doi: 10.1016/j.ceramint.2023.11.001
[10] Li X C. Microstructure and hot corrosion performance of laser cladding NiCoCrAlYSi coating modified via high current pulsed electron beam[D]. Nanjing: Jiangsu University, 2022
[10] 李向成. 强流脉冲电子束作用下激光熔覆NiCoCrAlYSi涂层微观结构及热腐蚀性能研究[D]. 南京: 江苏大学, 2022
[11] Qi H Y, Yang J S, Yang X G, et al. Fatigue behavior of uncoated and MCrAlY-coated DS nickel-based superalloys pre-exposed in hot corrosion condition[J]. Rare Met., 2018, 37: 936
doi: 10.1007/s12598-016-0867-4
[12] Wang K, Zou L X, Guo L, et al. High-temperature corrosion and protection of thermal barrier coatings for aeroengines and gas turbines[J]. J. Chin. Soc. Corros. Prot., 2025, 45: 1
[12] 王 昆, 邹兰欣, 郭 磊 等. 航空发动机及燃气轮机热障涂层高温腐蚀与防护[J]. 中国腐蚀与防护学报, 2025, 45: 1
[13] El-Awadi G A, Abdel-Samad S, Elshazly E S. Hot corrosion behavior of Ni based inconel 617 and inconel 738 superalloys[J]. Appl. Surf. Sci., 2016, 378: 224
doi: 10.1016/j.apsusc.2016.03.181
[14] Kumawat M K, Parlikar C, Alam M Z, et al. Type-I hot corrosion of Ni-base superalloy CM247LC in presence of molten Na2SO4 film[J]. Metall. Mater. Trans., 2021, 52A: 378
[15] Yang B S, Li B, Chen X X, et al. Influence of temperature on hot corrosion behavior of GH4169 superalloy subjected to Na2SO4-NaCl salts attack[J]. Mater. Chem. Phys., 2024, 325: 129731
doi: 10.1016/j.matchemphys.2024.129731
[16] Dong R F, Liu D, Zhang T B, et al. Hot-corrosion behavior associated with the evolution of corrosion scales of a Ni-based superalloy in molten salts[J]. Prog. Nat. Sci. Mater. Int., 2021, 31: 486
doi: 10.1016/j.pnsc.2021.04.004
[17] Liu M K, Li Y M, Liu Y, et al. Hot corrosion behaviors test of DSM11 Ni-base superalloy under different temperature[J]. Aeroengine, 2023, 49(2): 168
[17] 刘明坤, 李艳明, 刘 宇 等. 不同温度下DSM11镍基高温合金热腐蚀试验[J]. 航空发动机, 2023, 49(2): 168
[18] Sun Y, Li Z B, Ma L W, et al. Research progress on corrosion failure of high-temperature coatings in aero-engines[J]. Therm. Spray Technol., 2024, 16(2): 1
doi: 10.1007/s11666-007-9016-9
[18] 孙 毅, 李宗宝, 马菱薇 等. 航空发动机高温涂层腐蚀失效研究进展[J]. 热喷涂技术, 2024, 16(2): 1
[19] Yang Z Q, Zhang J, Luo C Y, et al. Effect of pre-oxidation and sea salt on the hot corrosion behavior of MCrAlY coatings and Al-Si coatings[J]. Surf. Coat. Technol., 2024, 477: 130354
doi: 10.1016/j.surfcoat.2023.130354
[20] Zamani P, Valefi Z. Hot corrosion resistance of Al2O3 nanoparticles reinforced CoNiCrAlY coatings deposited by LPPS and HVOF processes in molten Na2SO4-V2O5 at 850 oC[J]. Surf. Coat. Technol., 2023, 472: 129949
doi: 10.1016/j.surfcoat.2023.129949
[21] Zhan X, Wang D, Dong J S, et al. Effect of coating degradation on the hot corrosion behaviour of directionally solidified superalloy[J]. Corros. Sci., 2023, 215: 111057
doi: 10.1016/j.corsci.2023.111057
[22] Sumner J, Potter A, Simms N J, et al. Hot corrosion resistance of gas turbine materials in combusted syngas environments[J]. Mater. High Temp., 2015, 32: 177
doi: 10.1179/0960340914Z.00000000098
[23] Li R Z, Pu J B, Cheng C Q, et al. Effect of hot corrosion on cycle deformation and fracture behavior of Ti-6Al-4V alloy under salt coating[J]. Corros. Sci., 2023, 224: 111545
doi: 10.1016/j.corsci.2023.111545
[24] Yang B S, Li B, Wang S Y, et al. High temperature hot corrosion of single crystal superalloy DD6 subject to varying amounts of sodium salt deposited[J]. Equip. Environ. Eng., 2023, 20(12): 10
[24] 杨百顺, 李 彪, 王思远 等. 钠盐量影响下DD6单晶高温合金的高温热腐蚀规律研究[J]. 装备环境工程, 2023, 20(12): 10
[25] Hu Q, Geng S J, Wang J L, et al. Hot corrosion behavior of Inconel 718 without and with aluminide coating in air beneath a thin film of salt mixture of Na2SO4 + 5%NaCl[J]. J. Chin. Soc. Corros. Prot., 2024, 44: 623
[25] 胡 琪, 耿树江, 王金龙 等. Inconel 718及其渗铝涂层在Na2SO4 + 5%NaCl混合盐膜下的热腐蚀行为[J]. 中国腐蚀与防护学报, 2024, 44: 623
[26] Doolabi M S, Ghasemi B, Sadrnezhaad S K, et al. Hot corrosion behavior and near-surface microstructure of a “low-temperature high-activity Cr-aluminide” coating on inconel 738LC exposed to Na2SO4, Na2SO4 + V2O5 and Na2SO4 + V2O5 + NaCl at 900 oC[J]. Corros. Sci., 2017, 128: 42
doi: 10.1016/j.corsci.2017.09.004
[27] Meng J S, Chen M X, Shi X P, et al. Effect of Co on oxidation and hot corrosion behavior of two nickel-based superalloys under Na2SO4-NaCl at 900 oC[J]. Trans. Nonferrous Met. Soc. China, 2021, 31: 2402
doi: 10.1016/S1003-6326(21)65662-5
[28] Cuevas-Arteaga C. Corrosion study of HK-40m alloy exposed to molten sulfate/vanadate mixtures using the electrochemical noise technique[J]. Corros. Sci., 2008, 50: 650
doi: 10.1016/j.corsci.2007.11.011
[29] Song P, Liu M F, Jiang X W, et al. Influence of alloying elements on hot corrosion resistance of nickel-based single crystal superalloys coated with Na2SO4 salt at 900 oC[J]. Mater. Des., 2021, 197: 109197
doi: 10.1016/j.matdes.2020.109197
[30] Ye L Y, Chen H F, Yang G, et al. Effect of V2O5 on the hot corrosion resistance of β-(Ni, Pt)Al coating[J]. Mater. Rep., 2025, 39(7): 176
[30] 叶利亚, 陈宏飞, 杨 光 等. V2O5对β-(Ni, Pt)Al涂层热腐蚀抗性的影响[J]. 材料导报, 2025, 39(7): 176
[31] Wang J J, Yao Z H, Zhang P, et al. Effect of element S on interfacial stability of matrix and thermal barrier coating in nickle-based superalloys[J]. Acta Metall. Sin., 2024, 60: 1250
doi: 10.11900/0412.1961.2022.00611
[31] 王京京, 姚志浩, 张 鹏 等. 镍基高温合金中S元素对基体与热障涂层界面稳定性的影响[J]. 金属学报, 2024, 60: 1250
doi: 10.11900/0412.1961.2022.00611
[32] Yang Y Q, Zhao Y C, Wen Z X, et al. Synergistic effect of multiple molten salts on hot corrosion behaviour of Ni-based single crystal superalloy[J]. Corros. Sci., 2022, 204: 110381
doi: 10.1016/j.corsci.2022.110381
[33] Mobin M, Malik A U. Studies on the interactions of transition metal oxides and sodium sulfate in the temperature range 900-1200 K in oxygen[J]. J. Alloys Compd., 1996, 235: 97
doi: 10.1016/0925-8388(95)02125-6
[1] 宝尔根, 王建韬, 徐文静, 马会, 陈星秋. 合金元素对 α-Fe中H原子溶解及扩散影响的第一性原理研究[J]. 金属学报, 2026, 62(3): 489-496.
[2] 申文龙, 廖宇轩, 吴学志, 姜彦博, 柳文波. 晶界沟槽形成过程的相场模拟[J]. 金属学报, 2026, 62(3): 523-531.
[3] 江国龙, 周霞. 超声辅助下Mg/Mg-Zn-Al钎焊界面行为的分子动力学模拟[J]. 金属学报, 2026, 62(2): 372-382.
[4] 杨旭, 杨振文, 王颖, 李会军, 李永兵. 超声冲击制备梯度纳米结构Zr-4合金低温扩散连接界面组织与力学性能[J]. 金属学报, 2026, 62(1): 159-172.
[5] 张洺川, 徐勤思, 刘意, 蔡雨升, 牟义强, 任德春, 吉海宾, 雷家峰. 热压温度对TC4合金扩散连接区组织与性能的影响[J]. 金属学报, 2025, 61(8): 1183-1192.
[6] 汤思璠, 魏晶晶, 岳怡心, 李鹏宇, 姚曼, 王旭东. 六重对称合金枝晶生长场变量扩散元胞自动机模型[J]. 金属学报, 2025, 61(6): 941-952.
[7] 郭星星, 帅美荣, 楚志兵, 李玉贵, 谢广明. 不锈钢复合钢筋近界面微观组织演变及元素扩散动力学[J]. 金属学报, 2025, 61(2): 336-348.
[8] 王海丰, 蒲振新, 张建宝. 非平衡界面动力学理论[J]. 金属学报, 2025, 61(1): 29-42.
[9] 马芳, 陆星宇, 周丽娜, 杜宁宇, 类承帅, 刘宏伟, 李殿中. M50钢中 M2C一次碳化物高温转变机制[J]. 金属学报, 2024, 60(7): 901-914.
[10] 许增光, 周士祺, 李晓, 刘志权. (111)取向纳米孪晶Cu的抗氧化性能及焊料润湿性[J]. 金属学报, 2024, 60(7): 957-967.
[11] 李聪, 王猛, 屠汉俊, 施立群. Y掺杂Ti膜的吸放氢行为[J]. 金属学报, 2024, 60(6): 826-836.
[12] 杜随更, 王松林, 胡弘毅. TiAl基合金与GH3039合金摩擦-扩散双重焊焊合区过渡相的形成、结构与原位开裂[J]. 金属学报, 2024, 60(12): 1637-1646.
[13] 宫声凯, 刘原, 耿粒伦, 茹毅, 赵文月, 裴延玲, 李树索. 涂层/高温合金界面行为及调控研究进展[J]. 金属学报, 2023, 59(9): 1097-1108.
[14] 徐文国, 郝文江, 李应举, 赵庆彬, 卢炳聿, 郭和一, 刘天宇, 冯小辉, 杨院生. 微量Al、Ti对Inconel 690合金高温氧化行为的影响[J]. 金属学报, 2023, 59(12): 1547-1558.
[15] 刘路军, 刘政, 刘仁辉, 刘永. Nd90Al10 晶界调控对晶界扩散磁体磁性能和微观结构的影响[J]. 金属学报, 2023, 59(11): 1457-1465.