Please wait a minute...
金属学报  2026, Vol. 62 Issue (6): 1043-1058    DOI: 10.11900/0412.1961.2025.00350
  研究论文 本期目录 | 过刊浏览 |
热处理对FGH96高温合金惯性摩擦焊接头微观组织演变及力学性能的影响
王彬1, 赵鹏2, 刘家伟1, 张春波3, 秦志伟1, 董红刚1, 李鹏1()
1 大连理工大学 材料科学与工程学院 大连 116024
2 中国航发动力股份有限公司 西安 710021
3 中国机械总院集团哈尔滨焊接研究所有限公司 哈尔滨 150028
Effect of Heat Treatment on Microstructural Evolution and Mechanical Properties of Inertial Friction Welded Joints for FGH96 Superalloy
WANG Bin1, ZHAO Peng2, LIU Jiawei1, ZHANG Chunbo3, QIN Zhiwei1, DONG Honggang1, LI Peng1()
1 School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China
2 AECC Aviation Power Co. Ltd., Xi'an 710021, China
3 CAM Harbin Welding Institute Limited Company, Harbin 150028, China
引用本文:

王彬, 赵鹏, 刘家伟, 张春波, 秦志伟, 董红刚, 李鹏. 热处理对FGH96高温合金惯性摩擦焊接头微观组织演变及力学性能的影响[J]. 金属学报, 2026, 62(6): 1043-1058.
Bin WANG, Peng ZHAO, Jiawei LIU, Chunbo ZHANG, Zhiwei QIN, Honggang DONG, Peng LI. Effect of Heat Treatment on Microstructural Evolution and Mechanical Properties of Inertial Friction Welded Joints for FGH96 Superalloy[J]. Acta Metall Sin, 2026, 62(6): 1043-1058.

全文: PDF(9627 KB)   HTML
摘要: 

针对惯性摩擦焊接头焊核区(WZ)强化相溶解和轴向/径向微观组织不均匀等固有工艺瓶颈,本工作提出一种基于FGH96高温合金惯性摩擦焊接头的焊后热处理精细化调控策略,系统研究了固溶时效和双级时效处理对接头微观组织演变及力学性能的影响规律。结果表明,随着固溶温度升高,接头晶粒尺寸和再结晶程度增加,γ′强化相的析出和长大更为显著,碳化物分布趋于均匀,WZ晶界锯齿化加剧。当固溶温度达到1140 ℃时,晶粒发生异常长大,γ′强化相粗化且分布不均。随固溶温度升高,固溶时效处理后接头冲击韧性提升,抗拉强度则呈现先增后降的趋势。当固溶温度为1080 ℃时,晶粒和γ′强化相尺寸适中且分布均匀,再结晶和晶界锯齿化程度较高,碳化物均匀弥散分布,接头沿轴/径向的微观组织不均匀性明显改善。接头在室温和750 ℃时的抗拉强度分别为1455和1042 MPa,室温冲击韧性为41 J/cm2,实现了接头强度与韧性的良好协同。双级时效处理促进焊缝区三次γ′强化相均匀析出,使接头在室温和750 ℃时的抗拉强度分别达到1574和1279 MPa,基本达到母材强度。同时,接头硬度显著提升并超过母材,但冲击韧性较焊态接头略有下降。

关键词 : 焊后热处理,  惯性摩擦焊接,  γ′强化相,  微观组织,  力学性能    
Abstract:

Aero engines serve as a critical indicator of national comprehensive strength and technological advancement. However, their performance enhancement poses considerable challenges to the manufacturing technologies of hot-end components. Hot-end structures undergo inertial friction welding, which effectively avoids the defects associated with fusion welding and has been widely adopted for high-quality joining of these structures. This study addresses the inherent process limitations of inertial friction welded joints, including strengthening phase dissolution within the welding zone (WZ), along with axial and radial microstructural heterogeneity, and proposes a customized post-weld heat treatment (PWHT) strategy for inertial friction welded joints of FGH96 superalloys. A systematic investigation was conducted on the effects of solution aging and double aging on microstructural evolution and mechanical properties. The results indicated that increasing the solution temperature leads to grain coarsening and enhanced recrystallization, accompanied by pronounced precipitation and growth of the γ′ strengthening phase, a more uniform carbide distribution, and intensified grain boundary serration within the WZ compared to joints at low solution temperature. At a solution temperature of 1140 oC, abnormal grain growth occurred, along with coarsening and inhomogeneous distribution of the γ′ strengthening phase. After solution aging, the impact toughness of the joints improved with increasing solution temperature, whereas the tensile strength initially increased and then decreased. At the solution temperature of 1080 oC, the grain size and γ′ strengthening phase were moderate and uniformly distributed, the degree of recrystallization and grain boundary serration were relatively high, carbides were uniformly dispersed, and microstructural inhomogeneity was notably improved. Under this condition, the ultimate tensile strengths of the joints at room temperature and 750 °C were 1455 and 1042 MPa, respectively; and the impact toughness reached 41 J/cm2, demonstrating an optimal strength-toughness synergy. Double aging promoted the uniform precipitation of tertiary γ′ strengthening phase in the WZ, resulting in tensile strengths of 1574 and 1279 MPa at room temperature and 750 oC, respectively, approaching base metal levels. Meanwhile, the hardness was considerably enhanced beyond the base metal, although the impact toughness was slightly reduced compared with the as-welded joints.

Key words: post-weld heat treatment    inertial friction welding    γ′ strengthening phase    microstructure    mechanical property
收稿日期: 2025-10-31     
ZTFLH:  TG132.3  
基金资助:国家自然科学基金项目(52375313);国家自然科学基金项目(51605075)
通讯作者: 李 鹏,lipeng2016@dlut.edu.cn,主要从事固相焊接理论与技术研究
Corresponding author: LI Peng, professor, Tel: (0411)84706283, E-mail: lipeng2016@dlut.edu.cn
作者简介: 王 彬,男,1999年生,博士
图1  微观组织形貌、热处理工艺流程、焊接设备照片以及组织观察和力学测试试样取样位置
图2  焊态及不同焊后热处理态接头中沿轴向晶粒分布的反极图(IPF)
图3  焊态及不同焊后热处理态接头的平均晶粒尺寸分布
图4  焊态及不同焊后热处理态接头沿轴向的晶粒分布图
图5  焊态及不同焊后热处理态接头沿轴向的晶粒占比
图6  焊态及不同焊后热处理态接头焊核区(WZ)和母材(BM)区强化相分布的SEM像
图7  焊态及不同焊后热处理态接头WZ和母材区晶界和碳化物的SEM像
图8  焊态接头不同区域微观组织的IPF
图9  焊态接头沿径向的特殊晶界分析
图10  1080 ℃ SA接头微观组织的IPF
图11  1080 ℃ SA接头平均晶粒尺寸分布
图12  焊态及焊后热处理态接头的显微硬度
图13  焊后热处理态接头的力学性能
图14  焊后热处理态接头照片和断口形貌的SEM像
[1] Bai R S, Tan Y, Cui H Y, et al. Effect of electron beam smelting power on microstructure, segregation, and γ′ phase precipitation behavior of GH4068 alloy[J]. Acta Metall. Sin., 2024, 60: 1189
[1] 白如圣, 谭 毅, 崔弘阳 等. 电子束熔炼功率对GH4068合金微观组织、偏析和γ′相析出行为的影响[J]. 金属学报, 2024, 60: 1189
doi: 10.11900/0412.1961.2023.00263
[2] Peng Z C, Luo J P, Zhao Y, et al. Evolution of microstrucutre during static recrystallization in FGH96 superalloy[J]. Acta Metall. Sin., 2025, 61: 235
doi: 10.11900/0412.1961.2022.00540
[2] 彭子超, 罗俊鹏, 赵 宇 等. FGH96合金静态再结晶过程的显微组织演化[J]. 金属学报, 2025, 61: 235
doi: 10.11900/0412.1961.2022.00540
[3] Zhou Q, Ding Q Q, Liu D Y, et al. The grain boundary brittleness at intermediate temperature in a precipitation strengthened Ni-based polycrystalline alloy[J]. Acta Mater., 2025, 285: 120681
doi: 10.1016/j.actamat.2024.120681
[4] Zhou Y, Fang X W, Xi N Y, et al. Enhanced strength and ductility of laser-directed energy deposition repaired IN718 superalloy via a novel tailored heat treatment[J]. J. Mater. Sci. Technol., 2024, 199: 86
doi: 10.1016/j.jmst.2024.03.008
[5] Li C A, Qin G L, Fu B L, et al. Simulation of interfacial friction regime transition in inertia friction welding[J]. Int. J. Mech. Sci., 2025, 303: 110643
doi: 10.1016/j.ijmecsci.2025.110643
[6] Liu Y, Liu Y F, Zhang S R, et al. Diffusion behavior of oxygen in FGH96 superalloys during consolidation process[J]. Corros. Sci., 2024, 238: 112357
doi: 10.1016/j.corsci.2024.112357
[7] Liu Y, Zhang S, Zhang L, et al. A new perspective about the surface structure of FGH96 superalloys powders[J]. Vacuum, 2024, 220: 112838
doi: 10.1016/j.vacuum.2023.112838
[8] Qin Z W, Zhao Q, Zhang L, et al. Research progress on inertial friction welding of nickel-based superalloy GH4065A and IN718[J]. J. Net. Form. Eng., 2024, 16(10): 28
[8] 秦志伟, 赵 强, 张 露 等. 镍基高温合金GH4065A与IN718惯性摩擦焊接研究进展[J]. 精密成形工程, 2024, 16(10): 28
[9] Wang J W, Wang H M, Gao H W, et al. Microstructure characteristics and failure mechanisms of hybrid manufacturing of FGH96 and IC10 bimetal component using laser directed energy deposition[J]. Mater. Sci. Eng., 2024, A889: 145965
[10] Xu X X, You G Q, Ding Y H, et al. Microstructure and mechanical properties of inertia friction welded joints between high-strength low-alloy steel and medium carbon steel[J]. J. Mater. Process. Technol., 2020, 286: 116811
doi: 10.1016/j.jmatprotec.2020.116811
[11] Wang B, Liu J W, Qin Z W, et al. Cumulative strain-induced gradient heterostructure for synchronously boosting mechanical properties and corrosion resistance[J]. J. Mater. Sci. Technol., 2026, 270: 1
doi: 10.1016/j.jmst.2026.01.029
[12] Tang T X, Shi Q Y, Zhang C B, et al. Elucidating the in-process interfacial friction regime and thermal responses during inertia friction welding of dissimilar superalloys[J]. J. Mater. Res. Technol., 2024, 30: 1650
doi: 10.1016/j.jmrt.2024.03.210
[13] Li C A, Qin G L, Wang H. Omnidirectional simulation analysis of thermo-mechanical coupling mechanism in inertia friction welding of Ni-based superalloy[J]. Chin. J. Aeronaut., 2025, 38: 103047
doi: 10.1016/j.cja.2024.05.003
[14] Cao K, Fan J K, Liu X D, et al. Microstructure and mechanical properties of nickel-based wrought superalloys under thermal-mechanical coupling: A review with Inconel 718, 625 as main cases[J]. Prog. Nat. Sci., 2025, 35: 65
doi: 10.1016/j.pnsc.2024.12.001
[15] Zhang C B, Liang W, Zhou J, et al. Effect of heat treatment on microstructure and microhardness of FGH96 inertia friction welding[J]. Trans. China Weld. Inst., 2023, 44(8): 57
[15] 张春波, 梁 武, 周 军 等. 热处理工艺对FGH96合金惯性摩擦焊组织与显微硬度的影响[J]. 焊接学报, 2023, 44(8): 57
[16] Li Y M, Liu C X, Yu L M, et al. Effect of high-temperature ageing on microstructure and mechanical properties of linear friction welded S31042 steel joint[J]. Acta Metall. Sin., 2018, 54: 981
doi: 10.11900/0412.1961.2017.00483
[16] 李彦默, 刘晨曦, 余黎明 等. 高温时效对S31042钢线性摩擦焊接头组织和力学性能的影响[J]. 金属学报, 2018, 54: 981
doi: 10.11900/0412.1961.2017.00483
[17] Gai Y C, Zhang R, Yang J X, et al. Effects of heat treatment on γ′ precipitates and tensile properties of a Ni-base superalloy[J]. Mater. Sci. Eng., 2022, A842: 143079
[18] Li H Y, Sun J F, Hardy M C, et al. Effects of microstructure on high temperature dwell fatigue crack growth in a coarse grain PM nickel based superalloy[J]. Acta Mater., 2015, 90: 355
doi: 10.1016/j.actamat.2015.02.023
[19] Semiatin S L, Levkulich N C, Saurber A E, et al. The kinetics of precipitate dissolution in a nickel-base superalloy[J]. Metall. Mater. Trans., 2017, 48A: 5567
[20] Liu J T, Liu G Q, Hu B F, et al. Study on grain growth of P/M FGH96 superalloy[J]. Trans. Mater. Heat Treat., 2004, 25(6): 25
[20] 刘建涛, 刘国权, 胡本芙 等. FGH96合金晶粒长大规律的研究[J]. 材料热处理学报, 2004, 25(6): 25
[21] Yang J, Li J L, Xiong J T, et al. Effect of solution treatment temperature on the γ′ precipitation distribution, high temperature tensile and fatigue properties of FGH96 joints prepared by inertia friction welding[J]. Mater. Res. Express, 2019, 6: 1165g9
[22] Han X F, Zhu G L, Tan Q B, et al. Effect of semi-aging heat treatment on microstructure and mechanical properties of an inertia friction welded joint of FGH96 powder metallurgy superalloy[J]. Metals, 2023, 13: 632
doi: 10.3390/met13030632
[23] Hao Z B, Tian T, Peng S Q, et al. Effect of heat treatment on microstructure and properties of FGH4096M superalloy processed by selective laser melting[J]. Met. Mater. Int., 2020, 26: 1270
doi: 10.1007/s12540-019-00467-0
[24] Fang B, Ji Z, Tian G F, et al. Investigation on complete solution temperature of γ' in the P/M superalloy of FGH96[J]. Powder Metall. Technol., 2013, 31(02): 89
[24] 方 彬, 纪 箴, 田高峰 等. FGH96高温合金中γ'相完全溶解温度的研究[J]. 粉末冶金技术, 2013, 31(02): 89
[25] Zhang C, Shen W F, Zhang L W, et al. The microstructure and gamma prime distributions in inertia friction welded joint of P/M superalloy FGH96[J]. J. Mater. Eng. Perform., 2017, 26: 1581
doi: 10.1007/s11665-017-2601-2
[26] Yang J, Li J L, Jin F. Effect of welding parameters on high-temperature tensile and fatigue properties of FGH96 inertia friction welded joints[J]. Weld. World, 2019, 63: 1033
doi: 10.1007/s40194-019-00740-1
[27] Senkov O N, Mahaffey D W, Semiatin S L. Effect of process parameters on process efficiency and inertia friction welding behavior of the superalloys LSHR and Mar-M247[J]. J. Mater. Process. Technol., 2017, 250: 156
doi: 10.1016/j.jmatprotec.2017.07.020
[28] Zheng K K, Yang Z K, Mou G. Effect of inertia friction welding speed on microstructure and mechanical properties of 2205/316L stainless steel joints[J]. Mater. Today Commun., 2023, 35: 106226
[29] Liu Y Y, Tian W T, Yang Q H, et al. Inertia radial friction welding of Ti60(near-α)/TC18(near-β) bimetallic components: Interfacial bon-ding mechanism, heterogenous microstructure and mechanical properties[J]. Mater. Charact., 2024, 208: 113598
doi: 10.1016/j.matchar.2023.113598
[30] Pan L W, Li P, Hao X H, et al. Inhomogeneity of microstructure and mechanical properties in radial direction of aluminum/copper friction welded joints[J]. J. Mater. Process. Technol., 2018, 255: 308
doi: 10.1016/j.jmatprotec.2017.12.027
[31] Mishra N K, Manikandan S G K, Shrivastava A. Interfacial inhomogeneous plastic deformation during rotary friction welding of dissimilar AA2219-SS321 joint combination with AA6061 interlayer[J]. J. Adv. Join. Process., 2024, 10: 100245
[32] Zhao P, Li P, Ding Z J, et al. Microstructural characterization and mechanical properties of inertia friction welded FGH96 joints[J]. Mater. Today Commun., 2025, 42: 111194
[1] 王玮, 张宇博, 赵燕, 王同敏, 李廷举. 高熵合金颗粒对选区激光熔化Al12Si合金固溶组织和力学性能的影响[J]. 金属学报, 2026, 62(6): 1009-1020.
[2] 秦志伟, 王彬, 赵强, 李家辰, 孙毓涛, 洪小龙, 李鹏, 董红刚. 热处理对GH4065A/IN718异质高温合金惯性摩擦焊接头界面微观组织的影响[J]. 金属学报, 2026, 62(6): 1032-1042.
[3] 许鼎锋, 韩飞扬, 姜琦成, 王欢, 尚利媛, 卢一平. AlCrFeCoNi低膨胀合金的成分设计及组织和性能优化[J]. 金属学报, 2026, 62(6): 1021-1031.
[4] 吕昭平, 申耀祖, 王先珍, 陈强, 唐建国, 张晓宾, 于勇, 蒋虽合, 刘雄军, 王辉, 吴渊. 面向极端服役条件的高熵合金结构材料:性能优势、瓶颈与突破路径[J]. 金属学报, 2026, 62(5): 743-755.
[5] 郭恩宇, 杜泽龙, 李炳志, 王同敏. 基于同步辐射原位表征技术的镁合金研究进展[J]. 金属学报, 2026, 62(5): 890-904.
[6] 郑玉峰, 谌雨农. 纯Mo及钼基可降解金属材料的研究现状与发展趋势[J]. 金属学报, 2026, 62(5): 905-922.
[7] 陈光, 陈奉锐, 朱德民, 李贵忠, 李罗, 宋伟东, 王子特, 相恒高, 陈旸, 祁志祥. 聚片孪生功能基元序构的高性能TiAl合金[J]. 金属学报, 2026, 62(4): 541-549.
[8] 王建峰, 许珍木, 刘战, 高转妮, 占小红. 超声振动对TC4钛合金窄间隙激光焊接组织及强化机理的影响[J]. 金属学报, 2026, 62(3): 406-420.
[9] 蒋志达, 胥杨洋, 于佳新, 刘文才, 朱浩文, 吴国华, 尚郑平. 高温无氧轧制Cu/1060Al/Cu三层复合材料的力学和导电性能[J]. 金属学报, 2026, 62(3): 431-444.
[10] 江国龙, 周霞. 超声辅助下Mg/Mg-Zn-Al钎焊界面行为的分子动力学模拟[J]. 金属学报, 2026, 62(2): 372-382.
[11] 陆善平, 孙健. 高强钢焊缝金属组织设计与强韧化机理研究进展[J]. 金属学报, 2026, 62(1): 1-16.
[12] 阴嘉琳, 石磊, 武传松. 超声振动对镁/铝异质合金搅拌摩擦搭接焊接头界面组织演变的影响[J]. 金属学报, 2026, 62(1): 133-147.
[13] 王启勇, 李晓博, 刘小超, 王心成, 张泰瑞, 倪中华, 陈彪. 低碳钢预制涡流搅拌摩擦焊工艺研究[J]. 金属学报, 2026, 62(1): 217-234.
[14] 李红, 姜玉清, 曹玉鹏, 王加友, 刘澍彬. 冷丝辅助旋转/摇动电弧窄间隙MAG焊缝成形特性及接头组织性能演变机制[J]. 金属学报, 2026, 62(1): 235-252.
[15] 张天宇, 张鹏, 肖娜, 王小海, 刘国强, 杨志刚, 张弛. 奥氏体化温度对2 GPa超高强钢显微组织和力学性能的影响[J]. 金属学报, 2025, 61(9): 1353-1363.