| 基于同步辐射原位表征技术的镁合金研究进展 |
郭恩宇1,2( ), 杜泽龙1, 李炳志1, 王同敏1,2( ) |
1 大连理工大学 材料科学与工程学院 辽宁省凝固控制与数字化制备技术重点实验室 大连 116024 2 大连理工大学宁波研究院 宁波 315032 |
|
| Research Progress on Magnesium Alloys Based on Synchrotron Radiation In Situ Characterization Techniques |
GUO Enyu1,2( ), DU Zelong1, LI Bingzhi1, WANG Tongmin1,2( ) |
1 Key Laboratory of Solidification Control and Digital Preparation Technology (Liaoning Province), School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China 2 Ningbo Research Institute of Dalian University of Technology, Ningbo 315032, China |
引用本文:
郭恩宇, 杜泽龙, 李炳志, 王同敏. 基于同步辐射原位表征技术的镁合金研究进展[J]. 金属学报, 2026, 62(5): 890-904.
Enyu GUO,
Zelong DU,
Bingzhi LI,
Tongmin WANG.
Research Progress on Magnesium Alloys Based on Synchrotron Radiation In Situ Characterization Techniques[J]. Acta Metall Sin, 2026, 62(5): 890-904.
| [1] |
Zhu Q C, Li Y X, Cao F Y, et al. Towards development of a high-strength stainless Mg alloy with Al-assisted growth of passive film [J]. Nat. Commun., 2022, 13: 5838
doi: 10.1038/s41467-022-33480-w
pmid: 36192418
|
| [2] |
Yu M D, Li Y F, Guo H, et al. Anomalous strain hardening via manipulating basal/pyramidal dislocation interactions in the Mg-Y-Ca alloy [J]. Acta Mater., 2025, 296: 121309
doi: 10.1016/j.actamat.2025.121309
|
| [3] |
Guru M K, Bohlen J, Aydin R C, et al. Machine learning pipeline for structure-property modeling in Mg-alloys using microstructure and texture descriptors [J]. Acta Mater., 2025, 295: 121132
doi: 10.1016/j.actamat.2025.121132
|
| [4] |
Ma C, Yu W, Zhang Z, et al. The effect of slow shot speed and casting pressure on the 3D microstructure of high pressure die casting AE44 magnesium alloy [J]. J. Magnes. Alloy., 2023, 11: 753
doi: 10.1016/j.jma.2021.09.011
|
| [5] |
Paliwal M, Jung I H. The evolution of the growth morphology in Mg-Al alloys depending on the cooling rate during solidification [J]. Acta Mater., 2013, 61: 4848
doi: 10.1016/j.actamat.2013.04.063
|
| [6] |
Ni R, Boehlert C J, Chen B, et al. Temperature-dependent interplay of intra- and inter-granular deformation mechanisms in Mg-10Y: Statistical analysis from an HRDIC perspective [J]. Acta Mater., 2025, 296: 121256
doi: 10.1016/j.actamat.2025.121256
|
| [7] |
Jeong J, Alfreider M, Konetschnik R, et al. In-situ TEM observation of 10 1 ¯ 2 twin-dominated deformation of Mg pillars: Twinning mechanism, size effects and rate dependency [J]. Acta Mater., 2018, 158: 407
doi: 10.1016/j.actamat.2018.07.027
|
| [8] |
Fan X Q, Fleming T G, Clark S J, et al. Magnetic modulation of keyhole instability during laser welding and additive manufacturing [J]. Science, 2025, 387: 864
doi: 10.1126/science.ado8554
pmid: 39977505
|
| [9] |
Ajayi T M, Shirato N, Rojas T, et al. Characterization of just one atom using synchrotron X-rays [J]. Nature, 2023, 618: 69
doi: 10.1038/s41586-023-06011-w
|
| [10] |
Guo E Y, Du Z L, Chen X B, et al. Development of magnesium alloys: Advanced characterization using synchrotron radiation techniques [J]. J. Mater. Sci. Technol., 2024, 195: 93
doi: 10.1016/j.jmst.2024.01.029
|
| [11] |
Mathiesen R H, Arnberg L, Mo F, et al. Time resolved X-ray imaging of dendritic growth in binary alloys [J]. Phys. Rev. Lett., 1999, 83: 5062
doi: 10.1103/PhysRevLett.83.5062
|
| [12] |
Abou-Khalil L, Da Cruz K S, Reinhart G, et al. Influence of growth velocity on fragmentation during directional solidification of Al-14 wt.% Sn alloy studied by in-situ synchrotron X-radiography [J]. Acta Mater., 2022, 241: 118370
doi: 10.1016/j.actamat.2022.118370
|
| [13] |
Azeem M A, Lee P D, Phillion A B, et al. Revealing dendritic pattern formation in Ni, Fe and Co alloys using synchrotron tomography [J]. Acta Mater., 2017, 128: 241
doi: 10.1016/j.actamat.2017.02.022
|
| [14] |
Buffiere J Y, Maire E, Adrien J, et al. In situ experiments with X ray tomography: An attractive tool for experimental mechanics [J]. Exp. Mech., 2010, 50: 289
doi: 10.1007/s11340-010-9333-7
|
| [15] |
Bale H A, Haboub A, MacDowell A A, et al. Real-time quantitative imaging of failure events in materials under load at temperatures above 1, 600 oC [J]. Nat. Mater., 2013, 12: 40
doi: 10.1038/nmat3497
|
| [16] |
Zhang K, Wigger T, Pineda R, et al. Unravelling dynamic recrystallisation in a microalloyed steel during rapid high temperature deformation using synchrotron X-rays [J]. Acta Mater., 2024, 278: 120265
doi: 10.1016/j.actamat.2024.120265
|
| [17] |
Wang T M, Cao F, Zhou P, et al. Study on diffusion behavior and microstructural evolution of Al/Cu bimetal interface by synchrotron X-ray radiography [J]. J. Alloys Compd., 2014, 616: 550
doi: 10.1016/j.jallcom.2014.07.172
|
| [18] |
Wang T M, Xu J J, Xiao T Q, et al. Evolution of dendrite morphology of a binary alloy under an applied electric current: An in situ observation [J]. Phys. Rev., 2010, 81E: 042601
|
| [19] |
Zhang W, Simpson C A, Leitner T, et al. The effect of anisotropic microstructure on the crack growth and fatigue overload behaviour of ultrafine-grained nickel [J]. Acta Mater., 2020, 184: 225
doi: 10.1016/j.actamat.2019.11.024
|
| [20] |
Wu Z K, Wu S C, Kruzic J J, et al. Critical damage events of 3D printed AlSi10Mg alloy via in situ synchrotron X-ray tomography [J]. Acta Mater., 2025, 282: 120464
doi: 10.1016/j.actamat.2024.120464
|
| [21] |
Lin Y, Qian W J, Lei L M, et al. Structural integrity issues of composite materials and structures in future transportation equipment [J]. Compos. Struct., 2025, 358: 118943
doi: 10.1016/j.compstruct.2025.118943
|
| [22] |
Casari D, Mirihanage W U, Falch K V, et al. α-Mg primary phase formation and dendritic morphology transition in solidification of a Mg-Nd-Gd-Zn-Zr casting alloy [J]. Acta Mater., 2016, 116: 177
doi: 10.1016/j.actamat.2016.06.035
|
| [23] |
Du J, Zhang A, Guo Z, et al. Effect of additional solute elements (X = Al, Ca, Y, Ba, Sn, Gd and Zn) oncrystallographic anisotropy during the dendritic growth of magnesium alloys [J]. J. Alloys Compd., 2019, 775: 322
doi: 10.1016/j.jallcom.2018.10.145
|
| [24] |
Tang Y, Wu Y, Zhang Y, et al. Intermittent nucleation and periodic growth of grains under thermo-solutal convection during directional solidification of Al-Cu alloy [J]. Acta Mater., 2021, 212: 116861
doi: 10.1016/j.actamat.2021.116861
|
| [25] |
Wang M Y, Jing T, Liu B C. Phase-field simulations of dendrite morphologies and selected evolution of primary α-Mg phases during the solidification of Mg-rich Mg-Al-based alloys [J]. Scr. Mater., 2009, 61: 777
doi: 10.1016/j.scriptamat.2009.06.028
|
| [26] |
Yang M, Xiong S M, Guo Z. Characterisation of the 3-D dendrite morphology of magnesium alloys using synchrotron X-ray tomography and 3-D phase-field modelling [J]. Acta Mater., 2015, 92: 8
doi: 10.1016/j.actamat.2015.03.044
|
| [27] |
Yang M, Xiong S M, Guo Z. Effect of different solute additions on dendrite morphology and orientation selection in cast binary magnesium alloys [J]. Acta Mater., 2016, 112: 261
doi: 10.1016/j.actamat.2016.04.014
|
| [28] |
Shuai S S, Guo E Y, Wang J, et al. Synchrotron tomographic quantification of the influence of Zn concentration on dendritic growth in Mg-Zn alloys [J]. Acta Mater., 2018, 156: 287
doi: 10.1016/j.actamat.2018.06.026
|
| [29] |
Shuai S S, Guo E Y, Phillion A B, et al. Fast synchrotron X-ray tomographic quantification of dendrite evolution during the solidification of Mg Sn alloys [J]. Acta Mater., 2016, 118: 260
doi: 10.1016/j.actamat.2016.07.047
|
| [30] |
Guo E Y, Phillion A B, Cai B, et al. Dendritic evolution during coarsening of Mg-Zn alloys via 4D synchrotron tomography [J]. Acta Mater., 2017, 123: 373
doi: 10.1016/j.actamat.2016.10.022
|
| [31] |
Aagesen L K, Johnson A E, Fife J L, et al. Universality and self-similarity in pinch-off of rods by bulk diffusion [J]. Nat. Phys., 2010, 6: 796
|
| [32] |
Gu L D, Shang X Q, Wang J, et al. The influence of SiC-Al2O3 reinforcements on the deformation and fracture mechanism of thixomolded Mg-based composite [J]. J. Mater. Sci., 2024, 59: 9892
doi: 10.1007/s10853-024-09386-x
|
| [33] |
Huang S J, Subramani M, Ali A N, et al. The effect of micro-SiCp content on the tensile and fatigue behavior of AZ61 magnesium alloy matrix composites [J]. Int. J. Metalcast., 2021, 15: 780
doi: 10.1007/s40962-020-00508-0
|
| [34] |
Wang P B, Shen J, Chen T J, et al. Simultaneously improving the strength and ductility of AZ91/GNPs composites through decorating graphene nanoplatelets with MgO [J]. J. Mater. Sci. Technol., 2024, 183: 133
doi: 10.1016/j.jmst.2023.10.020
|
| [35] |
Pu Z P, Wang S F, Yan Q, et al. Grain refinement mechanism of SiC nanoparticles/Mg-9 wt.% Al composite investigated by sharp interface model at microscale and nanoscale [J]. J. Alloys Compd., 2022, 922: 166269
doi: 10.1016/j.jallcom.2022.166269
|
| [36] |
Guo E Y, Shuai S S, Kazantsev D, et al. The influence of nanoparticles on dendritic grain growth in Mg alloys [J]. Acta Mater., 2018, 152: 127
doi: 10.1016/j.actamat.2018.04.023
|
| [37] |
Du Z L, Wang C, Liu F Y, et al. Unraveling the individual and synergistic effects of copper and gadolinium on the microstructure and mechanical properties of Mg-6Zn-0.5Ca alloy [J]. J. Alloys Compd., 2025, 1036: 181421
doi: 10.1016/j.jallcom.2025.181421
|
| [38] |
Du Z L, Yang X Q, Wang Q, et al. A synergetic approach to enhancing mechanical properties of trace TiB2 particles reinforced AZ91D composites through α-Mg grain refinement and β-Mg17Al12 manipulation [J]. Composites, 2025, 198: 109114
|
| [39] |
Yang X Q, Du Z L, Guo E Y, et al. Achieving simultaneous refinement of α-Mg grains and β-Mg17Al12 phases via trace multi-scale TiB2 for strength-ductility synergy in AZ91D composites [J]. J. Alloys Compd., 2025, 1048: 185116
doi: 10.1016/j.jallcom.2025.185116
|
| [40] |
Wu H Z, Du Z L, An Y K, et al. Grain refinement and mechanical property enhancement of AM60B magnesium alloy via TiB2 particle regulation [J]. Mater. Today Commun., 2025, 47: 112999
|
| [41] |
Ma C S, Yu W B, Zhang T T, et al. The effect of slow shot speed and casting pressure on the 3D microstructure of high pressure die casting AE44 magnesium alloy [J]. J. Magnes. Alloy., 2023, 11: 753
doi: 10.1016/j.jma.2021.09.011
|
| [42] |
Walmsley I A. Quantum optics: Science and technology in a new light [J]. Science, 2015, 348: 525
doi: 10.1126/science.aab0097
pmid: 25931550
|
| [43] |
Trang T T T, Zhang J H, Kim J H, et al. Designing a magnesium alloy with high strength and high formability [J]. Nat. Commun., 2018, 9: 2522
doi: 10.1038/s41467-018-04981-4
pmid: 29955065
|
| [44] |
Offerman S E, van Dijk N H, Sietsma J, et al. Grain nucleation and growth during phase transformations [J]. Science, 2002, 298: 1003
pmid: 12411699
|
| [45] |
Zhou X L, Feng Z Q, Zhu L L, et al. High-pressure strengthening in ultrafine-grained metals [J]. Nature, 2020, 579: 67
doi: 10.1038/s41586-020-2036-z
|
| [46] |
Zhang D S, Liu W, Li Y X, et al. In situ observation of crystal rotation in Ni-based superalloy during additive manufacturing process [J]. Nat. Commun., 2023, 14: 2961
doi: 10.1038/s41467-023-38727-8
pmid: 37221206
|
| [47] |
Schmidt S, Nielsen S F, Gundlach C, et al. Watching the growth of bulk grains during recrystallization of deformed metals [J]. Science, 2004, 305: 229
pmid: 15247474
|
| [48] |
Oddershede J, Camin B, Schmidt S, et al. Measuring the stress field around an evolving crack in tensile deformed Mg AZ31 using three-dimensional X-ray diffraction [J]. Acta Mater., 2012, 60: 3570
doi: 10.1016/j.actamat.2012.02.054
|
| [49] |
Huang Z H, Wang L Y, Zhou B J, et al. Observation of non-basal slip in Mg-Y by in situ three-dimensional X-ray diffraction [J]. Scr. Mater., 2018, 143: 44
doi: 10.1016/j.scriptamat.2017.09.011
|
| [50] |
Zhang N B, Zhang Y Y, Chen S, et al. Onset of detwinning in Mg-3Al-1Zn alloy: A synchrotron-based X-ray diffraction study [J]. Scr. Mater., 2021, 190: 113
doi: 10.1016/j.scriptamat.2020.08.044
|
| [51] |
Yi S B, Davies C H J, Brokmeier H G, et al. Deformation and texture evolution in AZ31 magnesium alloy during uniaxial loading [J]. Acta Mater., 2006, 54: 549
doi: 10.1016/j.actamat.2005.09.024
|
| [52] |
Wang W Y, Tang B, Shang S L, et al. Local lattice distortion mediated formation of stacking faults in Mg alloys [J]. Acta Mater., 2019, 170: 231
doi: 10.1016/j.actamat.2019.03.030
|
| [53] |
Garces G, Morris D G, Muñoz-Morris M A, et al. Plasticity analysis by synchrotron radiation in a Mg97Y2Zn1 alloy with bimodal grain structure and containing LPSO phase [J]. Acta Mater., 2015, 94: 78
doi: 10.1016/j.actamat.2015.04.048
|
| [54] |
Garces G, Medina J, Perez P, et al. The effect of temperature on load partitioning evolution in magnesium metal matrix composite reinforced with Ti particles using in-situ synchrotron radiation diffraction experiments [J]. J. Magnes. Alloy., 2023, 11: 706
doi: 10.1016/j.jma.2022.09.022
|
| [55] |
Arul Kumar M, Clausen B, Capolungo L, et al. Deformation twinning and grain partitioning in a hexagonal close-packed magnesium alloy [J]. Nat. Commun., 2018, 9: 4761
doi: 10.1038/s41467-018-07028-w
pmid: 30420672
|
| [56] |
Bong H J, Hu X H, Sun X, et al. Mechanism-based constitutive modeling of ZEK100 magnesium alloy with crystal plasticity and in-situ HEXRD experiment [J]. Int. J. Plast., 2019, 113: 35
doi: 10.1016/j.ijplas.2018.09.005
|
| [57] |
Zhang H J, Jérusalem A, Salvati E, et al. Multi-scale mechanisms of twinning-detwinning in magnesium alloy AZ31B simulated by crystal plasticity modeling and validated via in situ synchrotron XRD and in situ SEM-EBSD [J]. Int. J. Plast., 2019, 119: 43
doi: 10.1016/j.ijplas.2019.02.018
|
| [58] |
Wang H, Clausen B, Tomé C N, et al. Studying the effect of stress relaxation and creep on lattice strain evolution of stainless steel under tension [J]. Acta Mater., 2013, 61: 1179
doi: 10.1016/j.actamat.2012.10.027
|
| [59] |
Hu X H, Sun X, Hector L G, et al. Individual phase constitutive properties of a TRIP-assisted QP980 steel from a combined synchrotron X-ray diffraction and crystal plasticity approach [J]. Acta Mater., 2017, 132: 230
doi: 10.1016/j.actamat.2017.04.028
|
| [60] |
Jia N, Cong Z H, Sun X, et al. An in situ high-energy X-ray diffraction study of micromechanical behavior of multiple phases in advanced high-strength steels [J]. Acta Mater., 2009, 57: 3965
doi: 10.1016/j.actamat.2009.05.002
|
| [61] |
Abdolvand H, Daymond M R, Mareau C. Incorporation of twinning into a crystal plasticity finite element model: Evolution of lattice strains and texture in Zircaloy-2 [J]. Int. J. Plast., 2011, 27: 1721
doi: 10.1016/j.ijplas.2011.04.005
|
| [62] |
Agnew S R, Singh A, Calhoun C A, et al. In-situ neutron diffraction of a quasicrystal-containing Mg alloy interpreted using a new polycrystal plasticity model of hardening due to {10.2} tensile twinning [J]. Int. J. Plast., 2018, 100: 34
doi: 10.1016/j.ijplas.2017.09.005
|
| [63] |
Agnew S R, Mulay R P, Polesak F J, et al. In situ neutron diffraction and polycrystal plasticity modeling of a Mg-Y-Nd-Zr alloy: Effects of precipitation on individual deformation mechanisms [J]. Acta Mater., 2013, 61: 3769
doi: 10.1016/j.actamat.2013.03.010
|
| [64] |
Neil C J, Wollmershauser J A, Clausen B, et al. Modeling lattice strain evolution at finite strains and experimental verification for copper and stainless steel using in situ neutron diffraction [J]. Int. J. Plast., 2010, 26: 1772
doi: 10.1016/j.ijplas.2010.03.005
|
| [65] |
Wang H M, Wu P D, Kurukuri S, et al. Strain rate sensitivities of deformation mechanisms in magnesium alloys [J]. Int. J. Plast., 2018, 107: 207
doi: 10.1016/j.ijplas.2018.04.005
|
| [66] |
Lee S, Pilipchuk M, Yildirim C, et al. Three-dimensional nucleation and growth of deformation twins in magnesium [J]. Science, 2025, 389: 632
doi: 10.1126/science.adv3460
pmid: 40773550
|
| [67] |
Wang C, Du Z L, Guo E Y, et al. Mechanical behavior of SiC reinforced ZA63 Mg matrix composites: Experiments and 3D finite element modelling [J]. J. Magnes. Alloy., 2025, 13: 1294
doi: 10.1016/j.jma.2024.03.027
|
| [68] |
Hu Y N, Wu S C, Guo Y, et al. Inhibiting weld cracking in high-strength aluminium alloys [J]. Nat. Commun., 2022, 13: 5816
doi: 10.1038/s41467-022-33188-x
pmid: 36192380
|
| [69] |
An Y K, Guo E Y, Xia D Y, et al. A new strategy for fabricating Mg-Al alloys with excellent strength-ductility synergy via pulse-coupled wire-arc directed energy deposition [J]. Int. J. Plast., 2026, 196: 104550
doi: 10.1016/j.ijplas.2025.104550
|
| [70] |
Kondori B, Morgeneyer T F, Helfen L, et al. Void growth and coalescence in a magnesium alloy studied by synchrotron radiation laminography [J]. Acta Mater., 2018, 155: 80
doi: 10.1016/j.actamat.2018.05.026
|
| [71] |
Wang Z Y, Wu S C, Kang G Z, et al. In-situ synchrotron X-ray tomography investigation of damage mechanism of an extruded magnesium alloy in uniaxial low-cycle fatigue with ratchetting [J]. Acta Mater., 2021, 211: 116881
doi: 10.1016/j.actamat.2021.116881
|
| [72] |
Karagadde S, Lee P D, Cai B, et al. Transgranular liquation cracking of grains in the semi-solid state [J]. Nat. Commun., 2015, 6: 8300
doi: 10.1038/ncomms9300
pmid: 26353994
|
| [73] |
Azghandi S H M, Weiss M, Arhatari B D, et al. A rationale for the influence of grain size on failure of magnesium alloy AZ31: An in situ X-ray microtomography study [J]. Acta Mater., 2020, 200: 619
doi: 10.1016/j.actamat.2020.09.016
|
| [74] |
Kumar R, Lhuissier P, Villanova J, et al. Elementary growth mechanisms of creep cavities in AZ31 alloy revealed by in situ X-ray nano-tomography [J]. Acta Mater., 2022, 228: 117760
doi: 10.1016/j.actamat.2022.117760
|
| [75] |
Zeller-Plumhoff B, Robisch A L, Pelliccia D, et al. Nanotomographic evaluation of precipitate structure evolution in a Mg-Zn-Zr alloy during plastic deformation [J]. Sci. Rep., 2020, 10: 16101
doi: 10.1038/s41598-020-72964-x
pmid: 32999352
|
| [76] |
Pollock T M. Weight loss with magnesium alloys [J]. Science, 2010, 328: 986
doi: 10.1126/science.1182848
pmid: 20489013
|
| [77] |
Yang G F, Kim Y C, Han H S, et al. In vitro dynamic degradation behavior of new magnesium alloy for orthopedic applications [J]. J. Biomed. Mater. Res., 2015, 103B: 807
|
| [78] |
Esmaily M, Svensson J E, Fajardo S, et al. Fundamentals and advances in magnesium alloy corrosion [J]. Prog. Mater. Sci., 2017, 89: 92
doi: 10.1016/j.pmatsci.2017.04.011
|
| [79] |
Ročňáková I, Montufar E B, Horynová M, et al. Assessment of localized corrosion under simulated physiological conditions of magnesium samples with heterogeneous microstructure: Value of X-ray computed micro-tomography platform [J]. Corros. Sci., 2016, 104: 187
doi: 10.1016/j.corsci.2015.12.009
|
| [80] |
Zhang C, Liu C, Li X, et al. Quantifying the influence of secondary phases on corrosion in multicomponent Mg alloys using X-ray computed microtomography [J]. Corros. Sci., 2022, 195: 110010
doi: 10.1016/j.corsci.2021.110010
|
| [81] |
Tian G Y, Wang J S, Zhang C, et al. Quantifying the influence of microstructure on the corrosion of Mg-Li alloys by using X-ray CT [J]. Corros. Sci., 2024, 229: 111848
doi: 10.1016/j.corsci.2024.111848
|
| [82] |
Wang X J, Chen Z N, Guo E Y, et al. Corrosion process of Mg-Sn alloys revealed via in situ synchrotron X-ray radiography [J]. Mater. Lett., 2022, 308: 131139
doi: 10.1016/j.matlet.2021.131139
|
| [83] |
Liu X Q, Wang X J, Guo E Y, et al. Influence of deformation on the corrosion behavior of LZ91 Mg-Li alloy [J]. Int. J. Miner. Metall. Mater., 2023, 30: 72
doi: 10.1007/s12613-022-2466-8
|
| [84] |
Chen Z N, Ji H T, Geng X Q, et al. 3-D distribution characteristics of the micro-defects in the PEO coating on ZM6 Mg-alloy during corrosion [J]. Corros. Sci., 2020, 174: 108821
doi: 10.1016/j.corsci.2020.108821
|
| [85] |
Li B Z, Ouyang Y B, Guo E Y, et al. Mao-based solid-like slippery composite coating with superior corrosion resistance and robust machinery performance upon magnesium-lithium alloy LA81 [J]. Chem. Eng. J., 2024, 497: 154801
doi: 10.1016/j.cej.2024.154801
|
| [86] |
Fischerauer S F, Kraus T, Wu X, et al. In vivo degradation performance of micro-arc-oxidized magnesium implants: A micro-CT study in rats [J]. Acta Biomater., 2013, 9: 5411
doi: 10.1016/j.actbio.2012.09.017
pmid: 23022544
|
| [87] |
Hou X R, Li B Z, Zhou Z H, et al. Superhydrophobic and corrosion-resistant coating on magnesium-lithium alloys [J]. J. Taiwan Inst. Chem. Eng., 2025, 176: 106319
doi: 10.1016/j.jtice.2025.106319
|
| [88] |
Ouyang Y B, Zhou Z H, Guo E Y, et al. Boosting corrosion resistance of Mg-Li alloy: Implanting bioinspired superhydrophobic surfaces into MAO matrix for enhanced protection [J]. Ceram. Int., 2024, 50: 48425
doi: 10.1016/j.ceramint.2024.09.192
|
| [89] |
Li B Z, Liu B C, Guo E Y, et al. MAO-based self-healing phase-change solid-like slippery composite coating with superior corrosion resistance and robust machinery performance [J]. J. Mater. Sci. Technol., 2026, 253: 298
doi: 10.1016/j.jmst.2025.05.081
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|