Please wait a minute...
金属学报  2026, Vol. 62 Issue (2): 289-308    DOI: 10.11900/0412.1961.2025.00047
  综述 本期目录 | 过刊浏览 |
先进导电铜基复合材料设计与制备研究进展
姜伊辉1,2,3, 张兴德1, 石浩1,2,3, 曹飞1,2,3, 马文君1, 王艳芳1,2,3, 梁淑华1,2,3()
1 西安理工大学 材料科学与工程学院 西安 710048
2 西安理工大学 导电材料与复合技术教育部工程研究中心 西安 710048
3 西安理工大学 陕西省电工材料与熔渗技术重点实验室 西安 710048
Research Progress in the Design and Preparation of Advanced Conductive Copper Matrix Composites
JIANG Yihui1,2,3, ZHANG Xingde1, SHI Hao1,2,3, CAO Fei1,2,3, MA Wenjun1, WANG Yanfang1,2,3, LIANG Shuhua1,2,3()
1 School of Materials Science and Engineering, Xi'an University of Technology, Xi'an 710048, China
2 Engineering Research Center of Conducting Materials and Composite Technology, Ministry of Education, Xi'an University of Technology, Xi'an 710048, China
3 Shaanxi Province Key Laboratory of Electrical Materials and Infiltration Technology, Xi'an University of Technology, Xi'an 710048, China
引用本文:

姜伊辉, 张兴德, 石浩, 曹飞, 马文君, 王艳芳, 梁淑华. 先进导电铜基复合材料设计与制备研究进展[J]. 金属学报, 2026, 62(2): 289-308.
Yihui JIANG, Xingde ZHANG, Hao SHI, Fei CAO, Wenjun MA, Yanfang WANG, Shuhua LIANG. Research Progress in the Design and Preparation of Advanced Conductive Copper Matrix Composites[J]. Acta Metall Sin, 2026, 62(2): 289-308.

全文: PDF(6768 KB)   HTML
摘要: 

铜基复合材料具有高强度、高导电、高导热、耐高温、耐磨、耐电弧烧蚀等优良性能,有望成为未来苛刻服役环境下的关键基础导电材料之一。本文对导电型铜基复合材料的典型材料体系、主要制备技术以及组织性能等进行了归纳和总结,分析了原位制备方法的基本原理和特点,阐述了多种类型高强高导铜基复合材料组织特征与综合性能的关系规律,并展望了未来研究所面临的问题及挑战。

关键词 : 铜基复合材料,  制备技术,  组织设计,  性能调控    
Abstract:

Copper matrix composites are expected to be essential conductive materials for harsh service environments in the future, due to their remarkable properties, including high strength, excellent electrical and thermal conductivity, and their resistance to high temperatures, wear, and arc ablation. This paper summarizes the typical materials, primary preparation techniques, microstructures, and properties of conductive copper matrix composites. It further analyzes the basic principles and characteristics of in situ preparation methods. Finally, the relationship between microstructures and the overall properties of various high-strength and high-conductivity copper matrix composites is discussed, and the problems and challenges that future research may face are considered.

Key words: copper matrix composites    preparation technology    microstructure design    property modulation
收稿日期: 2025-02-24     
ZTFLH:  TG146.1  
基金资助:国家自然科学基金项目(52322409);国家自然科学基金项目(52127802);国家自然科学基金项目(52271137)
通讯作者: 梁淑华,liangsh@xaut.edu.cn,主要从事导电材料成型技术、难熔金属及粉末冶金技术等方面的研究
Corresponding author: LIANG Shuhua, professor, Tel: (029)82312185, E-mail: liangsh@xaut.edu.cn
作者简介: 姜伊辉,男,1985年生,教授,博士
图1  铜基复合材料的反应铸造技术[10,14,18,19]
图2  铜基复合材料的喷射沉积技术 [21,22]
图3  铜基复合材料的增材制造技术[28,33]
图4  铜基复合材料的固相原位制备技术[39,45,56]
图5  铜基复合材料的液-固原位制备技术[61~63]
图6  微米尺度增强相对铜基复合材料力学性能影响及其机理[19,69]
图7  铜基复合材料的载流摩擦磨损和耐电接触机理[75,79]
图8  纳米尺度增强相对铜基复合材料力学和导电性能的影响[27,71,82]
图9  常见铜基复合材料的抗拉强度与导电率对应关系[3,23,27,33,34,36,39,63,69,78,86,88~93]
图10  微纳双尺度颗粒混杂增强铜基复合材料微观组织及其性能[96]
图11  多元混杂增强铜基复合材料的微观组织和性能[83,97,99]
图12  非连通构型复合材料的微观组织及其强塑性[105,107]
图13  连通构型复合材料的微观组织及强塑性[108,109]
[1] Xiao Z, Ding Y J, Wang Z J, et al. Research and development of advanced copper matrix composites [J]. Trans. Nonferrous Met. Soc. China, 2024, 34: 3789
doi: 10.1016/S1003-6326(24)66641-0
[2] Zhang X H, Zhang Y, Tian B H, et al. Review of nano-phase effects in high strength and conductivity copper alloys [J]. Nanotechnol. Rev., 2019, 8: 383
doi: 10.1515/ntrev-2019-0034
[3] Zhang X H, Li X X, Chen H, et al. Investigation on microstructure and properties of Cu-Al2O3 composites fabricated by a novel in-situ reactive synthesis [J]. Mater. Des., 2016, 92: 58
doi: 10.1016/j.matdes.2015.12.018
[4] Minneci R P, Lass E A, Bunn J R, et al. Copper-based alloys for structural high-heat-flux applications: A review of development, properties, and performance of Cu-rich Cu-Cr-Nb alloys [J]. Int. Mater. Rev., 2021, 66: 394
doi: 10.1080/09506608.2020.1821485
[5] Chen M X, Li X P, Ji G, et al. Novel composite powders with uniform TiB2 nano-particle distribution for 3D printing [J]. Appl. Sci., 2017, 7: 250
doi: 10.3390/app7030250
[6] Kini A R, Maischner D, Weisheit A, et al. In-situ synthesis via laser metal deposition of a lean Cu-3.4Cr-0.6Nb (at%) conductive alloy hardened by Cr nano-scale precipitates and by Laves phase micro-particles [J]. Acta Mater., 2020, 197: 330
doi: 10.1016/j.actamat.2020.07.035
[7] Zhang Z, Chen D L. Consideration of Orowan strengthening effect in particulate-reinforced metal matrix nanocomposites: A model for predicting their yield strength [J]. Scr. Mater., 2006, 54: 1321
doi: 10.1016/j.scriptamat.2005.12.017
[8] Zhou M Y, Ren L B, Fan L L, et al. Progress in research on hybrid metal matrix composites [J]. J. Alloys Compd., 2020, 838: 155274
doi: 10.1016/j.jallcom.2020.155274
[9] Guo Q, Li Z Q, Zhao L, et al. Metal matrix composites with microstructural architectures [J]. Mater. China, 2016, 35: 641
[9] 郭 强, 李志强, 赵 蕾 等. 金属材料的构型复合化 [J]. 中国材料进展, 2016, 35: 641
[10] Zou C, Kang H, Li R, et al. The effect of rotating magnetic field on the microstructure of in situ TiB2/Cu composites [J]. IOP Conf. Ser.: Mater. Sci. Eng., 2016, 117: 012043
[11] Arunachalam R, Krishnan P K, Muraliraja R. A review on the production of metal matrix composites through stir casting—Furnace design, properties, challenges, and research opportunities [J]. J. Manuf. Processes, 2019, 42: 213
doi: 10.1016/j.jmapro.2019.04.017
[12] Wang T M, Zou C L, Chen Z N, et al. In situ synthesis of TiB2 particulate reinforced copper matrix composite with a rotating magnetic field [J]. Mater. Des., 2015, 65: 280
doi: 10.1016/j.matdes.2014.09.025
[13] Feng J, Liang S H, Song K X, et al. Micro-nano dual-scale particle-reinforced TiB2/Cu-0.5Cr composites prepared by vacuum arc melting [J]. J. Mater. Eng. Perform., 2020, 29: 3353
doi: 10.1007/s11665-020-04850-6
[14] Pan S H, Zheng T Q, Yao G C, et al. High-strength and high-conductivity in situ Cu-TiB2 nanocomposites [J]. Mater. Sci. Eng., 2022, A831: 141952
[15] Guo M X, Shen K, Wang M P. Effect of in situ reaction conditions on the microstructure changes of Cu-TiB2 alloys by combining in situ reaction and rapid solidification [J]. Mater. Chem. Phys., 2012, 131: 589
doi: 10.1016/j.matchemphys.2011.10.019
[16] Lee A K, Sanchez-Caldera L E, Chun J H, et al. Material with novel compositions and fine Microstructljres produced via the mixalloy process [J]. MRS Online Proc. Libr., 1988, 132: 87
doi: 10.1557/PROC-132-87
[17] Guo M X, Shen K, Wang M P. Relationship between microstructure, properties and reaction conditions for Cu-TiB2 alloys prepared by in situ reaction [J]. Acta Mater., 2009, 57: 4568
doi: 10.1016/j.actamat.2009.06.030
[18] Liang S H, Li W Z, Jiang Y H, et al. Microstructures and properties of hybrid copper matrix composites reinforced by TiB whiskers and TiB2 particles [J]. J. Alloys Compd., 2019, 797: 589
doi: 10.1016/j.jallcom.2019.05.129
[19] Cao F, Zhang X D, Jiang Y H, et al. Effect of different rare earths on microstructures and tensile strength of in situ hybrid reinforced (TiB2p + TiBw)/Cu composites [J]. Mater. Charact., 2022, 184: 111624
doi: 10.1016/j.matchar.2021.111624
[20] Lee J, Kim N J, Jung J Y, et al. The influence of reinforced particle fracture on strengthening of spray formed Cu-TiB2 composite [J]. Scr. Mater., 1998, 39: 1063
doi: 10.1016/S1359-6462(98)00246-2
[21] Lee J, Jung J Y, Lee E S, et al. Microstructure and properties of titanium boride dispersed Cu alloys fabricated by spray forming [J]. Mater. Sci. Eng., 2000, A277: 274
[22] Chen D, Jiang Y H, Li Y F, et al. In situ TiB2/Cu composites fabricated by spray deposition using solid-liquid and liquid-liquid reactions [J]. Trans. Nonferrous Met. Soc. China, 2020, 30: 1849
doi: 10.1016/S1003-6326(20)65344-4
[23] Tu J P, Wang N Y, Yang Y Z, et al. Preparation and properties of TiB2 nanoparticle reinforced copper matrix composites by in situ processing [J]. Mater. Lett., 2002, 52: 448
doi: 10.1016/S0167-577X(01)00442-6
[24] Zheng R G, Zhan Z J, Wang W K. Wear behavior of Cu-La2O3 composite with or without electrical current [J]. Wear, 2010, 268: 72
doi: 10.1016/j.wear.2009.06.026
[25] Jeyaprakash N, Saravana Kumar M, Yang C H. Enhanced nano-level mechanical responses on additively manufactured Cu-Cr-Zr copper alloy containing Cu2O nano precipitates [J]. J. Alloys Compd., 2023, 930: 167425
doi: 10.1016/j.jallcom.2022.167425
[26] Liu Y G, Zhang J Q, Sun Q, et al. Laser powder bed fusion of copper matrix iron particle reinforced nanocomposite with high strength and high conductivity [J]. J. Mater. Sci. Technol., 2023, 134: 50
doi: 10.1016/j.jmst.2022.06.007
[27] Liu Y A, Zhang J Q, Niu R M, et al. Manufacturing of high strength and high conductivity copper with laser powder bed fusion [J]. Nat. Commun., 2024, 15: 1283
doi: 10.1038/s41467-024-45732-y pmid: 38347023
[28] Wang G, Ouyang H, Fan C, et al. The origin of high-density dislocations in additively manufactured metals [J]. Mater. Res. Lett., 2020, 8(8): 283
doi: 10.1080/21663831.2020.1751739
[29] Stašić J, Božić D. Obtaining of reinforced Cu-Ti, Cu-Ti-TiB2 foils through green compact laser sintering [J]. J. Alloys Compd., 2018, 762: 231
doi: 10.1016/j.jallcom.2018.05.135
[30] Tang X P, Chen X H, Sun F J, et al. The current state of CuCrZr and CuCrNb alloys manufactured by additive manufacturing: A review [J]. Mater. Des., 2022, 224: 111419
doi: 10.1016/j.matdes.2022.111419
[31] Teasley T, Gradl P, Garcia M B, et al. Extreme environment hot fire durability of post processed additively manufactured GRCop-alloy combustion chambers [A]. Proceedings of the AIAA Propulsion and Energy 2021 Forum [C]. AIAA (August 9-11, 2021, Virtual Event), 2021: 3233
[32] Seltzman A H, Wukitch S J. Fracture characteristics and heat treatment of laser powder bed fusion additively manufactured GRCop-84 copper [J]. Mater. Sci. Eng., 2021, A827: 141690
[33] Wang L Q, Qu S, Fu H L, et al. Additively manufactured copper alloy with heterogeneous nanoprecipitates-dislocation architecture for superior strength-ductility-conductivity synergy [J]. Addit. Manuf., 2024, 84: 104100
[34] Cao F, Dong G Z, Jiang Y H, et al. Effect of La addition on microstructures and properties of TiB2(-TiB)/Cu hybrid composites prepared by in situ reaction [J]. Mater. Sci. Eng., 2020, A789: 139605
[35] Zhang S R, Kang H J, Li R G, et al. Microstructure evolution, electrical conductivity and mechanical properties of dual-scale Cu5Zr/ZrB2 particulate reinforced copper matrix composites [J]. Mater. Sci. Eng., 2019, A762: 138108
[36] Zou C L, Kang H J, Wang W, et al. Effect of La addition on the particle characteristics, mechanical and electrical properties of in situ Cu-TiB2 composites [J]. J. Alloys Compd., 2016, 687: 312
doi: 10.1016/j.jallcom.2016.06.129
[37] Zhai Q M, Xu W Q, Wang J H, et al. Study status of in-situ reaction copper matrix composite [J]. Mater. Heat Treat., 2006, 35(14): 58
[37] 翟启明, 徐文清, 王冀恒 等. 原位反应铜基复合材料的研究现状 [J]. 热加工工艺, 2006, 35(14): 58
[38] Guo M X, Wang M P, Li Z, et al. The studies of TiB2/Cu metal matrix composites [J]. Mater. Rep., 2004, 18(8): 39
[38] 郭明星, 汪明朴, 李 周 等. TiB2/Cu金属基复合材料的研究 [J]. 材料导报, 2004, 18(8): 39
[39] Yan Y F, Kou S Q, Yang H Y, et al. Ceramic particles reinforced copper matrix composites manufactured by advanced powder metallurgy: preparation, performance, and mechanisms [J]. Int. J. Extrem. Manuf., 2023, 5: 032006
[40] Saheb N, Iqbal Z, Khalil A, et al. Spark plasma sintering of metals and metal matrix nanocomposites: A review [J]. J. Nanomater., 2012, 2012: 983470
doi: 10.1155/jona.v2012.1
[41] Jiang X S, Liu W X, Li Y J, et al. Microstructures and mechanical properties of Cu/Ti3SiC2/C/graphene nanocomposites prepared by vacuum hot-pressing sintering and hot isostatic pressing [J]. Composites, 2018, 141B: 203
[42] Tian B H, Liu P, Song K X, et al. Microstructure and properties at elevated temperature of a nano-Al2O3 particles dispersion-strengthened copper base composite [J]. Mater. Sci. Eng., 2006, A435-436: 705
[43] Zhuo H O, Tang J C, Ye N. A novel approach for strengthening Cu-Y2O3 composites by in situ reaction at liquidus temperature [J]. Mater. Sci. Eng., 2013, A584: 1
[44] Xiang Z Q, Li Z, Lei Q, et al. High temperature mechanical behavior of alumina dispersion strengthened copper alloy with high content of alumina [J]. Trans. Nonferrous Met. Soc. China, 2015, 25: 444
doi: 10.1016/S1003-6326(15)63622-6
[45] Lan T, Jiang Y H, Zhang X J, et al. Competitive precipitation behavior of hybrid reinforcements in copper matrix composites fabricated by powder metallurgy [J]. Int. J. Miner. Metall. Mater., 2021, 28: 1090
doi: 10.1007/s12613-020-2052-x
[46] Jiang Y H, Wang C, Liang S H, et al. TiB2(-TiB)/Cu in-situ composites prepared by hot-press with the sintering temperature just beneath the melting point of copper [J]. Mater. Charact., 2016, 121: 76
doi: 10.1016/j.matchar.2016.09.038
[47] Guo X F, Jia L, Lu Z L, et al. Preparation of Cu/CrB2 composites with well-balanced mechanical properties and electrical conductivity by ex-situ powder metallurgy [J]. J. Mater. Res. Technol., 2022, 17: 1605
doi: 10.1016/j.jmrt.2022.01.112
[48] Jiang Y H, Shi Y Y, Zhang X J, et al. Copper matrix composite with bimodal microstructures fabricated by liquid nitrogen temperature rolling [J]. Mater. Sci. Technol., 2022, 38: 654
doi: 10.1080/02670836.2022.2062651
[49] Zhang X K, Lei Q, Liu B, et al. Enhanced softening resistance and mechanical properties of Mo2C particle-reinforced Cu-matrix composites [J]. Compos. Struct., 2023, 305: 116503
doi: 10.1016/j.compstruct.2022.116503
[50] Ren J Q, Liang S H, Jiang Y H, et al. Research on the microstructure and properties of in situ (TiB2-TiB)/Cu composites [J]. Acta Metall. Sin., 2019, 55: 126
[50] 任建强, 梁淑华, 姜伊辉 等. 原位(TiB2-TiB)/Cu复合材料组织与性能研究 [J]. 金属学报, 2019, 55: 126
doi: 10.11900/0412.1961.2017.00532
[51] Huang F, Wang H, Yang B, et al. Uniformly dispersed Y2O3 nanoparticles in nanocrystalline copper matrix via multi-step ball milling and reduction process [J]. Mater. Lett., 2019, 242: 119
doi: 10.1016/j.matlet.2019.01.120
[52] Guo M X, Wang M P. The relationship among microstructure evolution, mechanical property and in situ reaction mechanisms in preparing Cu-1.6wt% TiB2 alloys [J]. Mater. Chem. Phys., 2013, 138: 95
doi: 10.1016/j.matchemphys.2012.11.014
[53] Li T J, Wang Y Q, Yang M, et al. High strength and conductivity copper matrix composites reinforced by in-situ graphene through severe plastic deformation processes [J]. J. Alloys Compd., 2021, 851: 156703
doi: 10.1016/j.jallcom.2020.156703
[54] Wei X, Tao J M, Hu Y, et al. Enhancement of mechanical properties and conductivity in carbon nanotubes (CNTs)/Cu matrix composite by surface and intratube decoration of CNTs [J]. Mater. Sci. Eng., 2021, A816: 141248
[55] Zhao N Q, Guo S Y, Zhang X, et al. Progress on graphene/copper composites focusing on reinforcement configuration design: A review [J]. Acta Metall. Sin., 2021, 57: 1087
doi: 10.11900/0412.1961.2021.00120
[55] 赵乃勤, 郭斯源, 张 翔 等. 基于增强相构型设计的石墨烯/Cu复合材料研究进展 [J]. 金属学报, 2021, 57: 1087
doi: 10.11900/0412.1961.2021.00120
[56] Chen Y K, Zhang X, Liu E Z, et al. Fabrication of three-dimensional graphene/Cu composite by in-situ CVD and its strengthening mechanism [J]. J. Alloys Compd., 2016, 688: 69
[57] Zhang X, Zhao N Q, He C N. The superior mechanical and physical properties of nanocarbon reinforced bulk composites achieved by architecture design—A review [J]. Prog. Mater Sci., 2020, 113: 100672
doi: 10.1016/j.pmatsci.2020.100672
[58] Jiang L, Li Z Q, Fan G L, et al. The use of flake powder metallurgy to produce carbon nanotube (CNT)/aluminum composites with a homogenous CNT distribution [J]. Carbon, 2012, 50: 1993
doi: 10.1016/j.carbon.2011.12.057
[59] Li Z, Wang H T, Guo Q, et al. Regain strain-hardening in high-strength metals by nanofiller incorporation at grain boundaries [J]. Nano Lett., 2018, 18(10): 6255
doi: 10.1021/acs.nanolett.8b02375 pmid: 30193069
[60] Shukla A K, Samuel M G, Suresh Kumar R, et al. Effect of powder oxidation on densification and properties of vacuum hot pressed Cu-Cr-Nb alloy [J]. Mater. Sci. Eng., 2013, A561: 452
[61] Shi H, Cao F, Wang T L, et al. A well-balanced strength and electrical conductivity in rolled composite prepared by in-situ TiB2p/Cu composite powder [J]. J. Mater. Res. Technol., 2023, 27: 1
doi: 10.1016/j.jmrt.2023.09.193
[62] Shi H, Zhao Y, Gao H B, et al. In-situ spherical TiB2/Cu composite powder: A new method of liquid phase reaction coupled with gas atomization [J]. Mater. Charact., 2022, 191: 112096
doi: 10.1016/j.matchar.2022.112096
[63] Shi H, Cao F, Zhang H D, et al. Densification behavior, mechanical and electrical properties of in-situ TiB2p/Cu composite powder via vacuum hot pressing [J]. Mater. Charact., 2023, 202: 113004
doi: 10.1016/j.matchar.2023.113004
[64] Wang L, Zheng C, Kombaiah B, et al. Contrasting roles of Laves_Cr2Nb precipitates on the creep properties of novel CuCr-NbZr alloys [J]. Mater. Sci. Eng., 2020, A779: 139110
[65] Lv X Q, Liu Z M, Lei T, et al. Effect of heat treatment on Cr2Nb phase and properties of spark plasma sintered Cu-2Cr-1Nb alloy [J]. Materials, 2020, 13: 2860
doi: 10.3390/ma13122860
[66] Cao F, Zhang X D, Cai P T, et al. Effect of reaction temperature and heat treatment time on electrical and mechanical performance of TiB2 particles and TiB whiskers reinforced copper matrix composites [J]. Metals, 2022, 12: 592
doi: 10.3390/met12040592
[67] Zai X F, Chen S Q, Wu H, et al. Preparation of spherical high-purity Zr powders by gas atomization without crucible [J]. Chin. J. Rare Met., 2018, 42: 864
[67] 宰雄飞, 陈仕奇, 吴 宏 等. 无坩埚熔炼气雾化技术制备高纯球形锆粉 [J]. 稀有金属, 2018, 42: 864
[68] Fu J W, Nie Q Q, Qiu W X, et al. Morphology, orientation relationships and formation mechanism of TiN in Fe-17Cr steel during solidification [J]. Mater. Charact., 2017, 133: 176
doi: 10.1016/j.matchar.2017.10.001
[69] Bahador A, Umeda J, Yamanoglu R, et al. Deformation mechanism and enhanced properties of Cu-TiB2 composites evaluated by the in-situ tensile test and microstructure characterization [J]. J. Alloys Compd., 2020, 847: 156555
doi: 10.1016/j.jallcom.2020.156555
[70] Chen Z, Qiu M L, Yang J J, et al. Thermal stability and grain growth kinetics of ultrafine-grained W with various amount of La2O3 addition [J]. Metall. Mater. Trans., 2020, 51A: 4113
[71] Pan S H, Guan Z Y, Yao G C, et al. Study on electrical behaviour of copper and its alloys containing dispersed nanoparticles [J]. Curr. Appl. Phys., 2019, 19: 452
doi: 10.1016/j.cap.2019.01.016
[72] Zou C L, Chen Z N, Guo E Y, et al. A nano-micro dual-scale particulate-reinforced copper matrix composite with high strength, high electrical conductivity and superior wear resistance [J]. RSC Adv., 2018, 8: 30777
doi: 10.1039/C8RA06020G
[73] Jin B, Chen G Y, He Y Y, et al. Lubrication properties of graphene under harsh working conditions [J]. Mater. Today Adv., 2023, 18: 100369
[74] Zhang S R, Kang H J, Wang Z C, et al. Microstructure and properties of dual-scale particulate reinforced copper matrix composites with superior comprehensive properties [J]. J. Alloys Compd., 2021, 860: 157888
doi: 10.1016/j.jallcom.2020.157888
[75] Jin B, Zhao J, He Y Y, et al. High-quality ultra-flat reduced graphene oxide nanosheets with super-robust lubrication performances [J]. Chem. Eng. J., 2022, 438: 135620
doi: 10.1016/j.cej.2022.135620
[76] Luan T Y, Gao T C, Zhao J M, et al. Properties and microstructure characterisation of high-strength, high-conductivity and high-resistance to arc ablation Cu-0.6Te-0.3Cr-0.15Zr-0.008P alloy [J]. Mater. Charact., 2024, 214: 114110
doi: 10.1016/j.matchar.2024.114110
[77] Dong L L, Li L, Li X, et al. Enhancing mechanisms of arc-erosion resistance for copper tungsten electrical contact using reduced graphene oxides in situ modified by copper nanoparticles [J]. Int. J. Refract. Met. Hard Mater., 2022, 108: 105934
doi: 10.1016/j.ijrmhm.2022.105934
[78] Fu Q Q, Li B, Gao M Q, et al. Quantitative mechanisms behind the high strength and electrical conductivity of Cu-Te alloy manufactured by continuous extrusion [J]. J. Mater. Sci. Technol., 2022, 121: 9
doi: 10.1016/j.jmst.2021.12.046
[79] Li S L, Guo X H, Zhang S L, et al. Arc erosion behavior of TiB2/Cu composites with single-scale and dual-scale TiB2 particles [J]. Nanotechnol. Rev., 2019, 8: 619
doi: 10.1515/ntrev-2019-0054
[80] Feng J, Liang S H, Guo X H, et al. Electrical conductivity anisotropy of copper matrix composites reinforced with SiC whiskers [J]. Nanotechnol. Rev., 2019, 8: 285
doi: 10.1515/ntrev-2019-0027
[81] Liu J B, Zeng Y W, Meng L. Crystal structure and morphology of a rare-earth compound in Cu-12wt.% Ag [J]. J. Alloys Compd., 2009, 468: 73
doi: 10.1016/j.jallcom.2007.12.070
[82] Li J, Liu B, Fang Q H, et al. Atomic-scale strengthening mechanism of dislocation-obstacle interaction in silicon carbide particle-reinforced copper matrix nanocomposites [J]. Ceram. Int., 2017, 43: 3839
doi: 10.1016/j.ceramint.2016.12.040
[83] Liu N, Zhang Q Q, Zhang H Y, et al. Experimental verification and numerical analysis on plastic deformation and mechanical properties of the in-situ TiB2 homogeneous composites and TiB2/Cu network composites prepared by powder metallurgy [J]. J. Alloys Compd., 2022, 920: 165897
doi: 10.1016/j.jallcom.2022.165897
[84] Zhang X X, Yuan Y L, Zhao S Q, et al. Microstructure stability, softening temperature and strengthening mechanism of pure copper, CuCrZr and Cu-Al2O3 up to 1000 oC [J]. Nucl. Mater. Energy, 2022, 30: 101123
[85] Li Z, Zhang D. The self-stimulation effect for high-performance metal matrix composites [J]. Mater. China, 2023, 42: 605
[85] 李 赞, 张 荻. 金属基复合材料的内源性效应 [J]. 中国材料进展, 2023, 42: 605
[86] Ke J G, Liu R, Xie Z M, et al. Ultrahigh strength, thermal stability and high thermal conductivity in hierarchical nanostructured Cu-W alloy [J]. Acta Mater., 2024, 264: 119547
doi: 10.1016/j.actamat.2023.119547
[87] Li N Y, Chang Y Q, Li M Y, et al. Enhanced mechanical property by introducing bimodal grains structures in Cu-Ta alloys fabricated by mechanical alloying [J]. J. Mater. Sci. Technol., 2024, 172: 104
doi: 10.1016/j.jmst.2023.06.056
[88] Zhang X H, Xiong D B, Liu Y Z, et al. Multilayer graphene interface enabled ultrahigh extensibility for high performance bulk nanostructured copper [J]. Acta Mater., 2024, 267: 119710
doi: 10.1016/j.actamat.2024.119710
[89] Cao F, Zhang X D, Dong G Z, et al. Microstructures and properties of in situ (TiB2p + TiBw)/Cu composites with different Ce content [J]. Adv. Eng. Mater., 2022, 24: 2200251
doi: 10.1002/adem.v24.8
[90] Zhou D S, Wang X K, Zeng W, et al. Doping Ti to achieve microstructural refinement and strength enhancement in a high volume fraction Y2O3 dispersion strengthened Cu [J]. J. Alloys Compd., 2018, 753: 18
doi: 10.1016/j.jallcom.2018.04.224
[91] Jia Y L, Zhou K, Sun W T, et al. Enhancement mechanisms of mechanical, electrical and thermal properties of carbon nanotube-copper composites: A review [J]. J. Mater. Res. Technol., 2024, 32: 1395
doi: 10.1016/j.jmrt.2024.07.181
[92] Zeng W, Xie J W, Zhou D S, et al. Bulk Cu-NbC nanocomposites with high strength and high electrical conductivity [J]. J. Alloys Compd., 2018, 745: 55
doi: 10.1016/j.jallcom.2018.02.215
[93] Xie J W, Zeng W, Zhou D S, et al. Microstructure and properties of a nanocrystalline Cu-Al-NbC composite with high strength and good conductivity [J]. Mater. Lett., 2018, 214: 174
doi: 10.1016/j.matlet.2017.12.009
[94] Cao J M, Li F J, Yang Q C, et al. A review on interfacial structure optimization and its mechanism on the properties of carbon reinforced metal-matrix composites [J]. Compos. Interfaces, 2023, 30(5): 543
doi: 10.1080/09276440.2023.2179248
[95] Pan Y, Xiao S Q, Lu X, et al. Fabrication, mechanical properties and electrical conductivity of Al2O3 reinforced Cu/CNTs composites [J]. J. Alloys Compd., 2019, 782: 1015
doi: 10.1016/j.jallcom.2018.12.222
[96] Zhang X D, Jiang Y H, Cao F, et al. Hybrid effect on mechanical properties and high-temperature performance of copper matrix composite reinforced with micro-nano dual-scale particles [J]. J. Mater. Sci. Technol., 2024, 172: 94
doi: 10.1016/j.jmst.2023.06.054
[97] Zhou T, Chen W, Jiang Y B, et al. Microstructure, properties and reaction kinetics of a Cu-Al2O3-TiB2 alloy prepared by a new liquid phase in-situ reaction technology [J]. J. Mater. Res. Technol., 2023, 26: 4024
doi: 10.1016/j.jmrt.2023.08.156
[98] Long F, Guo X H, Song K X, et al. An internal-oxidation-based strategy induced high-density alumina in-situ nanoprecipitation and carbon nanotube interface optimization for co-reinforcing copper matrix composites [J]. Composites, 2022, 229B: 109455
[99] Xu K, Chen X H, Zhou H L, et al. Preparation and formation mechanism of CNTs/Cu-Al2O3 composite powders by in situ CVD using internally-oxidized Cu-Al alloy powders [J]. Mater. Lett., 2019, 254(1): 390
doi: 10.1016/j.matlet.2019.07.018
[100] Nageswaran G, Natarajan S, Ramkumar K R. Synthesis, structural characterization, mechanical and wear behaviour of Cu-TiO2-Gr hybrid composite through stir casting technique [J]. J. Alloys Compd., 2018, 768: 733
doi: 10.1016/j.jallcom.2018.07.288
[101] Fan G L, Guo Z Q, Tan Z Q, et al. Architecture design strategies and strengthening-toughening mechanisms of metal matrix composites [J]. Acta Metall. Sin., 2022, 58: 1416
doi: 10.11900/0412.1961.2022.00355
[101] 范根莲, 郭峙岐, 谭占秋 等. 金属材料的构型化复合与强韧化 [J]. 金属学报, 2022, 58: 1416
doi: 10.11900/0412.1961.2022.00355
[102] Wegst U G K, Bai H, Saiz E, et al. Bioinspired structural material [J]. Nat. Mater., 2015, 14: 23
doi: 10.1038/nmat4089
[103] Zhao L, Zheng W S, Hu Y, et al. Heterostructured metal matrix composites for structural applications: A review [J]. J. Mater. Sci., 2024, 59: 9768
doi: 10.1007/s10853-023-09300-x
[104] Cao M, Xiong D B, Yang L, et al. Ultrahigh electrical conductivity of graphene embedded in metals [J]. Adv. Funct. Mater., 2019, 29: 1806792
doi: 10.1002/adfm.v29.17
[105] Han F, Jiang Y H, Cao F, et al. Role of gradient heterogeneous interfaces in synergetic strengthening and toughening of layered CuCrZr/Cu composites [J]. Mater. Sci. Eng., 2023, A885: 145613
[106] Cao F, Cai L, Han F, et al. Effects of the layer thickness ratio on the microstructure and mechanical properties of Cu-TiB2/Cu layered composites [J]. Foundry Technol., 2024, 45: 61
[106] 曹 飞, 蔡 磊, 韩 非 等. 层厚比对Cu-TiB2/Cu层状复合材料微观组织和力学性能的影响 [J]. 铸造技术, 2024, 45: 61
[107] Xiong D B, Cao M, Guo Q, et al. Graphene-and-copper artificial nacre fabricated by a preform impregnation process: Bioinspired strategy for strengthening-toughening of metal matrix composite [J]. ACS Nano, 2015, 9: 6934
doi: 10.1021/acsnano.5b01067
[108] Yang Z Y, Wang L D, Cui Y, et al. High strength and ductility of graphene-like carbon nanosheet/copper composites fabricated directly from commercial oleic acid coated copper powders [J]. Nanoscale, 2018, 10: 16990
doi: 10.1039/c8nr04451a pmid: 30183044
[109] Zhang X, Shi C S, Liu E Z, et al. Achieving high strength and high ductility in metal matrix composites reinforced with a discontinuous three-dimensional graphene-like network [J]. Nanoscale, 2017, 9: 11929
doi: 10.1039/c6nr07335b pmid: 28786440
[110] Jiang Y H, Han L, Xu Y Q, et al. Arc erosion behaviour of in-situ TiB2/Cu composites with a three-dimensional network structure [J]. Mater. Res. Express, 2022, 9: 046503
[1] 孙军, 刘刚, 杨冲, 张鹏, 薛航. 耐热铝合金:组织设计与合金制备[J]. 金属学报, 2025, 61(4): 521-525.
[2] 熊天英, 王吉强. 中国科学院金属研究所冷喷涂技术研究进展[J]. 金属学报, 2023, 59(4): 537-546.
[3] 徐流杰, 宗乐, 罗春阳, 焦照临, 魏世忠. 难熔高熵合金的强韧化途径与调控机理[J]. 金属学报, 2022, 58(3): 257-271.
[4] 李少杰, 金剑锋, 宋宇豪, 王明涛, 唐帅, 宗亚平, 秦高梧. “工艺-组织-性能”模拟研究Mg-Gd-Y合金混晶组织[J]. 金属学报, 2022, 58(1): 114-128.
[5] 赵乃勤, 郭斯源, 张翔, 何春年, 师春生. 基于增强相构型设计的石墨烯/Cu复合材料研究进展[J]. 金属学报, 2021, 57(9): 1087-1106.
[6] 高一涵, 刘刚, 孙军. 耐热铝基合金研究进展:微观组织设计与析出策略[J]. 金属学报, 2021, 57(2): 129-149.
[7] 张国庆,张义文,郑亮,彭子超. 航空发动机用粉末高温合金及制备技术研究进展[J]. 金属学报, 2019, 55(9): 1133-1144.
[8] 任建强, 梁淑华, 姜伊辉, 杜翔. 原位(TiB2-TiB)/Cu复合材料组织与性能研究[J]. 金属学报, 2019, 55(1): 126-132.
[9] 卢磊 卢柯. 纳米孪晶金属材料[J]. 金属学报, 2010, 46(11): 1422-1427.