| 低合金化Mg-Ag镁空气电池阳极材料的电化学行为和放电性能 |
郝旭邦1, 程伟丽1,2( ), 李戬2, 王利飞1, 崔泽琴1, 闫国庆3, 翟凯3, 余晖4 |
1 太原理工大学 材料科学与工程学院 太原 030024 2 青海大学 盐湖化工大型系列研究设施 西宁 810016 3 山西瑞格金属新材料有限公司 运城 043800 4 河北工业大学 材料科学与工程学院 天津 300132 |
|
| Electrochemical Behavior and Discharge Performance of a Low-Alloyed Mg-Ag Alloy as Anode for Mg-Air Battery |
HAO Xubang1, CHENG Weili1,2( ), LI Jian2, WANG Lifei1, CUI Zeqin1, YAN Guoqing3, ZHAI Kai3, YU Hui4 |
1 School of Materials Science and Engineering, Taiyuan University of Technology, Taiyuan 030024, China 2 Salt Lake Chemical Engineering Research Complex, Qinghai University, Xining 810016, China 3 Shanxi Regal Advanced Material Co. Ltd., Yuncheng 043800, China 4 School of Materials Science and Engineering, Hebei University of Technology, Tianjin 300132, China |
引用本文:
郝旭邦, 程伟丽, 李戬, 王利飞, 崔泽琴, 闫国庆, 翟凯, 余晖. 低合金化Mg-Ag镁空气电池阳极材料的电化学行为和放电性能[J]. 金属学报, 2025, 61(6): 837-847.
Xubang HAO,
Weili CHENG,
Jian LI,
Lifei WANG,
Zeqin CUI,
Guoqing YAN,
Kai ZHAI,
Hui YU.
Electrochemical Behavior and Discharge Performance of a Low-Alloyed Mg-Ag Alloy as Anode for Mg-Air Battery[J]. Acta Metall Sin, 2025, 61(6): 837-847.
| 1 |
Zou Q, Le Q C, Chen X R, et al. The influence of Ga alloying on Mg-Al-Zn alloys as anode material for Mg-air primary batteries [J]. Electrochim. Acta, 2022, 401: 139372
|
| 2 |
Ma B J, Tan C, Ouyang L Z, et al. Microstructure and discharge performance of Mg-La alloys as the anodes for primary magnesium-air batteries [J]. J. Alloys Compd., 2022, 918: 165803
|
| 3 |
Bao J X, Sha J C, Li L H, et al. Electrochemical properties and discharge performance of Mg-3Sn-xCa alloy as a novel anode for Mg-air battery [J]. J. Alloys Compd., 2023, 934: 167849
|
| 4 |
Tong F L, Chen X Z, Teoh T E, et al. Mg-Sn alloys as anodes for magnesium-air batteries [J]. J. Electrochem. Soc., 2021, 168: 110531
|
| 5 |
Chen X R, Liao Q Y, Le Q C, et al. The influence of samarium (Sm) on the discharge and electrochemical behaviors of the magnesium alloy AZ80 as an anode for the Mg-air battery [J]. Electrochim. Acta, 2020, 348: 136315
|
| 6 |
Chen X R, Zou Q, Le Q C, et al. The quasicrystal of Mg-Zn-Y on discharge and electrochemical behaviors as the anode for Mg-air battery [J]. J. Power Sources, 2020, 451: 227807
|
| 7 |
Chen X R, Zou Q, Shi Z M, et al. The discharge performance of an as-extruded Mg-Zn-La-Ce anode for the primary Mg-air battery [J]. Electrochim. Acta, 2022, 404: 139763
|
| 8 |
Gong C W, Yan X, He X Z, et al. Influence of homogenization treatment on corrosion behavior and discharge performance of the Mg-2Zn-1Ca anodes for primary Mg-air batteries [J]. Mater. Chem. Phys., 2022, 280: 125802
|
| 9 |
Jiang P L, Li D P, Hou R Q, et al. A micro-alloyed Mg-Zn-Ge alloy as promising anode for primary Mg-air batteries [J]. J. Magnes. Alloy., doi: 10.1016/j.jma.2023.05.004
|
| 10 |
Jiang P L, Blawert C, Hou R Q, et al. Microstructural influence on corrosion behavior of MgZnGe alloy in NaCl solution [J]. J. Alloys Compd., 2019, 783: 179
|
| 11 |
Liu X, Xue J L, Zhang P J, et al. Effects of the combinative Ca, Sm and La additions on the electrochemical behaviors and discharge performance of the as-extruded AZ91 anodes for Mg-air batteries [J]. J. Power Sources, 2019, 414: 174
|
| 12 |
Chen X R, Venezuela J, Shi Z M, et al. Tailoring the discharge performance of extruded Mg-Sm-Al anode for Mg-air battery applications via control of Al content [J]. Mater. Today Energy, 2023, 36: 101363
|
| 13 |
Deng M, Höche D, Lamaka S V, et al. Mg-Ca binary alloys as anodes for primary Mg-air batteries [J]. J. Power Sources, 2018, 396: 109
|
| 14 |
Xiao L R, Chen X F, Wei K, et al. Effect of dislocation configuration on Ag segregation in subgrain boundary of a Mg-Ag alloy [J]. Scr. Mater., 2021, 191: 219
|
| 15 |
Zerankeshi M M, Alizadeh R. Ag-incorporated biodegradable Mg alloys [J]. Materialia, 2022, 23: 101445
|
| 16 |
Shangguan F E, Cheng W L, Chen Y H, et al. Elucidating the dependence of electrochemical behavior and discharge performance on the grain structure of lean Mg-0.3Bi-0.3Ag-0.3In anodes in primary Mg-air battery [J]. J. Power Sources, 2023, 564: 232856
|
| 17 |
Zhang Z M, Yu K, Ren W W, et al. Microstructure of directly extruded Mg-1Zn-1Ca alloy and its corrosion behavior in SBF solution [J]. Acta Metall. Sin., 2015, 51: 985
doi: 10.11900/0412.1961.2014.00652
|
| 17 |
张忠明, 余 凯, 任伟伟 等. 正挤压态Mg-1Zn-1Ca合金的显微组织及其在SBF溶液中的腐蚀行为 [J]. 金属学报, 2015, 51: 985
|
| 18 |
Wang N G, Huang Y X, Liu J J, et al. AZ31 magnesium alloy with ultrafine grains as the anode for Mg-air battery [J]. Electrochim. Acta, 2021, 378: 138135
|
| 19 |
Wang L Q, Snihirova D, Deng M, et al. Insight into physical interpretation of high frequency time constant in electrochemical impedance spectra of Mg [J]. Corros. Sci., 2021, 187: 109501
|
| 20 |
Tong F L, Chen X Z, Wei S H, et al. Microstructure and battery performance of Mg-Zn-Sn alloys as anodes for magnesium-air battery [J]. J. Magnes. Alloy., 2021, 9: 1967
|
| 21 |
Gong C W, He X Z, Fang D Q, et al. Effect of second phases on discharge properties and corrosion behaviors of the Mg-Ca-Zn anodes for primary Mg-air batteries [J]. J. Alloys Compd., 2021, 861: 158493
|
| 22 |
Li S B, Li H, Zhao C C, et al. Effects of Ca addition on microstructure, electrochemical behavior and magnesium-air battery performance of Mg-2Zn-xCa alloys [J]. J. Electroanal. Chem., 2022, 904: 115944
|
| 23 |
Zhang Y W X, Fan L L, Guo Y Y, et al. Discharge performance of Mg-Y binary alloys as anodes for Mg-air batteries [J]. Electrochim. Acta, 2023, 460: 142594
|
| 24 |
Ma Y B, Li N, Li D Y, et al. Performance of Mg-14Li-1Al-0.1Ce as anode for Mg-air battery [J]. J. Power Sources, 2011, 196: 2346
|
| 25 |
Tong F L, Chen X Z, Wang Q, et al. Hypoeutectic Mg-Zn binary alloys as anode materials for magnesium-air batteries [J]. J. Alloys Compd., 2021, 857: 157579
|
| 26 |
Liu X, Xue J L. The role of Al2Gd cuboids in the discharge performance and electrochemical behaviors of AZ31-Gd anode for Mg-air batteries [J]. Energy, 2019, 189: 116314
|
| 27 |
Cheng W L, Gu X J, Cheng S M, et al. Discharge performance and electrochemical behaviors of the extruded Mg-2Bi-0.5Ca-0.5In alloy as anode for Mg-air battery [J]. Acta Metall. Sin., 2021, 57: 623
|
| 27 |
程伟丽, 谷雄杰, 成世明 等. 镁空气电池阳极用挤压态Mg-2Bi-0.5Ca-0.5In合金的放电性能和电化学行为 [J]. 金属学报, 2021, 57: 623
doi: 10.11900/0412.1961.2020.00272
|
| 28 |
Yang L, Shi Y Q, Shen L J, et al. Effect of Ag on cathodic activation and corrosion behaviour of Mg-Mn-Ag alloys [J]. Corros. Sci., 2021, 185: 109408
|
| 29 |
Liu X, Liu S Z, Xue J L. Discharge performance of the magnesium anodes with different phase constitutions for Mg-air batteries [J]. J. Power Sources, 2018, 396: 667
|
| 30 |
Gu X J, Cheng W L, Cheng S M, et al. Tailoring the microstructure and improving the discharge properties of dilute Mg-Sn-Mn-Ca alloy as anode for Mg-air battery through homogenization prior to extrusion [J]. J. Mater. Sci. Technol., 2021, 60: 77
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|