| Au-Pt合金凝固-固态相变微观组织演化相场法模拟 |
余东1, 马威龙2, 王亚莉1, 王锦程1( ) |
1 西北工业大学 凝固技术国家重点实验室 西安 710072 2 西安理工大学 材料科学与工程学院 西安 710048 |
|
| Phase Field Modeling of Microstructure Evolution During Solidification and Subsequent Solid-State Phase Transformation of Au-Pt Alloys |
YU Dong1, MA Weilong2, WANG Yali1, WANG Jincheng1( ) |
1 State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, China 2 College of Materials Science and Engineering, Xi'an University of Technology, Xi'an 710048, China |
引用本文:
余东, 马威龙, 王亚莉, 王锦程. Au-Pt合金凝固-固态相变微观组织演化相场法模拟[J]. 金属学报, 2025, 61(1): 109-116.
Dong YU,
Weilong MA,
Yali WANG,
Jincheng WANG.
Phase Field Modeling of Microstructure Evolution During Solidification and Subsequent Solid-State Phase Transformation of Au-Pt Alloys[J]. Acta Metall Sin, 2025, 61(1): 109-116.
| 1 |
Kurz W, Fisher D J, Trivedi R. Progress in modelling solidification microstructures in metals and alloys: dendrites and cells from 1700 to 2000[J]. Int. Mater. Rev., 2019, 64: 311
|
| 2 |
Kurz W, Rappaz M, Trivedi R. Progress in modelling solidification microstructures in metals and alloys. Part II: Dendrites from 2001 to 2018[J]. Int. Mater. Rev., 2021, 66: 30
|
| 3 |
Zhai W, Chang J, Geng D L, et al. Progress and prospect of solidification research for metallic materials[J]. Chin. J. Nonferrous Met., 2019, 29: 1953
|
| 3 |
翟 薇, 常 健, 耿德路 等. 金属材料凝固过程研究现状与未来展望[J]. 中国有色金属学报, 2019, 29: 1953
|
| 4 |
Liu F, Zhang X, Zhang Y B. Unified analysis of non-equilibrium solidification and solid-state phase transformations[J]. Acta Metall. Sin., 2018, 54: 701
doi: 10.11900/0412.1961.2018.00112
|
| 4 |
刘 峰, 张 旭, 张玉兵. 非平衡凝固与固态相变的一体化研究[J]. 金属学报, 2018, 54: 701
|
| 5 |
Ghosh S, Zollinger J, Zaloznik M, et al. Modeling of hierarchical solidification microstructures in metal additive manufacturing: challenges and opportunities[J]. Addit. Manuf., 2023, 78: 103845
|
| 6 |
Wang T M, Wei J J, Wang X D, et al. Progress and application of microstructure simulation of alloy solidification[J]. Acta Metall. Sin., 2018, 54: 193
doi: 10.11900/0412.1961.2017.00428
|
| 6 |
王同敏, 魏晶晶, 王旭东 等. 合金凝固组织微观模拟研究进展与应用[J]. 金属学报, 2018, 54: 193
doi: 10.11900/0412.1961.2017.00428
|
| 7 |
Wang J C, Guo C W, Li J J, et al. Recent progresses in competitive grain growth during directional solidification[J]. Acta Metall. Sin., 2018, 54: 657
doi: 10.11900/0412.1961.2017.00543
|
| 7 |
王锦程, 郭春文, 李俊杰 等. 定向凝固晶粒竞争生长的研究进展[J]. 金属学报, 2018, 54: 657
doi: 10.11900/0412.1961.2017.00543
|
| 8 |
Liu B C, Xu Q Y, Jing T, et al. Advances in multi-scale modeling of solidification and casting processes[J]. JOM, 2011, 63(4): 19
|
| 9 |
Warnken N, Larsson H, Reed R C. Coupled modelling of solidification and solution heat treatment of advanced single crystal nickel base superalloy[J]. Mater. Sci. Technol., 2009, 25: 179
|
| 10 |
Meng X N, Gao X H, Huang S, et al. Cross-scale modeling of MnS precipitation for steel solidification[J]. Metals, 2018, 8: 529
|
| 11 |
Shi R P, Khairallah S, Heo T W, et al. Integrated simulation framework for additively manufactured Ti-6Al-4V: Melt pool dynamics, microstructure, solid-state phase transformation, and microelastic response[J]. JOM, 2019, 71: 3640
|
| 12 |
Liu P W, Wang Z, Xiao Y H, et al. Integration of phase-field model and crystal plasticity for the prediction of process-structure-property relation of additively manufactured metallic materials[J]. Int. J. Plast., 2020, 128: 102670
|
| 13 |
Zhang Q, Wang J C, Zhang Y C, et al. Simulation of multi-grain solidification and subsequent spinodal decomposition by using phase field crystal model[J]. Acta Phys. Sin., 2011, 60: 088104
|
| 13 |
张 琪, 王锦程, 张亚丛 等. 多晶凝固及后续调幅分解过程的晶体相场法模拟[J]. 物理学报, 2011, 60: 088104
|
| 14 |
Kodama T, Nakai R, Goto K, et al. Preparation of an Au-Pt alloy free from artifacts in magnetic resonance imaging[J]. Magn. Reson. Imaging, 2017, 44: 38
doi: S0730-725X(17)30124-8
pmid: 28700894
|
| 15 |
Silvestri Z, Davis R S, Genevès G, et al. Volume magnetic susceptibility of gold-platinum alloys: Possible materials to make mass standards for the watt balance experiment[J]. Metrologia, 2003, 40: 172
|
| 16 |
Liu M W, Weissmüller J. Phase decomposition in nanoporous Au-Pt[J]. Acta Mater., 2022, 241: 118419
|
| 17 |
Celik F A, Özel S. A simulation study on the orientational phase transformation behavior of Au-Pt alloy for different concentration of Pt[J]. Solid State Commun., 2020, 316-317: 113940
|
| 18 |
Vidano S, Novara C, Pagone M, et al. The LISA DFACS: Model Predictive Control design for the test mass release phase[J]. Acta Astron., 2022, 193: 731
|
| 19 |
Kim S G. A phase-field model with antitrapping current for multicomponent alloys with arbitrary thermodynamic properties[J]. Acta Mater., 2007, 55: 4391
|
| 20 |
Steinbach I, Pezzolla F. A generalized field method for multiphase transformations using interface fields[J]. Physica, 1999, 134D: 385
|
| 21 |
Xu X N, Qin G W, Ren Y P, et al. Experimental study of the miscibility gap and calculation of the spinodal curves of the Au-Pt system[J]. Scr. Mater., 2009, 61: 859
|
| 22 |
Grolier V, Schmid-Fetzer R. Experimental study of Au-Pt-Sn phase equilibria and thermodynamic assessment of the Au-Pt and Au-Pt-Sn systems[J]. J. Electron. Mater., 2008, 37: 264
|
| 23 |
Liu Y J, Wang J, Du Y, et al. Phase boundary migration, Kirkendall marker shift and atomic mobilities in fcc Au-Pt alloys[J]. Calphad, 2012, 36: 94
|
| 24 |
Rappaz M, Gandin C A. Probabilistic modelling of microstructure formation in solidification processes[J]. Acta Metall. Mater., 1993, 41: 345
|
| 25 |
Ye W C, Kou H H, Liu Q Z, et al. Electrochemical deposition of Au-Pt alloy particles with cauliflower-like microstructures for electrocatalytic methanol oxidation[J]. Int. J. Hydrogen Energy, 2012, 37: 4088
|
| 26 |
Ramanarayan H, Abinandanan T A. Spinodal decomposition in polycrystalline alloys[J]. Physica, 2003, 318A: 213
|
| 27 |
Li L L, Li Z M, da Silva A K, et al. Segregation-driven grain boundary spinodal decomposition as a pathway for phase nucleation in a high-entropy alloy[J]. Acta Mater., 2019, 178: 1
|
| 28 |
Guo C, Zhao Y P, Deng Y Y, et al. A phase-field study on interaction process of moving grain boundary and spinodal decomposition[J]. Acta Phys. Sin., 2022, 71: 078101
|
| 28 |
郭 灿, 赵玉平, 邓英远 等. 运动晶界与调幅分解相互作用过程的相场法研究[J]. 物理学报, 2022, 71: 078101
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|