| 巨磁致伸缩Fe-Ga合金薄带的抑制剂与二次再结晶行为 |
翟欣雅1, 和正华1( ), 沙玉辉2, 朱晓飞3, 李锋1, 陈立佳1, 左良2,3 |
1 沈阳工业大学 材料科学与工程学院 沈阳 110870 2 东北大学 材料各向异性与织构教育部重点实验室 沈阳 110819 3 中国科学院金属研究所 沈阳 110016 |
|
| Inhibitor and Secondary Recrystallization Behavior of Giant Magnetostriction of Fe-Ga Thin Sheet |
ZHAI Xinya1, HE Zhenghua1( ), SHA Yuhui2, ZHU Xiaofei3, LI Feng1, CHEN Lijia1, ZUO Liang2,3 |
1 School of Materials Science and Engineering, Shenyang University of Technology, Shenyang 110870, China 2 Key Laboratory for Anisotropy and Texture of Materials, Ministry of Education, Northeastern University, Shenyang 110819, China 3 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China |
引用本文:
翟欣雅, 和正华, 沙玉辉, 朱晓飞, 李锋, 陈立佳, 左良. 巨磁致伸缩Fe-Ga合金薄带的抑制剂与二次再结晶行为[J]. 金属学报, 2024, 60(11): 1559-1570.
Xinya ZHAI,
Zhenghua HE,
Yuhui SHA,
Xiaofei ZHU,
Feng LI,
Lijia CHEN,
Liang ZUO.
Inhibitor and Secondary Recrystallization Behavior of Giant Magnetostriction of Fe-Ga Thin Sheet[J]. Acta Metall Sin, 2024, 60(11): 1559-1570.
| 1 |
Guruswamy S, Srisukhumbowornchai N, Clark A E, et al. Strong, ductile, and low-field-magnetostrictive alloys based on Fe-Ga [J]. Scr. Mater., 2000, 43: 239
|
| 2 |
Kellogg R A, Russell A M, Lograsso T A, et al. Tensile properties of magnetostrictive iron-gallium alloys [J]. Acta Mater., 2004, 52: 5043
|
| 3 |
Fu Q, Sha Y H, Zhang F, et al. Correlative effect of critical parameters for η recrystallization texture development in rolled Fe81Ga19 sheet: Modeling and experiment [J]. Acta Mater., 2019, 167: 167
|
| 4 |
Ma T Y, Hu S S, Bai G H, et al. Structural origin for the local strong anisotropy in melt-spun Fe-Ga-Tb: Tetragonal nanoparticles [J]. Appl. Phys. Lett., 2015, 106: 112401
|
| 5 |
Srisukhumbowornchai N, Guruswamy S. Crystallographic textures in rolled and annealed Fe-Ga and Fe-Al alloys [J]. Metall. Mater. Trans., 2004, 35A: 2963
|
| 6 |
Na S M, Yoo J H, Flatau A B. Abnormal (110) grain growth and magnetostriction in recrystallized galfenol with dispersed niobium carbide [J]. IEEE Trans. Magn., 2009, 45: 4132
|
| 7 |
Li J H, Gao X X, Zhu J, et al. Texture and magnetostriction in rolled Fe-Ga alloy [J]. Acta Metall. Sin., 2008, 44: 1031
|
| 7 |
李纪恒, 高学绪, 朱 洁 等. 轧制Fe-Ga合金的织构及磁致伸缩 [J]. 金属学报, 2008, 44: 1031
|
| 8 |
He Z H, Sha Y H, Fu Q, et al. Secondary recrystallization and magnetostriction in binary Fe81Ga19 thin sheets [J]. J. Appl. Phys., 2016, 119: 123904
|
| 9 |
He Z H, Sha Y H, Shan N, et al. Secondary recrystallization Goss texture development in a binary Fe81Ga19 sheet induced by inherent grain boundary mobility [J]. Metals, 2019, 9: 1254
|
| 10 |
Sun A L, Liu J H, Jiang C B. Recrystallization, texture evolution, and magnetostriction behavior of rolled (Fe81Ga19)98B2 sheets during low-to-high temperature heat treatments [J]. J. Mater. Sci., 2014, 49: 4565
|
| 11 |
Jiang L P, Yang J D, Hao H B, et al. Giant enhancement in the magnetostrictive effect of FeGa alloys doped with low levels of terbium [J]. Appl. Phys. Lett., 2013, 102: 222409
|
| 12 |
Na S M, Flatau A B. Single grain growth and large magnetostriction in secondarily recrystallized Fe-Ga thin sheet with sharp Goss (011)[100] orientation [J]. Scr. Mater., 2012, 66: 307
|
| 13 |
Na S M, Flatau A B. Global Goss grain growth and grain boundary characteristics in magnetostrictive galfenol sheets [J]. Smart Mater. Struct., 2013, 22: 125026
|
| 14 |
Yuan C, Li J H, Zhang W L, et al. Secondary recrystallization behavior in the rolled columnar-grained Fe-Ga alloys [J]. J. Magn. Magn. Mater., 2015, 391: 145
|
| 15 |
Yuan C, Li J H, Bao X Q, et al. Influence of annealing process on texture evolution and magnetostriction in rolled Fe-Ga based alloys [J]. J. Magn. Magn. Mater., 2014, 362: 154
|
| 16 |
Li J H, Zhang W L, Yuan C, et al. Inhibition force of precipitates for promoting abnormal grain growth in magnetostrictive Fe83Ga17-(B, NbC) alloy sheets [J]. Rare Met., 2017, 36: 886
|
| 17 |
He Z H, Du H J, Sha Y H, et al. Secondary recrystallization texture and magnetostriction in Fe-Ga alloy ultra-thin sheet [J]. IEEE Trans. Magn., 2022, 58: 2501906
|
| 18 |
He Z H, Hao H B, Sha Y H, et al. Sharp secondary recrystallization and large magnetostriction in Fe81Ga19 sheet induced by composite nanometer-sized inhibitors [J]. J. Magn. Magn. Mater., 2019, 478: 109
|
| 19 |
Lei F, Sha Y H, He Z H, et al. Rapid secondary recrystallization of the Goss texture in Fe81Ga19 sheets using nanosized NbC particles [J]. Materials, 2021, 14: 3818
|
| 20 |
Liu Y Y, Li J H, Mu X, et al. Strong NbC particle pinning for promoting abnormal growth of Goss grain in Fe82Ga4.5Al13.5 rolled sheets [J]. J. Magn. Magn. Mater., 2017, 444: 364
|
| 21 |
Mao W M, Li Y, Guo W, et al. Influence of MnS particles inside grains on the boundary migration before secondary recrystallization of grain oriented electrical steels [J]. Solid State Phenom., 2010, 160: 247
|
| 22 |
Mao W M, An Z G, Li S X. Influence of MnS particles on the behaviors of grain boundary migration in Fe-3%Si alloys [J]. Chin. Sci. Bull., 2009, 54: 4537
|
| 23 |
He Z H, Du H J, Sha Y H, et al. Secondary recrystallization behavior in magnetostrictive Fe-Ga thin sheets induced by nano-sized composite precipitates [J]. AIP Adv., 2021, 11: 035313
|
| 24 |
Fu Q, Sha Y H, He Z H, et al. Recrystallization texture and magnetostriction in binary Fe81Ga19 sheets [J]. Acta Metall. Sin., 2017, 53: 90
|
| 24 |
付 全, 沙玉辉, 和正华 等. Fe81Ga19二元合金薄板的再结晶织构与磁致伸缩性能 [J]. 金属学报, 2017, 53: 90
|
| 25 |
Zhao L J, Tian X, Yao Z Q, et al. Enhanced magnetostrictive properties of lightly Pr-doped Fe83Ga17 alloys [J]. J. Rare Earths, 2020, 38: 257
|
| 26 |
He Z H, Sha Y H, Zhang F, et al. Development of strong η fiber recrystallization texture in rolled Fe81Ga19 thin sheet [J]. Metall. Mater. Trans., 2014, 45A: 129
|
| 27 |
Park J T, Szpunar J A. Evolution of recrystallization texture in nonoriented electrical steels [J]. Acta Mater., 2003, 51: 3037
|
| 28 |
Dorner D, Zaefferer S, Raabe D. Retention of the Goss orientation between microbands during cold rolling of an Fe3%Si single crystal [J]. Acta Mater., 2007, 55: 2519
|
| 29 |
Dorner D, Zaefferer S, Lahn L, et al. Overview of microstructure and microtexture development in grain-oriented silicon steel [J]. J. Magn. Magn. Mater., 2006, 304: 183
|
| 30 |
Samajdar I, Cicale S, Verlinden B, et al. Primary recrystallization in a grain oriented silicon steel: On the origin of Goss {110}<001> grains [J]. Scr. Mater., 1998, 39: 1083
|
| 31 |
Hayakawa Y, Szpunar J A. A new model of Goss texture development during secondary recrystallization of electrical steel [J]. Acta Mater., 1997, 45: 4713
|
| 32 |
Lin P, Palumbo G, Harase J, et al. Coincidence site lattice (CSL) grain boundaries and Goss texture development in Fe-3%Si alloy [J]. Acta Mater., 1996, 44: 4677
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|