| 层间温度对9%Cr热强钢管道多层多道焊接头残余应力的影响 |
胡磊1, 王学1,2( ), 尹孝辉1, 刘洪3, 马群双1 |
1 安徽工业大学材料科学与工程学院 马鞍山 243032 2 武汉大学动力与机械学院 武汉 430072 3 东方电气集团东方锅炉股份有限公司 自贡 643001 |
|
| Influence of Inter-Pass Temperature on Residual Stress in Multi-Layer and Multi-Pass Butt-Welded 9%Cr Heat-Resistant Steel Pipes |
Lei HU1, Xue WANG1,2( ), Xiaohui YIN1, Hong LIU3, Qunshuang MA1 |
1 School of Materials Science and Engineering, Anhui University of Technology, Ma'anshan, Anhui 243032, China 2 School of Power and Mechanics, Wuhan University, Wuhan 430072, China 3 Dong Fang Boiler Group Co., Ltd., Dong Fang Electric Corporation, Zigong 643001, China |
引用本文:
胡磊, 王学, 尹孝辉, 刘洪, 马群双. 层间温度对9%Cr热强钢管道多层多道焊接头残余应力的影响[J]. 金属学报, 2018, 54(12): 1767-1776.
Lei HU,
Xue WANG,
Xiaohui YIN,
Hong LIU,
Qunshuang MA.
Influence of Inter-Pass Temperature on Residual Stress in Multi-Layer and Multi-Pass Butt-Welded 9%Cr Heat-Resistant Steel Pipes[J]. Acta Metall Sin, 2018, 54(12): 1767-1776.
| [1] | Abson D J, Rothwell J S.Review of type IV cracking of weldments in 9-12%Cr creep strength enhanced ferritic steels[J]. Int. Mater. Rev., 2013, 58: 437 | | [2] | Wang X, Wang X, Li H J, et al.Laves phase precipitation behavior in the simulated fine-grained heat-affected zone of creep strength enhanced ferritic steel P92 and its role in creep void nucleation and growth[J]. Weld. World, 2017, 61: 231 | | [3] | Liu W, Lu F G, Wei Y H, et al.Special zone in multi-layer and multi-pass welded metal and its role in the creep behavior of 9Cr-1Mo welded joint[J]. Mater. Des., 2016, 108: 195 | | [4] | Paddea S, Francis J A, Paradowska A M, et al.Residual stress distributions in a P91 steel-pipe girth weld before and after post weld heat treatment[J]. Mater. Sci. Eng., 2012, A534: 663 | | [5] | Francis J A, Bhadeshia H K D H, Withers P J. Welding residual stresses in ferritic power plant steels[J]. Mater. Sci. Technol., 2007, 23: 1009 | | [6] | Ooi S W, Garnham J E, Ramjaun T I.Review: Low transformation temperature weld filler for tensile residual stress reduction[J]. Mater. Des., 2014, 56: 773 | | [7] | Wang X, Li Y, Ren Y Y, et al.Effect of Laves phase precipitation on redistribution of alloying elements in P92 steel[J]. Acta Metall. Sin., 2014, 50: 1203(王学, 李勇, 任遥遥等. Laves相析出对P92钢合金元素再分布的影响[J]. 金属学报, 2014, 50: 1203) | | [8] | Yang J P, Guo J, Qiao Y X.Study on welding procedure of P92 steel using in ultra supercritical plants[J]. Proc. CSEE, 2007, 27(23): 55(杨建平, 郭军, 乔亚霞. 超超临界机组用P92钢焊接技术的研究[J]. 中国电机工程学报, 2007, 27(23): 55) | | [9] | Qiao Y X, Guo J.P92 steel (martensitic steel) welding used for power plant boilers[J]. Electr. Power Constr., 2007, 28(6): 87(乔亚霞, 郭军. 电站锅炉用马氏体耐热钢P92钢的焊接[J]. 电力建设, 2007, 28(6): 87) | | [10] | Richardot D, Vaillant J C, Arbab A, et al.The T92/P92 Book[M]. Boulogne: Vallourec & Mannesmann Tubes, 2000: 7 | | [11] | Haarmann K, Vailant J C, Vandenberghe B, et al.The T91/P91 Book[M]. Boulogne: Vallourec & Mannesmann Tubes, 1999: 6 | | [12] | Wang X, Hu L, Chen D X, et al.Effect of martensitic transformation on stress evolution in multi-pass butt-welded 9%Cr heat-resistant steel pipes[J]. Acta Metall. Sin., 2017, 53: 888(王学, 胡磊, 陈东旭等. 马氏体相变对9%Cr热强钢管道多道焊接头残余应力演化的影响[J]. 金属学报, 2017, 53: 888) | | [13] | Wang Z Y, Li S J, Hao X J, et al.Ultrasonic testing of interlayer cracks in P91 butt weld[J]. Nondestr. Test., 2011, 33(5): 54(王志永, 李树军, 郝晓军等. P91钢管对接焊缝层间裂纹的超声波检测[J]. 无损检测, 2011, 33(5): 54) | | [14] | Chen J P, Yang W F, Han T, et al.The ultrasonic testing of micro-crack in P91/92 steel pipe butt weld[J]. Nondestr. Test., 2016, 38(8): 44(陈君平, 杨文峰, 韩腾等. P91/P92钢管道对接焊缝微裂纹的超声波检测[J]. 无损检测, 2016, 38(8): 44) | | [15] | Javadi Y, Smith M C, Abburi Venkata K, et al.Residual stress measurement round robin on an electron beam welded joint between austenitic stainless steel 316L(N) and ferritic steel P91 [J]. Int. J. Press. Vessels Pip., 2017, 154: 41 | | [16] | Pu X W, Zhang C H, Li S, et al.Simulating welding residual stress and deformation in a multi-pass butt-welded joint considering balance between computing time and prediction accuracy[J]. Int. J. Adv. Manuf. Technol., 2017, 93: 2215 | | [17] | Deng D A, Ren S D, Li S, et al.Influence of multi-thermal cycle and constraint condition on residual stress in P92 steel weldment[J]. Acta Metall. Sin., 2017, 53: 1532(邓德安, 任森栋, 李索等. 多重热循环和约束条件对P92钢焊接残余应力的影响[J]. 金属学报, 2017, 53: 1532) | | [18] | Galler J P, Dupont J N, Siefert J A.Influence of alloy type, peak temperature and constraint on residual stress evolution in Satoh test[J]. Sci. Technol. Weld. Joining, 2016, 21: 106 | | [19] | Thomas S H, Liu S.Analysis of low transformation temperature welding (LTTW) consumables-distortion control and evolution of stresses[J]. Sci. Technol. Weld. Joining, 2014, 19: 392 | | [20] | Yaghi A H, Hyde T H, Becker A A, et al.Finite element simulation of welding and residual stresses in a P91 steel pipe incorporating solid-state phase transformation and post-weld heat treatment[J]. J. Strain Anal. Eng. Des., 2008, 43: 275 | | [21] | Koistinen D P, Marburger R E.A general equation prescribing the extent of the austenite-martensite transformation in pure iron-carbon alloys and plain carbon steels[J]. Acta Metall., 1959, 7: 59 | | [22] | Wang X, Pan Q G, Tao Y S, et al.Type IV creep rupture characteristics of P92 steel weldment[J]. Acta Metall. Sin., 2012, 48: 427(王学, 潘乾刚, 陶永顺等. P92钢焊接接头IV型蠕变断裂特性[J]. 金属学报, 2012, 48: 427) | | [23] | Yaghi A H, Hyde T H, Becker A A, et al.Finite element simulation of welded P91 steel pipe undergoing post-weld heat treatment[J]. Sci. Technol. Weld. Joining, 2011, 16: 232 | | [24] | Deng D A, Zhang Y B, Li S, et al.Influence of solid-state phase transformation on residual stress in P92 steel welded joint[J]. Acta Metall. Sin., 2016, 52: 394(邓德安, 张彦斌, 李索等. 固态相变对P92钢焊接接头残余应力的影响[J]. 金属学报, 2016, 52: 394) | | [25] | Li S, Ren S D, Zhang Y B, et al.Numerical investigation of formation mechanism of welding residual stress in P92 steel multi-pass joints[J]. J. Mater. Process. Technol., 2017, 244: 240 | | [26] | Radaj D.Heat Effects of Welding: Temperature Field, Residual Stress, Distortion[M]. Berlin: Springer-Verlag, 1992: 174 |
|
|