| 定向凝固U720Li合金的高温塑性变形行为* |
高博1,王磊1( ),梁涛沙1,刘杨1,宋秀1,曲敬龙2 |
1 东北大学材料各向异性与织构教育部重点实验室, 沈阳 110819 2 钢铁研究总院高温材料研究所, 北京 100081 |
|
| PLASTIC DEFORMATION BEHAVIOR OF DIRECTION-ALLY SOLIDIFIED U720Li ALLOY AT ELEVATEDTEMPERATURE |
Bo GAO1,Lei WANG1( ),Taosha LIANG1,Yang LIU1,Xiu SONG1,Jinglong QU2 |
1 Key Lab for Anisotropy and Texture of Materials, Ministry of Education, Northeastern University, Shenyang 110819, China 2 High Temperature Material Research Institute, Central Iron and Steel Research Institute, Beijing 100081, China |
引用本文:
高博,王磊,梁涛沙,刘杨,宋秀,曲敬龙. 定向凝固U720Li合金的高温塑性变形行为*[J]. 金属学报, 2016, 52(4): 437-444.
Bo GAO,
Lei WANG,
Taosha LIANG,
Yang LIU,
Xiu SONG,
Jinglong QU.
PLASTIC DEFORMATION BEHAVIOR OF DIRECTION-ALLY SOLIDIFIED U720Li ALLOY AT ELEVATEDTEMPERATURE[J]. Acta Metall Sin, 2016, 52(4): 437-444.
| [1] | Guo J T.Materials Science and Engineering for Superalloys. Vol.1, Beijing: Science Press, 2008: 3 | | [1] | (郭建亭. 高温合金材料学(上册). 北京: 科学出版社, 2008: 3) | | [2] | Huang Q Y, Li H K.Superalloy. Beijing: Metallurgy Industry Press, 2000: 1 | | [2] | (黄乾尧, 李汉康. 高温合金. 北京:冶金工业出版社, 2000: 1) | | [3] | Sharqhi-Moshtaqhin R, Asqari S.J Mater Process Technol, 2004; 147: 343 | | [4] | Guo J T.Materials Science and Engineering for Superalloys. Vol.2, Beijing: Science Press, 2008: 127 | | [4] | (郭建亭. 高温合金材料学(中册). 北京: 科学出版社, 2008: 127) | | [5] | Jackson M P, Reed R C.Mater Sci Eng, 1998; A259: 85 | | [6] | Pang H T, Reed P A S.Int J Fatigue, 2008; 30: 2009 | | [7] | Qu J L, Du J H, Bi Z N, Wang M Q, Zhang J, Wu G L.J Iron Steel Res, 2011; 23(suppl2): 247 | | [7] | (曲敬龙, 杜金辉, 毕中南, 王民庆, 张继, 吴桂林. 钢铁研究学报, 2011; 23(增刊2): 247) | | [8] | The Editorial Board of China Aeronautical Materials Handbook. China Aeronautical Materials Handbook. Vol.2, 2nd Ed., Beijing: Standards Press of China, 2002: 271 | | [8] | (《中国航空材料手册》编委会. 中国航空材料手册. 第2卷, 第二版, 北京: 中国标准出版社, 2002: 271) | | [9] | Wang L A.Manufacturing Engineering for Hard Wrought Forgings. Beijing: National Defend Industry Press, 2005: 98 | | [9] | (王乐安. 难变形合金锻件生产技术. 北京: 国防工业出版社, 2005: 98) | | [10] | Monajati H, Jahazi M, Yue S, Taheri A K.Metall Mater Trans, 2005; 36A: 895 | | [11] | Guo X P, Gao L M, Guan P, Kusabiraki K, Fu H Z. Mater Sci Forum, 2007; 539-543: 3690 | | [12] | Tao C H, Zhang W F, Li Y J, Shi H J.Failure Analysis Prevention, 2006; 1(4): 1 | | [12] | (陶春虎, 张卫方, 李运菊, 施惠基. 失效分析与预防, 2006; 1(4): 1) | | [13] | Tao C H, Zhang W F, Shi H J, Zhang Z L.Recrystallization of Directionally Solidified Superalloy. Beijing: National Defend Industry Press, 2007: 1 | | [13] | (陶春虎, 张卫方, 施惠基, 张宗林. 定性凝固高温合金的再结晶. 北京: 国防工业出版社, 2007: 1) | | [14] | Zhao X B, Liu L, Yu Z H, Wang W G, Fu H Z.Mater Charact, 2010; 61: 7 | | [15] | Warnken N, Ma D, Mathes M, Steinbach I. Mater Sci Eng, 2005; A413-414: 267 | | [16] | Li X C.Met Sci Technol, 1986; 5(1): 99 | | [16] | (李秀臣. 金属科学与工艺, 1986; 5(1): 99) | | [17] | Xia W J.PhD Dissertation, Hunan University, Changsha, 2010 | | [17] | (夏伟军. 湖南大学博士学位论文, 长沙, 2010) | | [18] | Ebrahimi R, Najafizadeh A.J Mater Processing Technol, 2004; 152: 136 | | [19] | Guo J H, Zhao S D, Murakami R, Ding R X, Fan S Q.J Alloys Compd, 2013; 566: 62 | | [20] | Wu Z G, Li D F.Chin J Nonferrous Met, 2010; 20: 1321 | | [20] | (吾志刚, 李德富. 中国有色金属学报, 2010; 20: 1321) | | [21] | Yu J W, Liu X F, Xie J X.Acta Metall Sin, 2011; 47: 482 | | [21] | (余均武, 刘雪峰, 谢建新. 金属学报, 2011; 47: 482) | | [22] | Ouyang D L, Lu S Q, Cui X, Wu C, Dong X J.Trans Mater Heat Treatment, 2009; 30: 116 | | [22] | (欧阳德来, 鲁世强, 崔霞, 吴超, 董显娟. 材料热处理学报, 2009; 30: 116) | | [23] | Wang L, Pyczak F, Zhang J, Lou L H, Singer R F.Mater Sci Eng, 2012; A532: 487 | | [24] | Humphreys F J, Hatherly M.Recrystallization and Related Annealing Phenomena. Oxford: Pergamon, 2004: 285 | | [25] | Wang Y, Shao W Z, Zhen L, Zhang X M.Mater Sci Eng, 2008; A486: 321 |
|
|