| 中间热处理对Zr-1Nb-0.2Y合金在420 ℃空气中氧化性能的影响* |
李长记1,2,熊良银1,2,刘实1,2( ) |
1 中国科学院金属研究所, 沈阳 110016 2 中国科学院金属研究所核用材料与安全评价重点实验室, 沈阳 110016 |
|
| EFFECT OF THE INTERMEDIATE HEAT TREATMENT PROCESSES ON THE OXIDATION CHARACTERIS- TICS OF Zr-1Nb-0.2Y ALLOY IN 420 ℃ AIR |
Changji LI1,2,Liangyin XIONG1,2,Shi LIU1,2( ) |
1 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2 Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China |
引用本文:
李长记,熊良银,刘实. 中间热处理对Zr-1Nb-0.2Y合金在420 ℃空气中氧化性能的影响*[J]. 金属学报, 2016, 52(1): 85-92.
Changji LI,
Liangyin XIONG,
Shi LIU.
EFFECT OF THE INTERMEDIATE HEAT TREATMENT PROCESSES ON THE OXIDATION CHARACTERIS- TICS OF Zr-1Nb-0.2Y ALLOY IN 420 ℃ AIR[J]. Acta Metall Sin, 2016, 52(1): 85-92.
| [1] | Cox B. J Nucl Mater, 2005; 336: 331 | | [2] | Yilmazbayhan A, Motta A T, Comstock R J, Sabol G P, Lai B, Cai Z H. J Nucl Mater, 2004; 324: 6 | | [3] | Gong W J, Zhang H L, Qiao Y, Tian H, Ni X D, Li Z K, Wang X T. Corros Sci, 2013; 74: 323 | | [4] | Nikulin S A, Khanzhin V G, Rozhnov A B, Belov V A. Met Sci Heat Treat, 2009; 51: 230 | | [5] | Petrova I I, Samsonov B N, Peletsky V E, Nikulina A V, Sokolov N B, Andreeva-Andrievskaya L N. Int J Thermophys, 2002; 23: 1347 | | [6] | Nikulina A V. Met Sci Heat Treat, 2004; 46: 458 | | [7] | Liu J Z. Nuclear Structure Materials. Beijing: Chemical Industry Press, 2007: 5 | | [7] | (刘建章. 核结构材料. 北京: 化学工业出版社, 2007: 5) | | [8] | Li Z K, Liu J Z, Zhou L, Li C, Zhang J J. Rare Met Mater Eng, 2002; 31: 261 | | [8] | (李中奎, 刘建章, 周 廉, 李 聪, 张建军. 稀有金属材料与工程, 2002; 31: 261) | | [9] | Canay M, Danón C A, Arias D. J Nucl Mater, 2000; 280: 365 | | [10] | Ni N, Lozano-Perez S, Sykes J M, Smith G D W, Grovenor C R M. Corros Sci, 2011; 53: 4073 | | [11] | Seok C S, Bae B K, Koo J M, Murty K L. Eng Fail Anal, 2006; 13: 389 | | [12] | Steinbrück M, B?ttcher M. J Nucl Mater, 2011; 414: 276 | | [13] | Park J Y, Yoo S J, Choi B K, Jeong Y H. J Nucl Mater, 2008; 373: 343 | | [14] | Park J Y, Choi B K, Yoo S J, Jeong Y H. J Nucl Mater, 2006; 359: 59 | | [15] | Zhou B X, Yao M Y, Li Z K, Wang X M, Zhou J, Long C S, Liu Q, Luan B F. J Mater Sci Technol, 2012; 28: 606 | | [16] | Zhao W J, Liu Y Z, Jiang H M, Peng Q. J Alloys Compd, 2008; 462: 103 | | [17] | Jeong Y H, Park S Y, Lee M H, Choi B K, Baek J H, Park J Y, Kim J H, Kim H G. J Nucl Sci Technol, 2006; 43: 977 | | [18] | Kim H G, Park J Y, Jeong Y H, Koo Y H, Yoo J S, Mok Y K, Kim Y H, Suh J M. J Nucl Sci Technol, 2014; 46: 423 | | [19] | Duriez C, Dupont T, Schmet B, Enoch F. J Nucl Mater, 2008; 380: 30 | | [20] | Batra I S, Singh R N, Sengupta P, Maji B C, Madangopal K, Manikrishna K V, Tewari R, Dey G K. J Nucl Mater, 2009; 389: 500 | | [21] | Batra I S, Singh R N, Khandelwal H K, Mukherjee A, Krishnamurthy N, Gargi C, Shah B K. J Nucl Mater, 2013; 434: 389 | | [22] | Li C J, Xiong L Y, Wu E D, Liu S. J Nucl Mater, 2015; 457: 142 | | [23] | Jeong Y H, Kim H G, Kim T H. J Nucl Mater, 2003; 317: 1 | | [24] | Kim H G, Choi B K, Park J Y, Jeong Y H. Corro Sci, 2009; 51: 2400 | | [25] | Kim H G, Park S Y, Lee M H, Jeong Y H, Kim S D. J Nucl Mater, 2008; 373; 429 | | [26] | Li Q, Liang X, Peng J C, Liu R D, Yu K, Zhou B X. Acta Metall Sin, 2011; 47: 893 | | [26] | (李 强, 梁 雪, 彭剑超, 刘仁多, 余 康, 周邦新. 金属学报, 2011; 47: 893) |
|
|