| 超细晶304L不锈钢在含Cl-溶液中点蚀行为的研究 |
朴楠1,2,陈吉1( ),尹成江1,3,孙成4,张星航4,武占文5 |
2 清华大学核能与新能源技术研究院, 北京 100084 3 东北石油大学机械工程学院, 大庆 163318 4 Department of Mechanical Engineering, Texas A&M University, College station, TX 77843-3123, USA 5 中海油能源发展股份有限公司管道工程分公司, 天津 300452 |
|
| INVESTIGATION ON PITTING CORROSION BEHAVIOR OF ULTRAFINE-GRAINED 304L STAINLESS STEEL IN Cl- CONTAINING SOLUTION |
Nan PIAO1,2,Ji CHEN1( ),Chengjiang YIN1,3,Cheng SUN4,Xinghang ZHANG4,Zhanwen WU5 |
1 Center of Corrosion and Protection Technology in Petro-Chemical Industry, Department of Mechanical Engineering, Liaoning Shihua University, Fushun 113001 2 Institute of Nuclear and New Energy Technology, Tsinghua University, Beijing 100084 3 Department of Mechanical Engineering, Northeast Petroleum University, Daqing 163318 4 Department of Mechanical Engineering, Texas A&M University, College station, TX 77843-3123, USA 5 CNOOC Energy Technology and Services-Pipe Engineering Co., Tianjin 300452 |
引用本文:
朴楠,陈吉,尹成江,孙成,张星航,武占文. 超细晶304L不锈钢在含Cl-溶液中点蚀行为的研究[J]. 金属学报, 2015, 51(9): 1077-1084.
Nan PIAO,
Ji CHEN,
Chengjiang YIN,
Cheng SUN,
Xinghang ZHANG,
Zhanwen WU.
INVESTIGATION ON PITTING CORROSION BEHAVIOR OF ULTRAFINE-GRAINED 304L STAINLESS STEEL IN Cl- CONTAINING SOLUTION[J]. Acta Metall Sin, 2015, 51(9): 1077-1084.
| [1] | Valiev R Z, Islangaliev P K, Alexandrov I V. Prog Mater Sci, 2000; 45: 103 | | [2] | Gleiter H. Acta Mater, 2000; 48: 1 | | [3] | Chen J, Lu L, Lu K. Scr Mater, 2006; 54: 1913 | | [4] | Lu K, Zhou F. Acta Metall Sin, 1997; 33: 99 (卢 柯, 周 飞. 金属学报, 1997; 33: 99) | | [5] | Huang C X, Gao Y L, Yang G, Wu S D, Li G Y, Li S X. J Mater Res, 2006; 21: 1687 | | [6] | Wang Y, Chen M, Zhou F, Ma E. Nature, 2002; 419: 912 | | [7] | Valiev R. Nat Mater, 2004; 3: 511 | | [8] | Valiev R Z, Langdon T G. Prog Mater Sci, 2006; 51: 881 | | [9] | Liu L, Li Y, Wang F H. J Mater Sci Technol, 2009; 54: 1339 | | [10] | Kabi S, Raeissi K, Saatchi A. J Appl Electrochem, 2009; 39: 1279 | | [11] | Yu B, Woo P, Erb U. Scr Mater, 2007; 56: 353 | | [12] | Afshari V, Dehghanian C. Corros Sci, 2009; 51: 1844 | | [13] | Li X L, Li Y, Wang F H. J Chin Soc Corros Prot, 2002; 22: 231 (李雪莉, 李 瑛, 王福会. 中国腐蚀与防护学报, 2002; 22: 321) | | [14] | Li N, Li Y, Wang S G, Wang F H. Electrochim Acta, 2006; 52: 760 | | [15] | Han X, Chen J, Sun C, Wu Z W, Wu X C, Zhang X H. Acta Metall Sin, 2013; 49: 265 (韩 啸, 陈 吉, 孙 成, 武占文, 吴新春, 张星航. 金属学报, 2013; 49: 265) | | [16] | Meng G Z, Li Y, Wang F H. Electrochim Acta, 2006; 51: 4277 | | [17] | Kiyotaka N, Zenji H, Minoru N, Terence G L. Mater Sci Eng, 2000; A280: 82 | | [18] | Ding J, Lin H C, Cao C N. Corros Sci, 2002; 14: 67 | | [19] | Yang R C, Bi H J, Niu S R, Jin S T, Shen P. J Lanzhou Univ Technol, 2010; 36: 5 (杨瑞成, 毕海娟, 牛绍蕊, 靳塞特, 申 鹏. 兰州理工大学学报, 2010; 36: 5) | | [20] | Dewald J F. J Phys Chem Solids, 1960; 14: 155 | | [21] | Buchler M, Schmuki P, Buhui H. Electrochim Acta, 1997; 43: 635 | | [22] | Hakiki N E, Belo M D C. J Electrochem Soc, 1996; 143: 3088 | | [23] | Gercasi C A, Folquer M E, Vallejo A E. Electrochim Acta, 2005; 50: 1113 | | [24] | Macdonald D D. J Electrochem Soc, 1992; 139: 3434 | | [25] | MacDonald D D, Urquidi-MacDonald M. J Electrochem Soc, 1990; 137: 2395 | | [26] | Chao C Y, Lin L F, MacDonald D D. J Electrochem Soc, 1981;128: 1187 | | [27] | Sikora E, Sikora J, MacDonald D D. Electrochim Acta, 1996; 41: 783 | | [28] | Guo H X, Lu B T, Luo J L. Electrochim Acta, 2006; 52: 1118 | | [29] | Glass G K, Hassanein A M, Buenfeld N R. Corrosion, 1998; 54: 887 | | [30] | Hamadou L, Kadri A, Benbrahim N. Appl Surf Sci, 2005; 252: 1510 | | [31] | Li D G, Feng Y R, Bai Z Q, Zhu J W, Zheng M S. Acta Chim Sin, 2008; 66: 1151 (李党国, 冯耀荣, 白真权, 朱杰武, 郑茂盛. 化学学报, 2008; 66: 1151) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|