金属学报  2015, Vol. 51 Issue (7): 853-858    DOI: 10.11900/0412.1961.2015.00007
  本期目录 | 过刊浏览 |
C对一种镍基高温合金与陶瓷型壳界面反应及润湿性的影响*
陈晓燕1,金喆2,白雪峰2,周亦胄1(),金涛1,孙晓峰1
2 沈阳黎明航空发动机(集团)有限责任公司, 沈阳 110043
EFFECT OF C ON THE INTERFACIAL REACTION AND WETTABILITY BETWEEN A Ni-BASED SUPERALLOY AND CERAMIC MOULD
Xiaoyan CHEN1,Zhe JIN2,Xuefeng BAI2,Yizhou ZHOU1(),Tao JIN1,Xiaofeng SUN1
1 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
2 Shenyang Liming Aero-Engine Group Corporation, Shenyang 110043
引用本文:

陈晓燕,金喆,白雪峰,周亦胄,金涛,孙晓峰. C对一种镍基高温合金与陶瓷型壳界面反应及润湿性的影响*[J]. 金属学报, 2015, 51(7): 853-858.
Xiaoyan CHEN, Zhe JIN, Xuefeng BAI, Yizhou ZHOU, Tao JIN, Xiaofeng SUN. EFFECT OF C ON THE INTERFACIAL REACTION AND WETTABILITY BETWEEN A Ni-BASED SUPERALLOY AND CERAMIC MOULD[J]. Acta Metall Sin, 2015, 51(7): 853-858.

全文: PDF(3918 KB)   HTML
摘要: 

采用座滴法研究了C对一种高温合金与陶瓷型壳的界面反应及润湿性的影响. 通过SEM和EPMA研究了合金与陶瓷型壳的界面组织形貌及反应区元素分布. 利用Thermo-Calc软件计算了合金熔体中C, Cr和Al的活度, 分析了C含量对合金熔体中C, Cr和Al的活度的影响. 探讨了合金/陶瓷界面反应与润湿性的关系. 结果表明, 合金中C含量高于0.1%时, C的活度明显增大, 合金熔体与陶瓷型壳发生界面反应, 合金熔体/陶瓷体系由非反应润湿变为反应润湿, 合金表面产生黏砂层且合金中Cr和Al扩散到陶瓷表面.

关键词 : 高温合金,  陶瓷型壳,  界面反应,  润湿性,  活度,  C    
Abstract:

Superalloy components are always produced by the way of investment casing. During investment casting, interfacial reactions may take place and bring about metal contamination and defect formation on the surface of the components. The influence of C content on the interfacial reaction and wettability between a Ni-based superalloy and ceramic mould was investigated by using a sessile drop method. The interfacial morphology and elements distribution were studied by SEM and EPMA. Activities of C, Cr and Al were calculated by using Thermo-Calc software. The relationship between interfacial reaction and wettability was discussed. It was found that when C content was higher than 0.1%, activity of C increased greatly and interfacial reaction took place. The wettability varied from non-reactive wetting to reactive wetting. In the reactive wetting systems, sand adhesions appeared and Al and Cr diffused to the ceramic surface.

Key words: superalloy    ceramic mould    interfacial reaction    wettability    activity    C
    
基金资助:* 国家自然科学基金项目51271186, 51331005和11332010, 以及国家高技术研究发展计划项目2014AA041701资助
图1  高温润湿性测试炉结构示意图
图2  合金熔体/陶瓷体系润湿角随时间的变化
图3  润湿实验后合金及陶瓷表面宏观形貌
图4  合金(0.2%C)/陶瓷接触区附近陶瓷表面形貌及元素面分布
图5  非反应润湿(0.05%C)与反应润湿(0.2%C)合金/陶瓷界面组织形貌以及反应润湿体系合金/陶瓷界面处元素面分布
Alloy aC / 10-4 aAl / 10-7 aCr / 10-4
A1 2.01 3.52 1.50
A2 2.51 3.52 1.50
A3 12.77 3.57 1.47
A4 26.05 3.63 1.45
A5 53.54 3.79 1.38
A6 81.78 3.86 1.35
表1  1550 ℃时A1~A6合金熔体中C, Al和Cr的活度
[1] Sun X F, Jin T, Zhou Y Z, Hu Z Q. Mater China, 2012; 31: 1 (孙晓峰, 金 涛, 周亦胄, 胡壮麒. 中国材料进展, 2012; 31: 1)
[2] Chen R Z, Wang L B, Li J H. J Aero Mater, 2000; 20(1): 55 (陈荣章, 王罗宝, 李建华. 航空材料学报, 2000; 20(1): 55)
[3] Konter M, Thumann M. J Mater Process Technol, 2001; 117: 386
[4] Volek A, Pyczak F, Singer R F, Mughrabi H. Scr Mater, 2005; 52: 141
[5] Yeh A C, Tin S. Scr Mater, 2005; 52: 519
[6] Li J R, Tang D Z, Li R L, Li S Z, Wang Z T. J Mater Sci Technol, 1999; 15: 53
[7] Reed R C, Tao T, Warnken N. Acta Mater, 2009; 57: 5898
[8] Maktouf W, Sai K. Eng Fail Anal, 2015; 47: 89
[9] Ford T. Aircraft Eng Aero Technol, 1997; 69: 564
[10] Kruglov E P, Kochetova G K. Russ Aero, 2007; 50: 227
[11] Wang Z J, Zhang L T. Acta Aerodyn Sin, 1989; 10: 167 (王祖锦, 张立同. 航空学报, 1989; 10: 167)
[12] Jin Z X. Foundry, 2000; 49: 172 (金仲信. 铸造, 2000; 49: 172)
[13] Hu G Q, Wang P, Pen F, Xiao N M. Foundry Technol, 2011; 32: 610 (扈广麒, 王 培, 彭 凡, 肖纳敏. 铸造技术, 2011; 32: 610)
[14] Kumar G, Prabhu K N. Adv Colloid Interface Sci, 2007; 133: 61
[15] Nakashima K, Matsumoto H, Mori K. Acta Mater, 2000; 48: 4677
[16] Cutler E R, Wasson A J, Fuchs G E. Scr Mater, 2008; 58: 146
[17] Xu Y L, Jin Q M, Xiao X S, Cao X L, Jia G Q, Zhu Y M, Yin H J. Mater Sci Eng, 2011; A528: 4600
[18] Jiang D L,Li L S,Ouyang S X,Shi J L. Material Handbook of Inorganic Metal. Beijing: Chemical Industry Press, 2009: 38 (江东亮,李龙士,欧阳世翕,施剑林. 无机非金属材料手册. 北京: 化学工业出版社, 2009: 38)
[19] Orlov M R. Russ Metall, 2008; 1: 70
[20] Liu X F, Guo W J, Lou Y C, Su G Q, Yu B. Foundry, 2010; 59: 1293 (刘孝福, 郭伟杰, 娄延春, 苏贵桥, 于 波. 铸造, 2010; 59: 1293)
[21] Wei Z J. Formation Process of Liquid Metals. Beijing: Higher Education Press, 2010: 252 (魏尊杰. 金属液态成型工艺. 北京: 高等教育出版社, 2010: 252)
[22] Liang Y J. Thermochemical Data of Inorganics. Shenyang: Northeastern University Press, 1993: 513 (梁英教. 无机热力学数据手册. 沈阳: 东北大学出版社, 1993: 513)
[23] Ma G F, He C L. Acta Metall Sin, 2013; 49: 495 (马国峰, 贺春林. 金属学报, 2013; 49: 495)
[24] Дemhиc И M, Кapпobич Ю Ф, Гjie3ep Г M. J Aero Mater, 1991; 11: 62 (Дemhиc И M, Кapпobич Ю Ф, Гjie3ep Г M. 航空材料学报, 1991; 11: 62)
[1] 李嘉荣, 董建民, 韩梅, 刘世忠. 吹砂对DD6单晶高温合金表面完整性和高周疲劳强度的影响[J]. 金属学报, 2023, 59(9): 1201-1208.
[2] 赵鹏, 谢光, 段慧超, 张健, 杜奎. 两种高代次镍基单晶高温合金热机械疲劳中的再结晶行为[J]. 金属学报, 2023, 59(9): 1221-1229.
[3] 毕中南, 秦海龙, 刘沛, 史松宜, 谢锦丽, 张继. 高温合金锻件残余应力量化表征及控制技术研究进展[J]. 金属学报, 2023, 59(9): 1144-1158.
[4] 郑亮, 张强, 李周, 张国庆. 增/降氧过程对高温合金粉末表面特性和合金性能的影响:粉末存储到脱气处理[J]. 金属学报, 2023, 59(9): 1265-1278.
[5] 马德新, 赵运兴, 徐维台, 王富. 重力对高温合金定向凝固组织的影响[J]. 金属学报, 2023, 59(9): 1279-1290.
[6] 陈佳, 郭敏, 杨敏, 刘林, 张军. 新型钴基高温合金中W元素对蠕变组织和性能的影响[J]. 金属学报, 2023, 59(9): 1209-1220.
[7] 张健, 王莉, 谢光, 王栋, 申健, 卢玉章, 黄亚奇, 李亚微. 镍基单晶高温合金的研发进展[J]. 金属学报, 2023, 59(9): 1109-1124.
[8] 王磊, 刘梦雅, 刘杨, 宋秀, 孟凡强. 镍基高温合金表面冲击强化机制及应用研究进展[J]. 金属学报, 2023, 59(9): 1173-1189.
[9] 宫声凯, 刘原, 耿粒伦, 茹毅, 赵文月, 裴延玲, 李树索. 涂层/高温合金界面行为及调控研究进展[J]. 金属学报, 2023, 59(9): 1097-1108.
[10] 冯强, 路松, 李文道, 张晓瑞, 李龙飞, 邹敏, 庄晓黎. γ' 相强化钴基高温合金成分设计与蠕变机理研究进展[J]. 金属学报, 2023, 59(9): 1125-1143.
[11] 江河, 佴启亮, 徐超, 赵晓, 姚志浩, 董建新. 镍基高温合金疲劳裂纹急速扩展敏感温度及成因[J]. 金属学报, 2023, 59(9): 1190-1200.
[12] 白佳铭, 刘建涛, 贾建, 张义文. 高W高Ta型粉末高温合金的蠕变性能及溶质原子偏聚[J]. 金属学报, 2023, 59(9): 1230-1242.
[13] 卢楠楠, 郭以沫, 杨树林, 梁静静, 周亦胄, 孙晓峰, 李金国. 激光增材修复单晶高温合金的热裂纹形成机制[J]. 金属学报, 2023, 59(9): 1243-1252.
[14] 穆亚航, 张雪, 陈梓名, 孙晓峰, 梁静静, 李金国, 周亦胄. 基于热力学计算与机器学习的增材制造镍基高温合金裂纹敏感性预测模型[J]. 金属学报, 2023, 59(8): 1075-1086.
[15] 丁桦, 张宇, 蔡明晖, 唐正友. 奥氏体基Fe-Mn-Al-C轻质钢的研究进展[J]. 金属学报, 2023, 59(8): 1027-1041.