| 铝热合成NiAl共格强化的FeNiCrAl合金的组织演化机理和力学性能 |
王星( ), 席文君, 崔跃, 李树杰 |
| 北京航空航天大学材料科学与工程学院, 北京100191 |
|
| MICROSTRUCTURE EVOLUTION MECHANISM AND MECHANICAL PROPERTIES OF FeNiCrAl ALLOY REINFORCED BY COHERENT NiAl SYNTHE- SIZED BY THERMITE PROCESS |
WANG Xing( ), XI Wenjun, CUI Yue, LI Shujie |
| Materials Science & Engineering School, Beihang University, Beijing 100191 |
引用本文:
王星, 席文君, 崔跃, 李树杰. 铝热合成NiAl共格强化的FeNiCrAl合金的组织演化机理和力学性能[J]. 金属学报, 2015, 51(4): 483-491.
Xing WANG,
Wenjun XI,
Yue CUI,
Shujie LI.
MICROSTRUCTURE EVOLUTION MECHANISM AND MECHANICAL PROPERTIES OF FeNiCrAl ALLOY REINFORCED BY COHERENT NiAl SYNTHE- SIZED BY THERMITE PROCESS[J]. Acta Metall Sin, 2015, 51(4): 483-491.
| [1] |
Masuyama F. ISIJ Int, 2001; 41: 612
|
| [2] |
Calderon H, Fine M E. Mater Sci Eng, 1984; 63: 197
|
| [3] |
Pearson W B. A Handbook of Lattice Spacings and Structures of Metals and Alloys. Oxford: Pergamon Press, 1958: 347
|
| [4] |
Stallybrass C, Schneider A, Sauthoff G. Intermetallics, 2005; 13: 1263
|
| [5] |
Sudbrack C K, Yoon K E, Noebe R D, Seidman D N. Acta Mater, 2006; 54: 3199
|
| [6] |
Calderon H A, Fine M E, Weertman J R. Metall Trans, 1988; 19A: 1135
|
| [7] |
Hao S M, Ishida K, Nishizawa T. Metall Trans, 1985; 16A: 179
|
| [8] |
Stallybrass C, Sauthoff G. Mater Sci Eng, 2004; A387: 985
|
| [9] |
Vo N Q, Liebscher C H, Rawlings M J, Asta M, Dunand D C. Acta Mater, 2014; 71: 89
|
| [10] |
Bradley A J, Taylor A. Proc R Soc London, 1938; 166(A926): 353
|
| [11] |
Yin S. Combustion Synthesis. Beijing: Metallurgical Industry Press, 2004: 1
|
| [11] |
(殷 声. 燃烧合成. 北京: 冶金工业出版社, 2004: 1)
|
| [12] |
Borovinskaya I P. Pure Appl Chem, 1992; 64: 919
|
| [13] |
Yukhvid V I. Pure Appl Chem, 1992; 64: 977
|
| [14] |
Fu Z Y. Acta Mater Comp Sin, 2000; 17(1): 5
|
| [14] |
(傅正义. 复合材料学报, 2000; 17(1): 5)
|
| [15] |
Hao S M, Takayama T, Ishida K, Nishizawa T. Metall Trans, 1984; 15A: 1819
|
| [16] |
Bradley A J. J Iron Steel Inst, 1949; 163: 19
|
| [17] |
Bradley A J. J Iron Steel Inst, 1951; 168: 233
|
| [18] |
Bradley A J. J Iron Steel Inst, 1952; 171: 41
|
| [19] |
Hanna J A, Baker I, Wittmann M W, Munroe P R. J Mater Res, 2005; 20: 791
|
| [20] |
Cahn J W. Acta Metall, 1961; 9: 795
|
| [21] |
Cahn J W. Acta Metall, 1962; 10: 179
|
| [22] |
Cahn J W. Acta Metall, 1962; 10: 907
|
| [23] |
Xi W, Peng R L, Wu W, Li N, Wang S, Johansson S. J Mater Sci, 2012; 47: 3585
|
| [24] |
Zhang C Q, Yao K F. Acta Metall Sin, 2006; 42: 870
|
| [24] |
(张长青, 姚可夫. 金属学报, 2006; 42: 870)
|
| [25] |
Ma N G, Kui H W. China Mech Eng, 2000; 11: 1298
|
| [25] |
(马南钢, Kui H W. 中国机械工程, 2000; 11: 1298)
|
| [26] |
Lee K L, Kui H W. J Mater Res, 1999; 14: 3653
|
| [27] |
Yuen C W, Lee K L, Kui H W. J Mater Res, 1997; 12: 314
|
| [28] |
Taillard R, Pineau A, Thomas B J. Mater Sci Eng, 1982; 54: 209
|
| [29] |
Rothman M F. High-Temperature Property Data: Ferrous Alloys. Metals Park, OH: ASM International, 1987: 250
|
| [30] |
Teng Z K, Liu C T, Ghosh G, Liaw P K, Fine M E. Intermetallics, 2010; 18: 1437
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|