ZG06Cr13Ni4Mo马氏体不锈钢中TRIP效应的同步辐射高能X射线原位研究* |
张盛华,王培( ),李殿中,李依依 |
|
INVESTIGATION OF TRIP EFFECT IN ZG06Cr13Ni4Mo MARTENSITIC STAINLESS STEEL BY IN SITU SYNCHROTRON HIGH ENERGY X-RAY DIFFRACTION |
Shenghua ZHANG,Pei WANG( ),Dianzhong LI,Yiyi LI |
Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
张盛华,王培,李殿中,李依依. ZG06Cr13Ni4Mo马氏体不锈钢中TRIP效应的同步辐射高能X射线原位研究*[J]. 金属学报, 2015, 51(11): 1306-1314.
Shenghua ZHANG,
Pei WANG,
Dianzhong LI,
Yiyi LI.
INVESTIGATION OF TRIP EFFECT IN ZG06Cr13Ni4Mo MARTENSITIC STAINLESS STEEL BY IN SITU SYNCHROTRON HIGH ENERGY X-RAY DIFFRACTION[J]. Acta Metall Sin, 2015, 51(11): 1306-1314.
[1] | Friis W L, Noren T M I. US Pat, 3378367, 1968 | [2] | Bilmes P D, Solari M, Llorente C L. Mater Charact, 2001; 46: 285 | [3] | Gesnouin C, Hazarabedian A, Bruzzoni P, Ovejero-Garcia J, Bilmes P, Llorente C. Corros Sci, 2004; 46: 1633 | [4] | Kane R D, Watkins M, Greer J B. Corrosion, 1977; 33: 231 | [5] | Bilmes P, Llorente C, Ipina J P. J Mater Eng Perform, 2000; 9: 609 | [6] | Song Y Y, Ping D H, Yin F X, Li X Y, Li Y Y. Mater Sci Eng, 2010; A527: 614 | [7] | Wang P, Xiao N M, Lu S P, Li D Z, Li Y Y. Mater Sci Eng, 2013; A586: 292 | [8] | Offerman S E, Van Dijk N H, Sietsma J, Grigull S, Lauridsen E M, Margulies L, Poulsen H F, Rekveldt M T, Van der Zwaag S. Science, 2002; 298: 1003 | [9] | Jacques P, Furnemont Q, Lani F, Pardoen T, Delannay F. Acta Mater, 2007; 55: 3681 | [10] | Lani F, Furnemont Q, Van Rompaey T, Delannay F, Jacques P J,Pardoen T. Acta Mater, 2007; 55: 3695 | [11] | Cheng S, Wang Y D, Choo H, Wang X L, Almer J D, Liaw P K, Lee Y K. Acta Mater, 2010; 58: 2419 | [12] | Blonde R, Jimenez-Melero E, Zhao L, Wright J P, Bruck E, Van der Zwaag S, Van Dijk N H. Acta Mater, 2012; 60: 565 | [13] | Choi K S, Liu W N, Sun X, Khaleel M A, Ren Y, Wang Y D. Metall Mater Trans, 2008; 39A: 3089 | [14] | Zhang S H, Wang P, Li D Z, Li Y Y. Mater Des, 2015; 84: 385 | [15] | Rietveld H M. Acta Cryst, 1967; 22: 151 | [16] | Jia N, Cong Z H, Sun X, Cheng S, Nie Z H, Ren Y, Liaw P K, Wang Y D. Acta Mater, 2009; 57: 3965 | [17] | Prince E. In: Young R A ed., The Rietveld Method. Oxford: Oxford University Press, 1993: 1 | [18] | Lutterotti L. MAUD. Version 2.038, Department of Materials Engineering, Engineering Faculty University of Trento, 2006 | [19] | Tomota Y, Tokuda H, Adachi Y, Wakita M, Minakawa N, Moriai A, Morii Y. Acta Mater, 2004; 52: 5737 | [20] | Timokhina I B, Hodgson P D, Pereloma E V. Metall Mater Trans, 2003; 34A: 1599 | [21] | Wang P, Lu S P, Li D Z, Kang X H, Li Y Y. Acta Metall Sin, 2008; 44: 681 (王 培, 陆善平, 李殿中, 康秀红, 李依依. 金属学报, 2008; 44: 681) | [22] | Dunn C G, Koch E F. Acta Mater, 1957; 5: 548 | [23] | Jacques P, Furnemont Q, Pardoen T, Delannay F. Acta Mater, 2001; 49: 139 | [24] | Rizk A, Bourell D L. Scr Met, 1982; 16: 1321 | [25] | Sangal S, Goel N C, Tangri K. Metall Mater Trans, 1985; 16A: 2023 |
|
|