铁基非晶涂层在NaCl和H2SO4溶液中的钝化行为 |
王勇1,2, 郑玉贵3, 王建强4, 李美玲5, 沈军1( ) |
1 同济大学材料科学与工程学院, 上海 201084 2 东北石油大学机械科学与工程学院, 大庆 163318 3 中国科学院金属研究所核用材料与安全评价重点实验室, 沈阳 110016 4 中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳 110016 5 鞍山师范学院物理系, 鞍山 114001 |
|
PASSIVATION BEHAVIOR OF Fe-BASED AMORPHOUS METALLIC COATING IN NaCl AND H2SO4 SOLUTIONS |
WANG Yong1,2, ZHENG Yugui3, WANG Jianqiang4, LI Meiling5, SHEN Jun1( ) |
1 School of Materials Science and Engineering, Tongji University, Shanghai 201084 2 School of Mechanical Science and Engineering, Northeast Petroleum University, Daqing 163318 3 Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 4 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 5 Physics Department, Anshan Normal College, Anshan 114001 |
引用本文:
王勇, 郑玉贵, 王建强, 李美玲, 沈军. 铁基非晶涂层在NaCl和H2SO4溶液中的钝化行为[J]. 金属学报, 2015, 51(1): 49-56.
Yong WANG,
Yugui ZHENG,
Jianqiang WANG,
Meiling LI,
Jun SHEN.
PASSIVATION BEHAVIOR OF Fe-BASED AMORPHOUS METALLIC COATING IN NaCl AND H2SO4 SOLUTIONS[J]. Acta Metall Sin, 2015, 51(1): 49-56.
[1] |
Hashimoto K. Corrosion, 2002; 58: 715
|
[2] |
Inoue A, Shinohara Y, Gook J S. Mater Trans JIM, 1995; 36: 1427
|
[3] |
Branagan D J, Swank W D, Haggard D C, Fincke J R. Metall Mater Trans, 2001; 32A: 2615
|
[4] |
Wang Y, Zheng Y G, Ke W, Sun W H, Wang J Q. Mater Corros, 2012; 63: 685
|
[5] |
Liu D Y, Wang C, Zhang H F, Hu Z Q. Acta Metall Sin, 2005; 41: 209
|
[5] |
(刘冬艳, 王 成, 张海峰, 胡壮麒. 金属学报, 2005; 41: 209)
|
[6] |
Wang Y, Jiang S L, Zheng Y G, Ke W, Sun W H, Wang J Q. Corros Sci, 2012; 63: 159
|
[7] |
Ni H S, Liu X H, Chang X C, Hou W L, Liu W, Wang J Q. J Alloys Compd, 2009; 46: 163
|
[8] |
Farmer J, Chol J S, Saw C, Haslam J, Day D, Hailey P, Lian T, Rebak R, Perepezko J, Payer J, Branagan D, Beardsley B, Amato A D, Aprigliano L. Metall Mater Trans, 2009; 40A: 1289
|
[9] |
Wang Y, Zheng Y G, Ke W, Sun W H, Hou W L, Chang X C, Wang J Q. Corros Sci, 2011; 53: 3177
|
[10] |
Zhang C, Liu L, Chan K C, Chen Q, Tang C Y. Intermetallics, 2012; 29: 80
|
[11] |
Wang S, Cheng J, Yi S H, Ke L. Trans Nonferrous Met Soc China, 2014; 24: 146
|
[12] |
Chen Q J, Hu L L, Zhou X L, Hua X Z. Rare Met Mater Eng, 2012; 41: 512
|
[12] |
(陈庆军, 胡林丽, 周贤良, 华小珍. 稀有金属材料与工程, 2012; 41: 512)
|
[13] |
Wang Y, Jiang S L, Zheng Y G, Ke W, Sun W H, Wang J Q. Corros Sci, 2012; 63: 159
|
[14] |
Guo J H, Wu J W, Ni X J, Li D R, Lian F Z, Lu Z C. Acta Metall Sin, 2007; 43: 780
|
[14] |
(郭金花, 吴嘉伟, 倪晓俊, 李德仁, 连法增, 卢志超. 金属学报, 2007; 43: 780)
|
[15] |
Pang S J, Zhang T, Asami K, Inoue A. Corros Sci, 2002; 44: 1847
|
[16] |
Wang S L, Yi S. Intermetallics, 2010; 18: 1950
|
[17] |
Liu X Q, Zheng Y G, Chang X C, Hou W L, Wang J Q, Tang Z, Burgess A. J Alloys Compd, 2009; 484: 300
|
[18] |
Wang A P, Chang X C, Hou W L, Wang J Q. Acta Metall Sin, 2006; 42: 537
|
[18] |
(王爱萍, 常新春, 侯万良, 王建强. 金属学报, 2006; 42: 537)
|
[19] |
Cao C N,Zhang J Q. Introduction of Electrochemical Impedance Spectroscopy. Beijing: Science Press, 2002: 118
|
[19] |
(曹楚南,张鉴清. 电化学阻抗谱导论. 北京: 科学出版社, 2002: 118)
|
[20] |
Pardo A, Merino M C, Otero E, Lo'pez M D, M'hichet A. J Non-cryst Solids, 2006; 352: 3179
|
[21] |
Wang W H. Prog Phys, 2013; 33: 177
|
[21] |
(汪卫华. 物理学进展, 2013; 33: 177)
|
[22] |
Scully J R, Payer J H. J Mater Res, 2008; 22: 302
|
[23] |
Wang Z M, Ma Y T, Zhang J, Hou W L, Chang X C, Wang J Q. Electrochim Acta, 2008; 54: 261
|
[24] |
Lloyd A C, Noel J J, McIntyre S, Shoesmith D W. Electrochim Acta, 2004; 49: 3015
|
[25] |
Habazaki H, Kawashima A, Asami K, Hashimoto K. J Electrochem Soc, 1991; 138: 76
|
[26] |
Maurice V, Strehblow H H, Marcus P. J Electrochem Soc, 1999; 146: 524
|
[27] |
Pedraza F, Roman E, Cristobal M J, Hierro M P, Perez F J. Thin Solid Films, 2002; 414: 231
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|