Please wait a minute...
金属学报  2015, Vol. 51 Issue (1): 1-10    DOI: 10.11900/0412.1961.2014.00395
  本期目录 | 过刊浏览 |
梯度纳米结构材料
卢柯()
中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳110016
GRADIENT NANOSTRUCTURED MATERIALS
LU Ke()
Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
引用本文:

卢柯. 梯度纳米结构材料[J]. 金属学报, 2015, 51(1): 1-10.
Ke LU. GRADIENT NANOSTRUCTURED MATERIALS[J]. Acta Metall Sin, 2015, 51(1): 1-10.

全文: PDF(3441 KB)   HTML
摘要: 

本文简要综述了近年来国内外关于梯度纳米结构材料的研究进展, 包括梯度纳米结构的分类, 梯度纳米结构材料的主要性能特点及制备加工技术. 对梯度纳米结构材料面临的一些基础科学问题和工业应用探索进行了讨论和展望.

关键词 : 纳米材料,  梯度纳米结构,  性能,  制备加工    
Abstract:

In this paper, research progresses on gradient nanostructured materials in recent years is briefly reviewed. It includes classification of gradient nanostructures, properties and processing techniques of the gradient nanostructured materials. Perspectives and challenges on scientific understanding and industrial applications of gradient nanostructured materials are addressed.

Key words: nanostructured materials    gradient nanostructure    property    synthesis and processing
收稿日期: 2014-07-18     
ZTFLH:  TG146  
图1  纯Ni 的强度随结构尺寸的变化[4]
图2  梯度纳米结构的分类: 梯度纳米晶粒结构、梯度纳米孪晶结构、梯度纳米层片结构和梯度纳米柱状结构[4]
图3  具有梯度纳米晶粒结构表层纯Cu棒状样品的拉伸曲线[3]及强度-拉伸均匀延伸率匹配
图4  具有梯度纳米晶粒结构表层纯Cu样品在不同拉伸变形量下的硬度随距表面深度的变化关系[19]
图5  梯度纳米材料的强度-塑性匹配与传统粗晶材料、纳米晶材料及纳米晶-粗晶混合材料的比较[24]
图6  Z5CND-16马氏体不锈钢经SMGT处理(及退火)后扭转疲劳性能测试结果[26]
图7  130 ℃时63Ni在纯Cu梯度纳米结构表层中不同层深处扩散系数、晶界扩散系数和孪晶界扩散系数的变化(退火态粗晶态大角晶界的扩散系数作为对比)[28]
图8  原始粗晶纯Fe和具有梯度纳米结构表层的纯Fe样品在300 ℃气体渗氮9 h后的表层截面组织[30]
图9  纯Cu中梯度纳米晶粒结构(GNG)与粗晶结构(CG)在拉伸变形后的表面形貌比较[4]
图10  三种梯度塑性变形方式: 表面压入式梯度变形、表面碾磨式梯度变形和表面碾压式梯度变形[4]
图11  梯度纳米结构表现的一些特性总结[4]
[1] Gleiter H. Prog Mater Sci, 1989; 33: 223
[2] Meyers M A, Mishra A, Benson D J. Prog Mater Sci, 2006; 51: 427
[3] Fang T H, Li W L, Tao N R, Lu K. Science, 2011; 331: 1587
[4] Lu K. In: Faester S, Hansen N, Juul Jensen D, Ralph B, Sun J eds., Proc 35th Riso International Symposium on Materials Science: New Frontiers of Nanometals, Department of Wind Energy, Riso Campus, Technical University of Denmark, 2014: 89
[5] Huang H W, Wang Z B, Lu K. Acta Mater, 2015, in revision
[6] Wang H T, Tao N R, Lu K. Scr Mater, 2013; 68: 22
[7] Liu X C, Zhang H W, Lu K. Science, 2013; 342: 337
[8] Han Z, Zhang Y S, Lu K. J Mater Sci Technol, 2008; 24: 483
[9] Zhang Y S, Han Z, Wang K, Lu K. Wear, 2006; 260: 942
[10] Wang Z B, Tao N R, Li S, Wang W, Liu G, Lu J, Lu K. Mater Sci Eng, 2003; A352: 144
[11] Li G B, Chen J, Guan D L. Tribology Int, 2010; 43: 2216
[12] Ba D M, Ma S N, Meng F J, Li C Q. Surf Coat Technol, 2007; 202: 254
[13] Arun P N, Gnanamoorthy R, Kamaraj M. Mater Sci Eng, 2010;B168: 176
[14] Yan W L, Fang L, Zheng Z G, Sun K, Xu Y H. Tribology Int, 2009; 42: 634
[15] Zhang Y S, Han Z. Tribology Lett, 2007; 27: 53
[16] Sun Y. Tribology Int, 2013; 57: 67
[17] Kumar S A, Raman S G S, Narayanan T S, Gnanamoorthy R. Surf Coat Technol, 2012; 206: 4425
[18] Zhou L, Liu G, Han Z, Lu K. Scr Mater, 2008; 58: 445
[19] Fang T H, Tao N R, Lu K. Scr Mater, 2014; 77: 17
[20] Yong X P. Master Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2001
[20] (雍兴平. 中国科学院金属研究所硕士学位论文, 沈阳, 2001)
[21] Roland T, Retraint D, Lu K, Lu J. Mater Sci Eng, 2007; A445-446: 281
[22] Wu X L, Jiang P, Chen L, Yuan F P, Zhu Y T. Proc Natl Acad Sci United State Am, 2014; 111: 7197
[23] Wei Y J, Li Y Q, Zhu L C, Liu Y, Lei X Q, Wang G, Wu Y X, Mi Z L, Liu J B, Wang H T, Gao H J. Nat Commun, 2014; 5: 3580-1
[24] Lu K. Science, 2014; 345: 1455
[25] Roland T, Retraint D, Lu K, Lu J. Scr Mater, 2006; 54: 1949
[26] Huang H W, Wang Z B, Yong X P, Lu K. Mater Sci Technol, 2013; 29: 1200
[27] Wang Z B, Tao N R, Tong W P, Lu J, Lu K. Acta Mater, 2003; 51: 4319
[28] Wang Z B, Lu K, Wilde G, Divinski S V. Acta Mater, 2010; 58: 2376
[29] Wang H L, Wang Z B, Lu K. Acta Mater, 2012; 60: 1762
[30] Tong W P, Tao N R, Wang Z B, Lu J, Lu K. Science, 2003; 299: 686
[31] Wang Z B, Lu J, Lu K. Acta Mater, 2005; 53: 2081
[32] Lu S D, Wang Z B, Lu K. Mater Sci Eng, 2010; A527: 995
[33] Zhang H W, Wang L, Hei Z K, Liu G, Lu J, Lu K. Z Metall, 2003; 94: 1143
[34] Tong W P, Han Z, Wang L M, Lu J, Lu K. Surf Coat Technol, 2008; 202: 4957
[35] Si X, Lu B N, Wang Z B. J Mater Sci Technol, 2009; 25: 433
[36] Guo S, Wang Z B, Wang L M, Lu K. Surf Coat Technol, 2014; 258: 329
[37] Sun H Q, Shi Y N, Zhang M X, Lu K. Surf Coat Technol, 2008; 202: 3947
[38] Chui P F, Sun K N, Sun C, Yang X Q, Shan T. Appl Surf Sci, 2011; 257: 6787
[39] Raja K S, Namjoshi S A, Misra M. Mater Lett, 2005; 59: 570
[40] Jelliti S, Richard C, Retraint D, Roland T, Chemkhi M, Demangel C. Surf Coat Technol, 2013; 224: 82
[41] Fu T, Zhou Z F, Zhou Y M, Zhu X D, Zeng Q F, Wang C P, Li K Y, Lu J. Surf Coat Technol, 2012; 207: 555
[42] Fu T, Wang C P, Hou B, Zhu X D, Ma S G. China Surf Eng, 2010; 23(5): 64
[42] (付 涛, 王长鹏, 侯 斌, 朱晓东, 马胜哥. 中国表面工程, 2010; 23(5): 64)
[43] Lu K, Lu J. J Mater Sci Technol, 1999; 15: 193
[44] Lu K, Lu J. Mater Sci Eng, 2004; A375-377: 38
[45] Li W L, Tao N R, Lu K. Scr Mater, 2008; 59: 546
[46] Li Y. To be published
[1] 宫声凯, 刘原, 耿粒伦, 茹毅, 赵文月, 裴延玲, 李树索. 涂层/高温合金界面行为及调控研究进展[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] 王磊, 刘梦雅, 刘杨, 宋秀, 孟凡强. 镍基高温合金表面冲击强化机制及应用研究进展[J]. 金属学报, 2023, 59(9): 1173-1189.
[3] 张健, 王莉, 谢光, 王栋, 申健, 卢玉章, 黄亚奇, 李亚微. 镍基单晶高温合金的研发进展[J]. 金属学报, 2023, 59(9): 1109-1124.
[4] 郑亮, 张强, 李周, 张国庆. 增/降氧过程对高温合金粉末表面特性和合金性能的影响:粉末存储到脱气处理[J]. 金属学报, 2023, 59(9): 1265-1278.
[5] 张雷雷, 陈晶阳, 汤鑫, 肖程波, 张明军, 杨卿. K439B铸造高温合金800℃长期时效组织与性能演变[J]. 金属学报, 2023, 59(9): 1253-1264.
[6] 陈礼清, 李兴, 赵阳, 王帅, 冯阳. 结构功能一体化高锰减振钢研究发展概况[J]. 金属学报, 2023, 59(8): 1015-1026.
[7] 丁桦, 张宇, 蔡明晖, 唐正友. 奥氏体基Fe-Mn-Al-C轻质钢的研究进展[J]. 金属学报, 2023, 59(8): 1027-1041.
[8] 李景仁, 谢东升, 张栋栋, 谢红波, 潘虎成, 任玉平, 秦高梧. 新型低合金化高强Mg-0.2Ce-0.2Ca合金挤压过程中的组织演变机理[J]. 金属学报, 2023, 59(8): 1087-1096.
[9] 刘伟, 陈婉琦, 马梦晗, 李恺伦. 聚变堆用W在等离子体作用下的辐照损伤行为研究进展[J]. 金属学报, 2023, 59(8): 986-1000.
[10] 袁江淮, 王振玉, 马冠水, 周广学, 程晓英, 汪爱英. Cr2AlC涂层相结构演变对力学性能的影响[J]. 金属学报, 2023, 59(7): 961-968.
[11] 司永礼, 薛金涛, 王幸福, 梁驹华, 史子木, 韩福生. Cr添加对孪生诱发塑性钢腐蚀行为的影响[J]. 金属学报, 2023, 59(7): 905-914.
[12] 张德印, 郝旭, 贾宝瑞, 吴昊阳, 秦明礼, 曲选辉. Y2O3 含量对燃烧合成Fe-Y2O3 纳米复合粉末性能的影响[J]. 金属学报, 2023, 59(6): 757-766.
[13] 刘俊鹏, 陈浩, 张弛, 杨志刚, 张勇, 戴兰宏. 高熵合金的低温塑性变形机制及强韧化研究进展[J]. 金属学报, 2023, 59(6): 727-743.
[14] 郭福, 杜逸晖, 籍晓亮, 王乙舒. 微电子互连用锡基合金及复合钎料热-机械可靠性研究进展[J]. 金属学报, 2023, 59(6): 744-756.
[15] 梁凯, 姚志浩, 谢锡善, 姚凯俊, 董建新. 新型耐热合金SP2215组织与性能的关联性[J]. 金属学报, 2023, 59(6): 797-811.