| 服役态Cr35Ni45Nb合金高温真空渗碳行为及相演化机理研究 |
彭以超1, 张麦仓1( ), 杜晨阳2, 董建新1 |
1 北京科技大学材料科学与工程学院, 北京 100083 2 中国特种设备检测研究院, 北京 100013 |
|
| HIGH TEMPERATURE VACUUM CARBURIZATION BEHAVIORS AND PHASE EVOLUTION MECHANISMS OF Cr35Ni45Nb ALLOY UNDER SERVICE CONDITION |
PENG Yichao1, ZHANG Maicang1( ), DU Chenyang2, DONG Jianxin1 |
1 School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083 2 China Special Equipment Inspection and Research Institute, Beijing 100013 |
引用本文:
彭以超, 张麦仓, 杜晨阳, 董建新. 服役态Cr35Ni45Nb合金高温真空渗碳行为及相演化机理研究[J]. 金属学报, 2015, 51(1): 11-20.
Yichao PENG,
Maicang ZHANG,
Chenyang DU,
Jianxin DONG.
HIGH TEMPERATURE VACUUM CARBURIZATION BEHAVIORS AND PHASE EVOLUTION MECHANISMS OF Cr35Ni45Nb ALLOY UNDER SERVICE CONDITION[J]. Acta Metall Sin, 2015, 51(1): 11-20.
| [1] |
Khodamorad S H, Haghshenas F D, Rezaie H, Sadeghipour A. Eng Fail Anal, 2012; 21: 1
|
| [2] |
Al-Meshari A, Al-Rabie M, Al-Dajane M. J Fail Anal Prev, 2013; 13: 282
|
| [3] |
Tari V, Najafizadeh A, Aghaei M, Mazloumi M. J Fail Anal Prev, 2009; 9: 316
|
| [4] |
Zhang J, Young D J. Oxid Met, 2008; 70(3-4): 189
|
| [5] |
Chauhan A, Anwar M, Montero K, White H, Si W. J Phase Equilib Diff, 2006; 27: 684
|
| [6] |
Mitchell D, Young D, Kleemann W. Mater Corros, 1998; 49: 231
|
| [7] |
Ramanarayanan T, Petkovic R, Mumford J, Ozekcin A. Mater Corros, 1998; 49: 226
|
| [8] |
Rahmel A, Grabke H, Steinkusch W. Mater Corros, 1998; 49: 221
|
| [9] |
Oquab D, Xu N, Monceau D, Young D. Corros Sci, 2010; 52: 255
|
| [10] |
Kaya A A. Mater Charact, 2002; 49: 23
|
| [11] |
Grabke H, Wolf I. Mater Sci Eng, 1987; A87: 23
|
| [12] |
Giggins C, Pettit F. Oxid Met, 1980; 14: 363
|
| [13] |
Borjali S, Allahkaram S R, Khosravi H. Mater Des, 2012; 34: 65
|
| [14] |
Mostafaei M, Shamanian M, Purmohamad H, Amini M, Saatchi A. Eng Fail Anal, 2011; 18: 164
|
| [15] |
Paz J N, Grabke H. Oxid Met, 1993; 39: 437
|
| [16] |
Petkovic-Luton R, Ramanarayanan T. Oxid Met, 1990; 34: 381
|
| [17] |
Hermse C, Asteman H, IJzerman R, Jakobi D. Mater Corros, 2013; 64: 856
|
| [18] |
Sustaita-Torres I A, Haro-Rodríguez S, Guerrero-Mata M P, de la Garza M, Valdés E, Deschaux-Beaume F, Colás R. Mater Chem Phys, 2012; 133: 1018
|
| [19] |
Kunzru D. In: Sara R K, Ray S, Maity B R, Ganguly S, Bhattacharyya D, Chakraborty S L eds., Petroleum Refining and Petrochemical Based Industries in Eastern India, New Delhi: Allied Publishers Ltd., 2000: 14
|
| [20] |
Kaya A, Krauklis P, Young D. Mater Charact, 2002; 49: 11
|
| [21] |
Bennett M, Price J. J Mater Sci, 1981; 16: 170
|
| [22] |
Song R K, Zhang M C, Dong J X, Du C Y. Adv Mater Res, 2014; 834: 390
|
| [23] |
Ryzhov N, Smirnov A, Fakhurtdinov R, Mulyakaev L, Gromov V. Met Sci Heat Treat, 2004; 46: 230
|
| [24] |
Ramanarayanan T, Srolovitz D. J Electrochem Soc, 1985; 132: 2268
|
| [25] |
Wagner C. J Electrochem Soc, 1952; 99(10): 369
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|