| 2099合金热变形过程中的动态软化机制* |
| 张飞1,2, 沈健1, 闫晓东1, 孙建林2, 蒋呐3, 周华3 |
1 北京有色金属研究总院, 北京 100088 2 北京科技大学材料科学与工程学院, 北京 100083 3 西南铝业(集团)有限责任公司, 重庆 401326 |
|
| DYNAMIC SOFTENING MECHANISM OF 2099 ALLOY DURING HOT DEFORMATION PROCESS |
| ZHANG Fei1,2, SHEN Jian1, YAN Xiaodong1, SUN Jianlin2, JIANG Na3, ZHOU Hua3 |
1 Beijing General Research Institute for Non-ferrous Metals, Beijing 100088 2 School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083 3 Southwest Aluminum (Group) Co., Ltd, Chongqing 401326 |
引用本文:
张飞, 沈健, 闫晓东, 孙建林, 蒋呐, 周华. 2099合金热变形过程中的动态软化机制*[J]. 金属学报, 2014, 50(6): 691-699.
Fei ZHANG,
Jian SHEN,
Xiaodong YAN,
Jianlin SUN,
Na JIANG,
Hua ZHOU.
DYNAMIC SOFTENING MECHANISM OF 2099 ALLOY DURING HOT DEFORMATION PROCESS[J]. Acta Metall Sin, 2014, 50(6): 691-699.
| [1] |
Jabra J, Romios M, Lai J, Lee E, Setiawan M, Lee E W, Witters J, Abourialy N, Ogren J R, Oppenheim T, Frazier W E, Es-Said O S. J Mater Eng Perform, 2006; 15: 601
|
| [2] |
Ma Y, Zhou X, Thompson G E, Hashimoto T, Thomson P, Fowles M. Mater Chem Phys, 2011; 126: 46
|
| [3] |
Romios M, Tiraschi R, Parrish C, Babel H W, Ogren J R, Es-Said O S. J Mater Eng Perform, 2005; 14: 641
|
| [4] |
Ward N, Tran A, Abad A, Lee E W, Hahn M, Fordan E, Es-Said O S. J Mater Eng Perform, 2011; 20: 989
|
| [5] |
Wei X Y, Zheng Z Q, She L J, Chen Q N, Li S C. Rare Met Mater Eng, 2010; 39: 1583
|
| [5] |
(魏修宇, 郑子樵, 佘玲娟, 陈秋妮, 李世晨. 稀有金属材料与工程, 2010; 39: 1583)
|
| [6] |
Gourdet S, Montheillet F. Mater Sci Eng, 2000; A283: 274
|
| [7] |
Tajally M, Huda Z, Masjuki H H. Met Sci Heat Treat, 2011; 53: 165
|
| [8] |
Hu H E, Zhen L, Zhang B Y, Yang L, Chen J Z. Mater Charact, 2008; 59: 1185
|
| [9] |
Faivre P, Doherty R D. J Mater Sci, 1979; 14: 897
|
| [10] |
Wan J L, Sun X J, Gu J L, Chen N P. Acta Metall Sin, 1999; 35:1031
|
| [10] |
(万菊林, 孙新军, 顾家琳, 陈南平. 金属学报, 1999; 35: 1031)
|
| [11] |
Xu X J, Wang B, Wu G C, Zhang F B, Song T, Luo Y, Cheng X N. Rare Met Mater Eng, 2011; 40(Suppl 2): 248
|
| [11] |
(许晓静, 王 彬, 吴桂潮, 张福豹, 宋 涛, 罗 勇, 程晓农. 稀有金属材料与工程, 2011; 40(增刊2): 248)
|
| [12] |
Song T, Xu X J, Fan Z, Luo Y, Wang B, Wu G C, Zhang Z Q, Zhang Y K. Rare Met Mater Eng, 2012; 41(Suppl 2): 374
|
| [12] |
(宋 涛, 许晓静, 范 真, 罗 勇, 王 彬, 吴桂潮, 张振强, 张允康. 稀有金属材料与工程, 2012; 41(增刊2): 374)
|
| [13] |
Zhu X H, Zheng Z Q, Zhong S. Chin J Nonferrous Met, 2010; 20: 1861
|
| [13] |
(朱小辉, 郑之樵, 钟 申. 中国有色金属学报, 2010; 20: 1861)
|
| [14] |
Fragomeni J, Wheeler R, Jata K V. J Mater Eng Perform, 2005; 14: 18
|
| [15] |
Song T, Xu X J, Fan Z, Zhang Z Q, Wang B, Luo Y. Chin J Rare Met, 2012; 36: 196
|
| [15] |
(宋 涛, 许晓静, 范 真, 张振强, 王 彬, 罗 勇. 稀有金属, 2012; 36: 196)
|
| [16] |
Kertz J E, Gouma P I, Buchheit R G. Metall Mater Trans, 2001; 32A: 2561
|
| [17] |
Csontos A A, Starke E A. Metall Mater Trans, 2000; 31A: 1965
|
| [18] |
Odeshi A G, Adesola A O, Badmos A Y. Eng Fail Anal, 2013; 35: 302
|
| [19] |
Zhang F, Shen J, Yan X D, Sun J L, Sun X L, Yang Y. Rare Met, 2014; 33: 28
|
| [20] |
Shen J. Chin J Nonferrous Met, 2001; 11: 593
|
| [20] |
(沈 健. 中国有色金属学报, 2001; 11: 593)
|
| [21] |
Rao K P, Prasad Y V R K. J Mech Work Technol, 1986; 13: 83
|
| [22] |
Li W, Li H, Wang Z X, Zheng Z Q. Mater Sci Eng, 2011; A528: 4101
|
| [23] |
Li J C M. J Appl Phys, 1962; 33: 2965
|
| [24] |
Samantaray D, Mandal S, Bhaduri A K. Mater Des, 2010; 31: 982
|
| [25] |
Song W X. Metallography. 2nd Ed., Beijing: Metallurgical Industry Press, 2010: 189
|
| [25] |
(宋维锡. 金属学. 第二版, 北京: 冶金工业出版社, 2010: 189)
|
| [26] |
Shen J. PhD Dissertation, Central South University of Technology, Changsha, 1996
|
| [26] |
(沈 健. 中南工业大学博士学位论文, 长沙, 1996)
|
| [27] |
Wang Y, Shao W Z, Zhen L, Zhang X M. Mater Sci Eng, 2008; A486: 321
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|