| X80管线钢高pH应力腐蚀开裂机制与电位的关系 |
| 范林,刘智勇,杜翠薇,李晓刚 |
| 北京科技大学腐蚀与防护中心教育部腐蚀与防护重点实验室, 北京100083 |
|
| RELATIONSHIP BETWEEN HIGH pH STRESS CORROSION CRACKING MECHANISMS AND APPLIED POTENTIALS OF X80 PIPELINE STEEL |
| FAN Lin, LIU Zhiyong, DU Cuiwei, LI Xiaogang |
| Key Laboratory of Chinese Ministry of Education for Corrosion and Protection, Corrosion and Protection Center, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
范林,刘智勇,杜翠薇,李晓刚. X80管线钢高pH应力腐蚀开裂机制与电位的关系[J]. 金属学报, 2013, 49(6): 689-698.
FAN Lin,
LIU Zhiyong,
DU Cuiwei,
LI Xiaogang.
RELATIONSHIP BETWEEN HIGH pH STRESS CORROSION CRACKING MECHANISMS AND APPLIED POTENTIALS OF X80 PIPELINE STEEL[J]. Acta Metall Sin, 2013, 49(6): 689-698.
| [1] Liang P, Li X G, Du C W, Chen X. Mater Des, 2009;30: 1712
[2] Gu B, Luo J L, Mao X. Corrosion, 1999; 55: 96
[3] Cheng Y F. J Mater Sci, 2007; 42: 2701
[4] Eslami A, Fang B, Kania R, Worthingham B, Been J, Eadie R,Chen W. Corros Sci, 2010; 52: 3750
[5] Eslami A, Kania R, Worthingham B, Boven G V, Eadie R, ChenW. Corros Sci, 2011; 53: 2318
[6] Torres-Islas A, Gonzalez-Rodriguez J G, Uruchurtu J,Serna S. Corros Sci, 2008; 50: 2831
[7] Liu Z Y, Li X G, Du C W, Zhai G L, Cheng Y F.Corros Sci, 2008; 50: 2251
[8] Zhang L, Li X G, Du C W, Huang Y Z. Mater Des,2009; 30: 2259
[9] Xiao J, Wu M, Chen X, Wang C X. Mater HeatTreat, 2010; 39(18): 28
(肖军, 吴明, 陈旭, 王成祥. 材料热处理技术, 2010; 39(18):28)
[10] Zhang L, Li X G, Du C W, Liang P. J Chin Soc Corros Prot, 2009; 29: 353
(张亮, 李晓刚, 杜翠薇, 梁平. 中国腐蚀与防护学报, 2009; 29:353)
[11] Chen X, Wu M, He C, Xiao J. Acta Metall Sin,2010; 46: 951
(陈旭, 吴明, 何川, 肖军. 金属学报, 2010; 46: 951)
[12] Parkins R N. Corros Sci, 1980; 20: 147
[13]Charles E A, Parkins R N. Corrosion, 1995; 51: 518
[14] Parkins R N. Corrosion, 1996; 52: 363
[15] Liu Z Y, Zhai G L, Du C W, Li X G. Acta Metall Sin, 2008; 44: 209
(刘智勇, 翟国丽, 杜翠薇, 李晓刚. 金属学报, 2008; 44: 209)
[16] Liu Z Y, Wang C P, Du C W, Li X G. Acta Metall Sin, 2011; 47: 1434
(刘智勇, 王长朋, 杜翠薇, 李晓刚. 金属学报, 2011; 47: 1434)
[17] Parkins R N, Zhou S. Corros Sci, 1997; 39: 175
[18] Parkins R N, O'Dell C S, Fessler R R. Corros Sci,1984; 24: 343
[19] Thomas J G N, Nurse T J, Walker R. Br Corros J,1970; 5: 87
[20] Cheng Y F, Niu L. Electrochem Commun, 2007; 9:558
[21] Yan M C, Wang J Q, Han E H, Ke W. Corros Sci,2008; 50: 1331
[22] Li M C, Cheng Y F. Electrochim Acta, 2007; 52:8111
[23] Bouaeshi W, Ironside S, Eadie R. Corrosion, 2007;63: 648
[24] Beavers J A, Harle B A. J Offshore Mech Arctic Eng, 2001; 123: 147
[25] Liu Z Y, Li X G, Zhang Y R, Du C W, Zhai G L. Acta Metall Sin (Eng Lett), 2009; 22: 58
|
|