Please wait a minute...
金属学报  2013, Vol. 49 Issue (11): 1411-1415    DOI: 10.3724/SP.J.1037.2013.00492
  论文 本期目录 | 过刊浏览 |
Nb微合金化Fe14Si2高硅钢温轧板织构演变规律
杨琨,梁永锋,叶丰,林均品
北京科技大学新金属材料国家重点实验室, 北京 100083
TEXTURE EVOLUTION OF Nb MICRO-ALLOYED Fe14Si2 HIGH SILICON STEEL DURING WARM ROLLING
YANG Kun, LIANG Yongfeng, YE Feng, LIN Junpin
State Key Laboratory for Advanced Metal and Materials, University of Science and Technology Beijing, Beijing 100083
引用本文:

杨琨,梁永锋,叶丰,林均品. Nb微合金化Fe14Si2高硅钢温轧板织构演变规律[J]. 金属学报, 2013, 49(11): 1411-1415.
YANG Kun, LIANG Yongfeng, YE Feng, LIN Junpin. TEXTURE EVOLUTION OF Nb MICRO-ALLOYED Fe14Si2 HIGH SILICON STEEL DURING WARM ROLLING[J]. Acta Metall Sin, 2013, 49(11): 1411-1415.

全文: PDF(2634 KB)  
摘要: 

采用Nb对Fe-6.5%Si(质量分数)高硅钢进行微合金化处理, 结果表明:Nb在高硅钢薄板制备过程中细晶效果明显.铸态、锻态和热轧态组织的晶粒分别细化了17.50%, 24.51%和30.13%.铸态样品压缩强度由1365 MPa提高至1520 MPa, 延伸率提高77.78%; 温轧板试样室温拉伸强度由573 MPa提高至621 MPa,延伸率提高44.44%. 利用XRD对厚度为0.30-1.68 mm的温轧板的板面织构演变过程进行跟踪测量, 结果发现:初始织构以(011)<100>Goss织构为主, 单道次变形量为26.2%的情况下,Goss织构完全转化为(100)<011>旋转立方织构, 随后,在单道次变形为22.6%的情况下, 旋转立方织构完全转化为{111}面织构,即纤维织构, 并稳定保持至0.30 mm.

关键词 : Fe-6.5%Si,  织构,  Nb微合金化,  细晶,  Fe14Si2    
Abstract:

Fe-6.5%Si (mass fraction) alloy possess perfect magnetic properties,though intermetallics of Fe14Si2 phase brought 6.5%Si leads to room temperature brittleness and hinder this significant materials industrialization. Nb was adopted into micro-alloying of Fe-6.5%Si high silicon steel. OM, thermal simulated test machine and XRD were employed to study the influence of Nb on high silicon steel in processing stages. Textures of warm-rolled high silicon steel strips were determined by XRD. The results indicate that Nb could refine the grains during fabrication of high silicon steel. Comparing to the non-Nb micro-alloyed high silicon steel, the grain size were reduced 17.50%, 24.51% and 30.13% in as-cast, forged and hot-rolled microstructure. Compression strength of as-cast specimen was enhanced from 1365 MPa to 1520 MPa with elongation rate from 0.225% to 0.400%. Tensile strength of warm-rolled strip was increased from 573 MPa to 621 MPa with elongation rate from 0.018% to 0.026%. XRD was carried out to indicate the surface texture evolution of warm-rolled high silicon steel with thickness from 0.30-1.68 mm during the warm rolling. The original (011)<100> Goss texture totally transformed to (100)>011> rotating cubetexture with single pass deformation of 26.2%. Then, rotating cube texture completely transformed to {111} fiber texture which remains until the thickness of 0.30 mm with single pass deformation of 22.6%.

Key words: Fe-6.5%Si    texture    Nb micro-alloying    grain-refining    Fe14Si2
收稿日期: 2013-08-15     
基金资助:

国家重点基础研究发展计划项目2011CB606304-2,国家高技术研究发展计划项目2012AA03A505和中央高校基本科研业务费专项资金项目资助

作者简介: 杨琨, 男, 1982年生, 博士生

[1] Paolinelli S C, Cunha M A. J Magn Magn Mater, 2006; 304: e596

[2] Raviprasad K, Chattopadhyay K. Acta Matall Mater, 1993; 41: 609
[3] Haiji H, Okada K, Hiratani T, Abe M, Ninomiya M. J Magn Magn Mater, 1996; 160: 109
[4] Phway T P P, Moses A J. J Magn Magn Mater, 2008; 320: E611
[5] Oda Y J, Kohno M, Honda A. J Magn Magn Mater, 2008; 320: 2430
[6] Cunha M A, Paolinelli S. J Magn Magn Mater, 2008; 320: 2485
[7] Liang Y F, Lin J P, Ye F, Wang Y L, Chen G L. Met Funct Mater, 2010; 17(2): 43
(梁永锋, 林均品, 叶丰, 王艳丽, 陈国良. 金属功能材料. 2010; 17(2): 43)
[8] Pan L M, Jin J N, Lin J P, Wang J G, Wang Y L, Lin Z, Chen G L. J Funct Mater, 2004; 35: 683
(潘丽梅, 金吉男, 林均品, 王建国, 王艳丽, 林志, 陈国良. 功能材料, 2004; 35: 683)
[9] Ye F, Liang Y F, Wang Y L, Lin J P, Chen G L. Mater Sci Forum, 2010; 638-642: 1428
[10] Chang P H, Preban A G. Acta Metall, 1985; 33: 897
[11] Jiang Z H, Guan Z Z, Lian J S. Mater Sci Eng, 1995; A190: 55
[12] Son Y I, Lee Y K, Park K T, Lee C S, Shin D H. Acta Mater, 2005; 53: 3125
[13] Tsipouridis P, Werner E, Krempaszky C, Tragl E. Steel Res Int, 2006; 77: 654
[14] Delince M, Brechet Y, Embury J D, Geers M G D, Jacques P J, Pardoen T.Acta Mater, 2007; 55: 2337
[15] Mukherjee K, Hazra S S, Militzer M. Metall Mater Trans, 2009; 40A: 2145
[16] Xue C F, Wang X H, Xin Y D. Heat Treat Met, 2003; 28(5): 15
(薛春芳, 王新华, 辛义德. 金属热处理, 2003; 28(5): 15)
[17] Chen S S. Heat Treat Met Abroad, 1996; 17(1-2): 5
(陈善述. 国外金属热处理, 1996; 17(1-2): 5)
[18] Zhao J, Xu H F, Shi J, Li J, Pu J, Cao W Q.  Iron Steel, 2012; 47(8): 57
(赵杰, 徐海峰, 时捷, 李箭, 蒲健, 曹文全. 钢铁, 2012; 47(8): 57)
[19] Szkliniarz A. Solid State Phenom, 2012; 191: 221
[20] Weng Y Q. Super Fine Grained Steels. Beijing: Metallurgical Industry Press, 2008: 327
(翁宇庆. 超细晶钢. 北京: 冶金工业出版社, 2008: 327)
[21] Lu J, Jin L, Zeng X Q, Ding W J. Foundry Eng, 2008; (1): 32
(路军, 靳丽, 曾小勤, 丁文江. 铸造工程, 2008; (1): 32)
[22] Belyakov A, Gao W, Miura H, Sakai T. Metall Mater Trans, 1998; 29A: 2957
[23] Zhong T B, Lin J P, Chen G L.  J Funct Mater, 2000; 31: 361
(钟太彬, 林均品, 陈国良. 功能材料, 2000; 31: 361)
[24] Liu J L, Sha Y H, Zhang F, Yao Y C, Li J C, Zuo L.  Funct Mater, 2011; 42: 2089
(柳金龙, 沙玉辉, 张芳, 姚勇创, 李继超, 左良. 功能材料, 2011; 42: 2089)
[1] 常松涛, 张芳, 沙玉辉, 左良. 偏析干预下体心立方金属再结晶织构竞争[J]. 金属学报, 2023, 59(8): 1065-1074.
[2] 刘满平, 薛周磊, 彭振, 陈昱林, 丁立鹏, 贾志宏. 后时效对超细晶6061铝合金微观结构与力学性能的影响[J]. 金属学报, 2023, 59(5): 657-667.
[3] 朱云鹏, 覃嘉宇, 王金辉, 马鸿斌, 金培鹏, 李培杰. 机械球磨结合粉末冶金制备AZ61超细晶镁合金的组织与性能[J]. 金属学报, 2023, 59(2): 257-266.
[4] 娄峰, 刘轲, 刘金学, 董含武, 李淑波, 杜文博. 轧制态Mg-xZn-0.5Er合金板材组织及室温成形性能[J]. 金属学报, 2023, 59(11): 1439-1447.
[5] 孙毅, 郑沁园, 胡宝佳, 王平, 郑成武, 李殿中. 3Mn-0.2C中锰钢形变诱导铁素体动态相变机理[J]. 金属学报, 2022, 58(5): 649-659.
[6] 姜伟宁, 武晓龙, 杨平, 顾新福, 解清阁. 热轧硅钢表层动态再结晶区形成规律及剪切织构特征[J]. 金属学报, 2022, 58(12): 1545-1556.
[7] 杨平, 王金华, 马丹丹, 庞树芳, 崔凤娥. 成分对真空脱锰法相变控制高硅电工钢{100}织构的影响[J]. 金属学报, 2022, 58(10): 1261-1270.
[8] 陈胜虎, 戎利建. 超细晶铁素体-马氏体钢的高温氧化成膜特性及其对Pb-Bi腐蚀行为的影响[J]. 金属学报, 2021, 57(8): 989-999.
[9] 丁宁, 王云峰, 刘轲, 朱训明, 李淑波, 杜文博. 高应变速率多向锻造Mg-8Gd-1Er-0.5Zr合金的微观组织、织构及力学性能[J]. 金属学报, 2021, 57(8): 1000-1008.
[10] 颜孟奇, 陈立全, 杨平, 黄利军, 佟健博, 李焕峰, 郭鹏达. 热变形参数对TC18钛合金β相组织及织构演变规律的影响[J]. 金属学报, 2021, 57(7): 880-890.
[11] 林鹏程, 庞玉华, 孙琦, 王航舵, 刘东, 张喆. 45钢块体超细晶棒材3D-SPD轧制法[J]. 金属学报, 2021, 57(5): 605-612.
[12] 左良, 李宗宾, 闫海乐, 杨波, 赵骧. 多晶Ni-Mn-X相变合金的织构化与功能行为[J]. 金属学报, 2021, 57(11): 1396-1415.
[13] 许占一, 沙玉辉, 张芳, 章华兵, 李国保, 储双杰, 左良. 取向硅钢二次再结晶过程中的取向选择行为[J]. 金属学报, 2020, 56(8): 1067-1074.
[14] 彭云,宋亮,赵琳,马成勇,赵海燕,田志凌. 先进钢铁材料焊接性研究进展[J]. 金属学报, 2020, 56(4): 601-618.
[15] 于雷,罗海文. 部分再结晶退火对无取向硅钢的磁性能与力学性能的影响[J]. 金属学报, 2020, 56(3): 291-300.