| 一种镍基高温合金PLC效应的温度依赖性研究 |
| 韩国明1),崔传勇1),谷月峰2),胡壮麒1),孙晓峰1) |
1)中国科学院金属研究所, 沈阳 110016
2) National Institute for Materials Science,Tsukuba 305-0047, Japan |
|
| INVESTIGATION OF TEMPERATURE DEPENDENCE OF PLC EFFECT IN A NICKEL BASE SUPERALLOY |
| HAN Guoming1), CUI Chuanyong1), GU Yuefeng2), HU Zhuangqi1), SUN Xiaofeng1) |
1) Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
2) National Institute for Materials Science, Tsukuba 305-0047, Japan |
引用本文:
韩国明,崔传勇,谷月峰,胡壮麒,孙晓峰. 一种镍基高温合金PLC效应的温度依赖性研究[J]. 金属学报, 2013, 49(10): 1243-1247.
HAN Guoming,
CUI Chuanyong,
GU Yuefeng,
HU Zhuangqi,
SUN Xiaofeng.
INVESTIGATION OF TEMPERATURE DEPENDENCE OF PLC EFFECT IN A NICKEL BASE SUPERALLOY[J]. Acta Metall Sin, 2013, 49(10): 1243-1247.
| [1] Cottrell A H. Philos Mag, 1953; 44: 829
[2] Beukel Den Van A. Phys Status Solidi, 1975; 30: 197
[3] McCormick P G. Acta Metall, 1972; 20: 351
[4] Kubin L P, Estrin Y. Acta Metall, 1990; 38: 697
[5] Zavattieri P D, Savic V, Hector Jr L G, Fekete J R, Tong W, Xuan Y. Int J Plast, 2009; 25: 2298
[6] Jiang H F, Chen X D, Fan Z C, Dong J, Jiang H, Lu S X. Acta Metall Sin, 2009; 45: 326
(江慧丰, 陈学东, 范志超, 董杰, 姜恒, 陆守香. 金属学报, 2009; 45: 326)
[7] Balik J, Luka P. Acta Metall, 1993; 41: 1447
[8] Jiang H, Zhang Q, Chen X, Chen Z, Jiang Z, Wu X, Fan J. Acta Metall, 2007; 55: 2219
[9] Schaarwachter W, Ebener H. Acta Metall, 1990; 38: 195
[10] Nortmann A, Schwink C. Acta Metall, 1997; 45: 2043
[11] Hayes R W, Hayes W C. Acta Metall, 1982; 30: 1295
[12] Nalawade S A, Sundararaman M, Kishore R, Shah J G. Scr Mater, 2008; 59: 991
[13] Gopinath K, Gogia A K, Kamat S V, Ramamurty U. Acta Mater, 2009; 57: 1243
[14] Brechet Y, Estrin Y. Acta Metall Mater, 1995; 43: 955
[15] Cui C Y, Gu Y F, Yuan Y, Harada H. Scr Mater, 2011; 64: 502
[16] Chihab K, Fressengeas C. Mater Sci Eng, 2003; A356: 102
[17] McCormick P G. Acta Metall, 1971; 19: 463
[18] Pink E. Acta Metall, 1989; 37: 1773
[19] Chmelik F, Pink E, Krol J, Balik J, Pesicka J, Luka P. Acta Mater, 1998; 46: 4435
[20] Fu S, Cheng T, Zhang Q, Hu Q, Cao P. Acta Mater, 2012; 60: 6650
[21] Chihab K, Estrin Y, Kubin L P, Vergnol J. Scr Mater, 1987; 21: 203
[22] Rodriguez P. Bull Mater Sci, 1984; 6: 653
[23] Charnock W. Philos Mag, 1969; 20: 427
[24] Cao P T. PhD Dissertation, University of Science and Technology of China, Hefei, 2010
(曹鹏涛. 中国科学技术大学博士学位论文, 合肥, 2010)
[25] Hayes R W. Acta Mater, 1983; 31: 365
[26] Shankar V, Valsan M, Rao K B S, Manan S L. Metall Trans, 2004; 35A: 3129
[27] Hale C L, Rollings W S, Weaver M L. Mater Sci Eng, 2001; A300: 153 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|