| 锆合金在LiOH水溶液中腐蚀的各向异性研究 |
| 孙国成1, 2), 周邦新1, 2), 姚美意1, 2), 谢世敬1, 2), 李强1, 2) |
1) 上海大学微结构重点实验室, 上海 200444
2) 上海大学材料研究所, 上海 200072 |
|
| STUDY OF ANISOTROPIC BEHAVIOR FOR ZIRCONIUM ALLOYS CORRODED IN LITHIATED WATER |
| SUN Guocheng1, 2), ZHOU Bangxin1, 2), YAO Meiyi1, 2), XIE Shijing1, 2), LI Qiang 1, 2) |
1) Laboratory for Microstructures, Shanghai University, Shanghai 200444
2) Institute of Materials, Shanghai University, Shanghai 200072 |
引用本文:
孙国成 周邦新 姚美意 谢世敬 李强. 锆合金在LiOH水溶液中腐蚀的各向异性研究[J]. 金属学报, 2012, 48(9): 1103-1108.
,
,
,
,
.
STUDY OF ANISOTROPIC BEHAVIOR FOR ZIRCONIUM ALLOYS CORRODED IN LITHIATED WATER[J]. Acta Metall Sin, 2012, 48(9): 1103-1108.
| [1] Garzarolli F, Seidel H, Tricot R, Gros J P. In: Eucken C M, Garde A M eds., Zirconium in the Nuclear Industry: 9th International Symposium, ASTM STP 1132, Baltimore: ASTM International, 1991: 395[2] Yilmazbayhan A, Breval E, Motta A T, Comstock R J. J Nucl Mater, 2006; 349: 265[3] Zhou B X, Li Q, Yao M Y, Liu W Q, Chu Y L. In: Kammenzind B, Limb¨ack M eds., Zirconium in the Nuclear Industry: 15th International Symposium, ASTM STP 1505, Baltimore: ASTM International, 2009: 360[4] Park J Y, Choi B K, Yoo S J, Jeong Y H. In: Kammenzind B, Limb¨ack M eds., Zirconium in the Nuclear Industry: 15th International Symposium, ASTM STP 1505, Baltimore: ASTM International, 2009: 471[5] Kim H G, Kim T H, Jeong Y H. J Nucl Mater, 2002; 306: 44[6] Zhou B X, Peng J C, Yao M Y, Li Q, Xia S, Du C X, Xu G. In: Limb¨ack M, Barb´eris P eds., Zirconium in the Nuclear Industry: 16th International Symposium, ASTM STP 1529, Bridgeport: ASTM International, 2011: 620[7] Charquet D, Tricot R, Wadier J E. In: Van Swam L F P, Eucken C M eds., Zirconium in the Nuclear Industry: 8th International Symposium, ASTM STP 1023, Baltimore: ASTM International, 1989: 374[8] Wang C T, Eucken C M, Graham R A. In: Eucken C M, Garde A M eds., Zirconium in the Nuclear Industry: 9th International Symposium, ASTM STP 1132, Baltimore: ASTM International, 1991: 319[9] Kearns J J. Report No.WAPD–TM–472, Report of Westinghouse Electric Corporation, Bettis Atomic Power Laboratory, Pittsburgh, PA, 1965: 2[10] Han J H, Rheem K S. J Nucl Mater, 1994; 217: 197[11] Pecheur D, Godlewski J, Billot P, Thomazet J. In: Sabol G P, Bradley E R eds., Zirconium in the Nuclear Industry: 11th International Symposium, ASTM STP 1295, Ann Arbor: ASTM International, 1996: 94[12] Sabol G P, Kilp G R, Balfour M G, Roberts E. In: Van Swam L F P, Eucken C M eds., Zirconium in the Nuclear Industry: 8th International Symposium, ASTM STP 1023, Baltimore: ASTM International, 1989: 227[13] Nikulina A V, Markelov V A, Peregud M M, Bibilashvili Y K, Kotrekhov V A, Lositsky A F, Kuzmenko N V, Shevnin YP, ShamardinVK, KobylyanskyGP, NovoselovAE. In:Sabol G P, Bradley E R eds., Zirconium in the Nuclear Industry: 11th International Symposium, ASTM STP 1295, Ann Arbor: ASTM International, 1996: 785[14] Zhou B X, Li Q, Huang Q, Miao Z, Zhao W J, Li C. Nucl Power Eng, 2000; 21: 439(周邦新, 李强, 黄强, 苗 志, 赵文金, 李聪. 核动力工程, 2000; 21: 439)[15] Zhou B X, Yao M Y, Li Z K,Wang X M, Zhou J, Long C S, Liu Q, Luan B F. J Mater Sci Technol, 2012; 28: 606[16] Zhou B X, Li Q, YaoMY, LiuWQ, Chu Y L. Nucl Power Eng, 2005; 26: 364(周邦新, 李强, 黄 强, 苗 志, 赵文金, 李 聪. 核动力工程, 2000; 21: 439)[17] Zhou B X, Li Q, Yao M Y, Liu W Q, Chu Y L. Corros Prot, 2009; 30: 589(周邦新, 李强, 姚美意, 刘文庆, 褚于良. 腐蚀与防护, 2009; 30: 589)[18] Du C X, Peng J C, Li H, Zhou B X. Acta Metall Sin, 2011; 47: 887(杜晨曦, 彭剑超, 李慧, 周邦新. 金属学报, 2011; 47: 887)[19] Geng J Q, Zhou B X, Yao M Y, Wang J H, Zhang X, Li S L, Du C X. J Shanghai Univ (Nat Sci Ed), 2011; 17: 293(耿建桥, 周邦新, 姚美意, 王锦红, 张欣, 李士炉, 杜晨曦. 上海大学学报(自然科学版), 2011; 17: 293)[20] Cox B. J Nucl Mater, 2005; 336: 331[21] Liu W Q, Zhou B X, Li Q. Nucl Power Eng, 2002; 23: 68(刘文庆, 周邦新, 李强. 核动力工程, 2002; 23: 68)[22] Zhou B X, Yao M Y, Li Q, Xia S, Liu W Q, Chu Y L. Rare Met Mater Eng, 2007; 36: 1317(周邦新, 姚美意, 李强, 夏爽, 刘文庆, 褚于良. 稀有金属材料与工程, 2007; 36: 1317) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|