| 抗菌时效处理对含Cu双相不锈钢组织和性能的影响 II. 耐蚀及抗菌性能 |
| 向红亮, 范金春, 刘东, 顾兴 |
| 福州大学机械工程及自动化学院, 福州 350108 |
|
| EFFECTS OF ANTIBACTERIAL AGING TREATMENT ON MICROSTRUCTURE AND PROPERTIES OF COPPER-CONTAINING DUPLEX STAINLESS STEEL
II. Corrosion Resistance and Antibacterial Properties |
| XIANG Hongliang, FAN Jinchun, LIU Dong, GU Xing |
| School of Mechanical Engineering and Automation, Fuzhou University, Fuzhou 350108 |
引用本文:
向红亮 范金春 刘东 顾兴. 抗菌时效处理对含Cu双相不锈钢组织和性能的影响 II. 耐蚀及抗菌性能[J]. 金属学报, 2012, 48(9): 1089-1096.
,
,
,
.
EFFECTS OF ANTIBACTERIAL AGING TREATMENT ON MICROSTRUCTURE AND PROPERTIES OF COPPER-CONTAINING DUPLEX STAINLESS STEEL
II. Corrosion Resistance and Antibacterial Properties[J]. Acta Metall Sin, 2012, 48(9): 1089-1096.
| [1] Suzuki S, Nakamura S, Ookubo N, Hasegawa M, Miyakuso K. CAMP–ISIJ, 1999; 12: 518[2] Chen S H, L¨u M Q, Zhang J D, Dong J S, Yang K. Acta Metall Sin, 2004; 40: 314(陈四红, 吕曼祺, 张敬党, 董加胜, 杨 柯. 金属学报, 2004; 40: 314)[3] Nan L, Liu Y Q, Yang W C, Xu H, Li Y, Lu M Q, Yang K. Acta Metall Sin, 2007; 43: 1065(南黎, 刘永前, 杨伟超, 徐慧, 李瑛, 吕曼祺, 杨 柯. 金属学报, 2007; 43: 1065)[4] Zhang Z X, Lin G, Xu Z. J Mater Process Technol, 2008; 205: 419[5] Nan L, Yang K. J Mater Sci Technol, 2010; 26: 941[6] Yang K, Dong J S, Chen S H, L¨u M Q. Chin J Mater Res, 2006; 20: 523(杨 柯, 董加胜, 陈四红, 吕曼棋. 材料研究学报, 2006; 20: 523)[7] Nan L, Yang W C, Liu Y Q, Xu H, Li Y, L¨u M Q, Yang K. J Mater Sci Technol, 2008; 24: 197[8] Hong I T, Koo C H. Mater Sci Eng, 2005; A393: 213[9] Wang X L, Zhao R D, Zhang W Q, Zhu H F. Spec Steel, 2006; 27(5): 35(王小丽, 赵荣达, 张伟强, 朱宏飞. 特殊钢, 2006; 27(5): 35)[10] Xiang H L, Fan J C, Liu D, Guo P P. Acta Metall Sin, 2012; 48: 1081(向红亮, 范金春, 刘东, 郭培培. 金属学报, 2012; 48: 1081)[11] Gong J, Jiang Y M, Deng B, Xu J L, Hu J P, Li J. Electroc Acta, 2010; 55: 5077[12] Yang K, Lu M Q. J Mater Sci Technol, 2007; 23: 333[13] Fu Y, Lin C J, Cai W D. Acta Metall Sin, 2005; 41: 302(付 燕, 林昌健, 蔡文达. 金属学报, 2005; 41: 302)[14] Jinil S, Sangshik K, Jehyun L, Byunghak C. Metall Mater Trans, 2003; 34A: 1617[15] Sourisseau T, Chauveau E, Baroux B. Corros Sci, 2005; 47: 1097[16] Banas J, Mazurkiewicz A. Mater Sci Eng, 2000; A277: 183[17] Wei B M. The Theory of Metal Corrosion and Application. Beijing: Chemical Industry Press, 1984: 37(魏宝明. 金属腐蚀理论及应用. 北京: 化学工业出版, 1984: 37)[18] Trethewey K R, Paton M. Mater Lett, 2004; 58: 3381[19] Lo I H, Fu Y, Lin C J, Tsai W T. Corros Sci, 2006; 48: 696[20] Xiao J M. The Metallurgical Problems of Stainless Steels. Beijing: Metallurgy Industry Press, 2006: 164(肖纪美. 不锈钢的金属学问题. 北京: 冶金工业出版社, 2006: 164)[21] Zhang Z X, Lin G, Jiang L Z, Xu Z. Mater Chem Phys, 2008; 111: 238[22] Ren H P, Liu Z C, An Z G, Wang H Y. Trans Mater Heat Treat, 2006; 27(4): 49(任慧平, 刘宗昌, 安治国, 王海燕. 材料热处理学报, 2006; 27(4): 49)[23] Ren H, Mao W. J Univ Sci Technol Beijing, 2002; 9(3): 185 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|