| 铝合金/镀锌钢板脉冲MIG电弧熔-钎焊接头组织与性能 |
| 秦国梁,苏玉虎,王术军 |
| 山东大学材料液固结构演变与加工教育部重点实验室, 济南 250061 |
|
| MICROSTRUCTURES AND PROPERTIES OF PULSED MIG ARC BRAZED–FUSION WELDED JOINT OF Al ALLOY AND GALVANIZED STEEL |
| QIN Guoliang, SU Yuhu, WANG Shujun |
| Key Laboratory for Liquid–Solid Structure Evolution and Processing of Materials, Ministry of Education, Shandong University, Jinan 250061 |
引用本文:
秦国梁 苏玉虎 王术军. 铝合金/镀锌钢板脉冲MIG电弧熔-钎焊接头组织与性能[J]. 金属学报, 2012, 48(8): 1018-1024.
,
,
.
MICROSTRUCTURES AND PROPERTIES OF PULSED MIG ARC BRAZED–FUSION WELDED JOINT OF Al ALLOY AND GALVANIZED STEEL[J]. Acta Metall Sin, 2012, 48(8): 1018-1024.
| [1] Elliott S, Wallach E R. Met Constr, 1981; 13: 221[2] Elrefaey A, Takahashi M, Ikeuchi K. Quart J Jpn Weld Soc, 2005; 23: 186[3] Sedykh V S. Weld Prod, 1985; 32(2): 28[4] Calderon P D, Walmsley D R, Munlr Z A. Weld J, 1985; 64: 404[5] Qiu R F, Iwamoto C, Satonaka S. Mater Charact, 2009; 60(2): 156[6] Tsujino J, Hidai K, Hasegawa A, Kanai R, Matsuura H, Matsushima K, Ueoka T. Ultrasonics, 2002; 40: 371[7] Czechowski M. Mater Corros, 2004; 55: 464[8] Liu S Y, Suzumura A, Ikeshoji T A, Yamazki T. JSME Int J, 2005; 48A: 420[9] Lin S Y, Qin G L, Lei Z, Wang X Y. Chin Pat, 200610007614.8, 2008[10] J´acome L A, Weber S, Leitner A, Arenholz E, Bruckner J, Hackl H, Pyzalla A R. Adv Eng Mater, 2009; 11: 350[11] Vraˇn´akov´a R, F¨ussel U, Zschetzsche J, Juttner S. Weld World, 2005, 49(9): 105[12] Murakami T, Nakata K, Tong H, Ushio M. ISIJ Int, 2003; 43(10): 159[13] Zhang H T, Feng J C, He P. Mater Charact, 2007; 58: 588[14] Dong H G, Yang L Q, Dong C, Kou S D. Mater Sci Eng, 2010; A527: 7151[15] Lin S B, Song J L, Yang C L, Ma G C. Acta Metall Sin, 2009; 45: 1211(林三宝, 宋建岭, 杨春利, 马广超. 金属学报, 2009; 45: 1211)[16] Laukant H, Wallmann E, M¨uller M, Korte W, Stirn B, Haldenwanger H G, Glatzel U. Sci Technol Weld Join, 2005; (2): 219[17] Dharmendra C, Rao K P, Wilden J, Reich S. Mater Sci Eng, 2011; A528: 1497[18] Torkamany M J, Tahamtan S, Sabbaghzadeh J. Mater Des, 2010; 31: 458[19] Mathieu A, Shabadi R, Deschamps A, Suery M, Matte¨? S, Grevey D, Cicala E. Opt Laser Technol, 2007; 39: 652[20] Bach F W, Beniyas A, Lau K, Versemann R. Adv Mater Res, 2005; (6–8): 143[21] Lei Z, Qin G L, Lin S Y, Wang X Y. J Mech Eng, 2009; 45(3): 94(雷振, 秦国梁, 林尚扬, 王旭友. 机械工程学报, 2009; 45(3): 94)[22] Yang X R. Mater Sci Technol, 2006; 14: 236(杨修荣. 材料科学与工艺, 2006; 14: 236)[23] Shi C X, Li H D, Zhou L. The Handbook of Materials Science and Engineering, Vol.1. Bejing: Chemical Industry Press, 2004: 233(师昌绪, 李恒德, 周廉. 材料科学与工程手册(上卷). 北京: 化学工业出版社. 2004: 233)[24] Maitra T, Gupta S P. Mater Charact, 2003; 49: 293[25] Gupta S P. Mater Charact, 2003; 49: 269[26] Heumann T, Dittrich N A. Z Metallk, 1959; 50: 617[27] Tomiad S, Nataka K. Surf Coat Technol, 2003; 174: 559 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|