镍基高温合金γ'相析出的经典动态模型及应用 |
石宇野1,焦少阳1,2,董建新1,张麦仓1 |
1. 北京科技大学材料科学与工程学院, 北京 100083
2. 中国核电工程有限公司, 北京 100840 |
|
CLASSICAL PRECIPITATION DYNAMIC MODEL OF γ' PHASE OF NICKEL--BASED SUPER ALLOYS AND APPLICATIONS |
SHI Yuye1, JIAO Shaoyang1,2, DONG Jianxin1, ZHANG Maicang1 |
1. School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083
2. China Nuclear Power Engineering Co. Ltd., Beijing 100840 |
引用本文:
石宇野,焦少阳,董建新,张麦仓. 镍基高温合金γ'相析出的经典动态模型及应用[J]. 金属学报, 2012, 48(6): 661-670.
,
,
,
.
CLASSICAL PRECIPITATION DYNAMIC MODEL OF γ' PHASE OF NICKEL--BASED SUPER ALLOYS AND APPLICATIONS[J]. Acta Metall Sin, 2012, 48(6): 661-670.
[1] Wang Y, Banerjee D, Su C C. Acta Mater, 1998; 46: 2983
[2] Wang G, Du D S, Ma N. Acta Mater, 2009; 57: 316
[3] Gale W F, Nemani R V, Horton J A. J Mater Sci, 1996; 31: 1681
[4] Mao J. PhD Thesis, West Virginia University, Morgantown, 2002
[5] Booth-Morrison C, Weninger J, Sudbrack C K, Mao Z, Noebe R D,Seidman D N. Acta Mater, 2008; 56: 3422
[6] Kelekanjeri S K, Gerhardt R A. Electrochim Acta, 2006; 51: 1873
[7] Yao Z H, Dong J X, Zhang M C, Yu Q Y. Trans Mater Heat Treat,2011; 32(10): 43
(姚志浩, 董建新, 张麦仓, 于秋颖. 材料热处理学报, 2011; 32(10): 43)
[8] Oja M, Chandran K S, Tryon R G. Int J Fatigue, 2010; 32: 551
[9] Moat R J, Pinkerton A J, Li L, Withers P J, Preuss M. Acta Mater,2009; 57: 1220
[10] Wisniewski A, Beddoes J. Mater Sci Eng, 2009; A510: 266
[11] Wang Y, Sun F, Dong X P, Zhang L T, Shan A D. Acta Metall Sin,2010; 46: 334
(王衣, 孙峰, 董显平, 张澜庭, 单爱党. 金属学报, 2010; 46: 334)
[12] Wang M G, Tian S G, Yu X F, Qian B J. Rare Met Mater Eng,2010; 39: 268
(王明罡, 田素贵, 于兴福, 钱本江. 稀有金属材料与工程, 2010; 39: 268)
[13] Zhu T, Wang C Y, Gan Y. Acta Phys Sin, 2009; 58: 156
(朱弢,王崇愚, 干勇. 物理学报, 2009; 58: 156)
[14] Wen Y H, Zhu T, Cao L X, Wang C Y. Acta Phys Sin, 2003; 52: 2520
(文玉华, 朱弢,曹立霞, 王崇愚. 物理学报, 2003; 52: 2520)
[15] Lifshitz I M, Slyozov V V. J Phys Chem Sol, 1961; 19: 35
[16] Wagner C. Z Elektrochem, 1961; 65: 581
[17] Wang X D, Wang Q, Jiang J Z. J Alloys Compd, 2007; 440: 189
[18] Hong C M, Dong J X, Zhang Y F, Zhang M C, Zheng L. Rare Met Mater Eng, 2009; 38: 510
(洪成淼, 董建新, 张玉峰, 张麦仓, 郑磊. 稀有金属材料与工程, 2009; 38: 510)
[19] Song X P, Li H Y, Gai J F, Chen G L. Acta Metall Sin,2005; 41: 1233
(宋西平, 李红宇, 盖靖峰, 陈国良. 金属学报, 2005; 41: 1233) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|