(Y, Gd)2O3∶Eu3+纳米粒子制备过程中的合成动力学 |
朱红艳1,马伟民1,闻雷2,管仁国3,马雷1,3,吴南1 |
1. 沈阳化工大学材料科学与工程学院~辽宁省稀土化学及应用重点实验室, 沈阳 110142
2. 中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳 110016
3. 东北大学材料与冶金学院, 沈阳 110819 |
|
SYNTHESIS KINETICS OF (Y, Gd)2O3∶Eu3+ NANO-POWDERS DURING PROCESS OF PREPARATION |
ZHU Hongyan1, MA Weimin1, WEN Lei2, GUAN Renguo3,MA Lei1,3, WU Nan1 |
1. Key Laboratory for Rare-earth Chemical and Applying of Liaoning Province, School of Material Science and Engineering, Shenyang University of Chemical Technology, Shenyang 110142
2. Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences,Shenyang 110016
3. Institute of Metallurgy and Materials, Northeastern University, Shenyang 110819 |
引用本文:
朱红艳,马伟民,闻雷,管仁国,马雷,吴南. (Y, Gd)2O3∶Eu3+纳米粒子制备过程中的合成动力学[J]. 金属学报, 2012, 48(6): 671-677.
,
.
SYNTHESIS KINETICS OF (Y, Gd)2O3∶Eu3+ NANO-POWDERS DURING PROCESS OF PREPARATION[J]. Acta Metall Sin, 2012, 48(6): 671-677.
[1] van Eijk C W E. Phys Med Biol, 2002; 47: 85
[2] Hell E, Knuepfer W, Mattern D. Nucl Instrum Methods Phys Res, 2000; 454A: 40
[3] Jung Y S, Kim K H, Jang T Y, Tak Y, Baeck S H. Curr Appl Phys, 2011; 11: 358·
[4] Louardi A, Rmili A, Ouachtari F, Bouaoud A, Elidrissi B, Erguig H. J Alloys Compd, 2011; 509: 9183
[5] Selvam N C S, Kumar R T, Yogeenth K, Kennedy L J, Sekaran G,Vijaga J J. Powder Technol, 2011; 211: 250
[6] Gunawidjaja R, Myint T, Eilers H. Ceram Int, 2012; 38: 775
[7] Taniguchi T, Watanabe T, Katsumata K, Okada K, Matsushita N. J Phys Chem, 2010; 114C: 3763
[8] Chien J T, Hsu D J, Inbaraj B S, Chen B H. Int J Mol Sci, 2010; 11: 2805
[9] Matiadis D, prousis K C, Markopoulou O I. Molecules, 2009; 14: 3914
[10] Si W, Wang J, Wang X H, Gao H, Zhai Y C. J Inorg Mater,2011; 26: 726
(司伟, 王晶, 王修慧, 高宏, 翟玉春. 无机材料学报, 2011; 26: 726)
[11] Si W, Gao H, Wang J, Jiang D, Zhai Y C. Chin J Inorg Chem,2010; 26: 1443
(司伟, 高宏, 王晶, 姜妲, 翟玉春. 无机化学学报,2010; 26: 1443)
[12] Jie X F, Liang G C, Wang L, Zhi X K, Gao L M. Adv Mater Res,2010; 178: 172
[13] Yu H Y, Ren W T, Zhang Y. J Appl Polym Sci, 2009; 113: 17
[14] Zhuang Y X, Xing P F, Duan T F, Shi H Y, He J C. J Rare Earths,2011; 29: 793
[15] Wang C S, Wang R Q, Wang Y, Fu Y X. Key Eng Mater, 2012; 501: 349
[16] Dai J F, Ling R Q, Wang K Z. Adv Mater Res, 2012; 418: 282
[17] Kok M V. Fuel Process Technol, 2012; 96: 134
[18] Ma W M, Wen L, Shen S F, Liu J, Wang H D. Acta Metall Sin,2009; 45: 759
(马伟民, 闻雷, 沈世妃, 刘晶, 王华栋. 金属学报, 2009; 45: 759)
[19] Ozawa T. Bull Chem Soc Jpn, 1965; 38: 1881
[20] Doyle C D. J Appl Polym Sci, 1961; 5: 285
[21] Kisssinger H E. J Res Nat Bue Stand, 1965; 57: 217
[22] Kissingger H E. Anal Chem, 1957; 29: 1702
[23] Zhao Y N, Zhang W L. Adv Mater Res, 2011; 194: 558
[24] Mullaugh K M, Luther G W. J Nanopart Res,2011; 13: 393 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|