激光悬浮区熔定向凝固Al2O3/YAG/ZrO2 三元过共晶合金的微观组织 |
宋衎,张军,贾晓娇,苏海军,刘林,傅恒志 |
西北工业大学凝固技术国家重点实验室, 西安 710072 |
|
MICROSTRUCTURE OF Al2O3/YAG/ZrO2 HYPEREUTECTIC ALLOY DIRECTIONALLY SOLIDIFIED BY LASER FLOATING ZONE METHOD |
SONG Kan, ZHANG Jun, JIA Xiaojiao, SU Haijun, LIU Lin, FU Hengzhi |
State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi’an 710072 |
引用本文:
宋衎 张军 贾晓娇 苏海军 刘林 傅恒志. 激光悬浮区熔定向凝固Al2O3/YAG/ZrO2 三元过共晶合金的微观组织[J]. 金属学报, 2012, 48(2): 220-226.
,
,
,
,
,
.
MICROSTRUCTURE OF Al2O3/YAG/ZrO2 HYPEREUTECTIC ALLOY DIRECTIONALLY SOLIDIFIED BY LASER FLOATING ZONE METHOD[J]. Acta Metall Sin, 2012, 48(2): 220-226.
[1] Waku Y, Nakagawa N, Wakamoto T, Ohtsubo H, Shimizu K, Kohtoku Y. Nature, 1997; 389: 49
[2] Waku Y, Nakagawa N, Wakamoto T, Ohtsubo H, Shimizu K, Kohtoku Y. J Mater Sci, 1998: 1217
[3] Su H J, Zhang J, Liu L, Fu H Z. Acta Metall Sin, 2008; 44: 457
(苏海军, 张军, 刘林, 傅恒志. 金属学报, 2008; 44: 457)
[4] Su H J, Zhang J, Cui C J, Liu L, Fu H Z. Mater Sci Eng, 2008; A479: 380
[5] Fritsch M, Klemm H. J Eur Ceram Soc, 2008; 28: 2353
[6] Fritsch M, Klemm H, Herrmann M, Schenk B. J Eur Ceram Soc, 2006; 26: 3557
[7] Ochiai S, Ueda T, Sato K, Hojo M, Waku Y, Nakagawa N, Sakata S, Mitani A, Takahashi T. Compos Sci Technol, 2001; 61: 2117
[8] Lee J H, Yoshikawa A, Kaiden H, Lebbou K, Fukuda T, Yoon D H, Waku Y. J Cryst Growth, 2001; 231: 179
[9] Larrea A, Orera V M, Merino R I, Pe˜na J I. J Eur Ceram Soc, 2005; 25: 1419
[10] Oliete P B, Pe˜na J I, Larrea A, Orera V M, Llorca J, Pastor J Y, Mart´?n A, Segurado J. Adv Mater, 2007; 19: 2313
[11] Calderon–Moreno J M, Yoshimura M. J Eur Ceram Soc, 2005; 25: 1365
[12] Pe˜na J I, Larsson M, Merino R I, Francisco I D, Orera V M, Llorca J, Pastor J Y, Mart´?n A, Segurado J. J Eur Ceram Soc, 2006; 26: 3113
[13] Su H J, Zhang J, Cui C J, Liu L, Fu H Z. J Cryst Growth, 2007; 307: 448
[14] Ester F J, Larrea A, Merino R I. J Eur Ceram Soc, 2011; 31: 1257
[15] Kurz W, Fisher D J. Int Met Rev, 1979; (5–6): 177
[16] Lakiza S M, Lopato L M. J Am Ceram Soc, 1997; 80: 893
[17] Echigoya J, Takabayashi Y, Sasaki K. Trans Jpn Inst Met, 1986; 27: 102
[18] Jackson K A, Hunt J D. Aime Met Soc Trans, 1966; 236: 1129
[19] Llorca J, Orera V M. Prog Mater Sci, 2006; 51: 711
[20] Flood S C, Hunt J D. J Mater Sci, 1981; 15: 287
[21] Merino R I, Pe N A J I, Larrea A, de la Fuente G F, Orera V M. Recent Res Devel Mater Sci, 2003; 4: 1
[22] Golubovi´c A, Nikoli´c S, Gaji´c R, Duri´c S, Valˇci´c A. J Serb Chem Soc, 2005; 70: 87
[23] Calderon–Moreno J M, Yoshimura M. Mater Sci Eng, 2004; A375–377: 1250
[24] Magnin P, Kurz W. Acta Metall, 1987; 35: 1119
[25] Liu L, Huang T, Qu M, Liu G, Zhang J, Fu H. J Mater Process Technol, 2010; 210: 159
[26] Oliete P B, Pe˜na J I. J Cryst Growth, 2007; 304: 514
[27] Sola D, Ester F J, Oliete P B, Pe˜na J I. J Eur Ceram Soc, 2011; 31: 1211
[28] Saitou M. J Appl Phys, 1997; 12: 6343
[29] Uhlmann D R, Chalmers B, Jackson K A. J Appl Phys, 1964; 10: 2986
[30] Winegard W C, Majka S, Thall B M, Chalmers B. Can J Chem, 1951; 29: 320 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|