| FeCo基薄带气流中应力退火感生的磁结构 |
| 方允樟1, 2), 许启明1), 叶慧群2), 范晓珍2), 裘剑锋2) |
1) 西安建筑科技大学材料科学与工程学院, 西安 710055
2) 浙江师范大学数理与信息工程学院, 金华 321004 |
|
| MAGNETIC STRUCTURE OF RAPIDLY QUENCHED FeCo-BASED RIBBON ANNEALED UNDER TENSILE STRESS IN FLOWING ATMOSPHERE |
| FANG Yunzhang1, 2), XU Qiming1), YE Huiqun2), FAN Xiaozhen2), QIU Jianfeng2) |
1) School of Materials Science and Engineering, Xi'an University of Architecture and Technology, Xi'an 710055
2) College of Mathematics, Physics and Information Engineering, Zhejiang Normal University, Jinhua 321004 |
引用本文:
方允樟 许启明 叶慧群 范晓珍 裘剑锋. FeCo基薄带气流中应力退火感生的磁结构[J]. 金属学报, 2011, 47(4): 475-481.
,
,
,
,
.
MAGNETIC STRUCTURE OF RAPIDLY QUENCHED FeCo-BASED RIBBON ANNEALED UNDER TENSILE STRESS IN FLOWING ATMOSPHERE[J]. Acta Metall Sin, 2011, 47(4): 475-481.
| [1] Duwez P, Lin S C H. J Appl Phys, 1967; 38: 4096[2] Masumoto T, Kimura H M, Inoue A, Waseda Y. Mater Sci Eng, 1976; 24: 141[3] Kikuchi M, Fujimori H, Obi T, Masumoto T. Jpn J Appl Phys, 1975; 14: 1077[4] Yoshizawa Y, Oguma S, Yamauchi K. J Appl Phys, 1988; 64: 6044[5] Wu H Z, Liu Y H, Zhang L, Xiao S Q, Dai Y Y. Acta Metall Sin, 2000; 36: 997(吴厚政, 刘宜华, 张 林, 萧淑琴, 代由勇. 金属学报, 2000; 36: 997)[6] Jiang H G, Tong H Y, Ding B Z, Hu Z Q, Song Q H, Dong L, Zhou Q. Acta Metall Sin, 1993; 29: B515(姜洪刚, 佟华宇, 丁炳哲, 胡壮麒, 宋启洪, 董林, 周强. 金属学报, 1993; 29: B515)[7] Chen W P, Xiao S Q, Wang W J, Liu Y H. Acta Metall Sin, 2004; 40: 1295(陈卫平, 萧淑琴, 王文静, 刘宜华. 金属学报, 2004; 40: 1295)[8] Inoue A. Acta Mater, 2000; 48: 279[9] Xu M, Sun Y, Quan M X, Wang Y D, Zuo L. Acta Metall Sin, 2007; 43: 699(徐民, 孙 羽, 全明秀, 王沿东, 左良. 金属学报, 2007; 43: 699)[10] Shen B L, Inoue A, Chang C T. Appl Phys Lett, 2004; 85: 4911[11] Wang Z C, Gong F F, Yang X L, Zeng L, Chen G, Yang J X, Qian S M, Yang D P. J Appl Phys, 2000; 87: 4819[12] Herzer G. J Magn Magn Mater, 1992; 112: 258[13] Yoshizawa Y, Oguma S, Yamauchi K. J Appl Phys, 1988; 64: 6044[14] Yoshizawa Y, Yamauchi K. IEEE Trans Magn, 1989; 25: 3324[15] Kraus L, Zaveta K, Heczko O, Duhaj P, Vlasak G, Schnaider T. J Magn Magn Mater, 1992; 112: 275[16] Herzer G. IEEE Trans Magn, 1994; 30: 4800[17] Fang Y Z, Zheng J J, Wu F M, Xu Q M, Ye H Q, Zhang J Q, Zheng J L, Li T Y. Appl Phys Lett, 2010; 96: 092508–1 [18] Yang J X, Yang X L, Chen G. Chin Sci Bull, 1998; 43: 1051(杨介信, 杨燮龙, 陈国. 科学通报, 1998; 43: 1051)[19] Phan M H, Peng H X. Prog Mater Sci, 2008; 53: 323 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|