| 连续柱状晶铜基合金BFe10-1-1的动态再结晶研究 |
| 余均武, 刘雪峰, 谢建新 |
| 北京科技大学材料先进制备技术教育部重点实验室, 北京 100083 |
|
| STUDY OF DYNAMIC RECRYSTALLIZATION OF A Cu-BASED ALLOY BFe10-1-1 WITH CONTINUOUS COLUMNAR GRAINS |
| YU Junwu, LIU Xuefeng, XIE Jianxin |
| Key Laboratory for Advanced Material Processing (Ministry of Education), University of Science and Technology Beijing, Beijing 100083 |
引用本文:
余均武 刘雪峰 谢建新. 连续柱状晶铜基合金BFe10-1-1的动态再结晶研究[J]. 金属学报, 2011, 47(4): 482-488.
,
,
.
STUDY OF DYNAMIC RECRYSTALLIZATION OF A Cu-BASED ALLOY BFe10-1-1 WITH CONTINUOUS COLUMNAR GRAINS[J]. Acta Metall Sin, 2011, 47(4): 482-488.
| [1] Xie J X, Huang J H, Kang Y L, Mao W M, Qu X H, Ren X P, Wang Z D, Wu C J, Zhou C. Advanced Processing Technologies of Materials. Beijing: Metallurgical Industry Press, 2004: 85(谢建新, 黄继华, 康永林, 毛卫民, 曲选辉, 任学平, 王自东, 吴春京, 周成. 材料加工新技术与新工艺. 北京: 冶金工业出版社, 2004: 85)[2] Liu X F, Wu Y H, Xie J X. Sci China, 2009; 52E: 2232[3] Zhang H, Xie J X, Wang Z D. J Univ Sci Technol Beijing (Engl Ed), 2004; 11: 240[4] Efird K D. Corrosion, 1975; 31: 77[5] Yan Z M, Li X T, Qi K, Cao Z Q, Zhang X L, Li T J. Mater Des, 2009; 30: 2072[6] Gan C L, Liu X F, Huang H Y, Xie J X. Acta Metall Sin, 2010; 46: 1549(甘春雷, 刘雪峰, 黄海友, 谢建新. 金属学报, 2010; 46: 1549)[7] Cui W F, Hong Q, Liu C M, Zhou L. J Northeast Univ (Nat Sci), 2003; 24: 572(崔文芳, 洪权, 刘春明, 周 廉. 东北大学学报(自然科学版), 2003; 24: 572)[8] Tang R Z. Physicometallurgical Foundation. Beijing: Metallurgical Industry Press, 1997: 283(唐仁政. 物理冶金基础. 北京: 冶金工业出版社, 1997: 283)[9] Zhang H, Xie J X, Wang Z D, Wang H. Mater Mech Eng, 2004; 28(2): 31(张鸿, 谢建新, 王自东, 王浩. 机械工程材料, 2004; 28(2): 31)[10] Shen G, Semiatantin S L, Altan T. J Mater Process Technol, 1993; 36: 303[11] Poliak E I, Jonas J J. ISIJ Int, 2003; 43: 684[12] Poliak E I, Jonas J J. Acta Mater, 1996; 44: 127[13] Imbert C, Ryan N D, McQueen H J. Metall Mater Trans, 1984; 15A: 185[14] Yuan H, Liu W C. Mater Sci Eng, 2005; A408: 281[15] Zhou J. Master Dissertation, Center South University, Changsha, 2007(周佳. 中南大学硕士学位论文, 长沙, 2007)[16] Lin G Y, Zhou J, Sun L P, Zhang Z F, Zhang S H. Mater Sci Technol, 2009; 17: 441(林高用, 周佳, 孙利平, 张振峰, 张胜华. 材料科学与工艺, 2009; 17: 441)[17] Liu C M, Liu Z J, Zhu X R, Zhou H T. Chin J Nonferr Met, 2006; 16: 1(刘楚明, 刘子娟, 朱秀荣, 周海涛. 中国有色金属学报, 2006; 16: 1)[18] Gu Y F, Lin D L, Shan A D, Chen J G, Hu F, Cao H Q. Acta Metall Sin, 1998; 34: 351(谷月峰, 林栋梁, 单爱党, 陈家光, 胡凡, 曹涵清. 金属学报, 1998; 34: 351)[19] Hu J, Lin D L. Acta Metall Sin, 2004; 40: 489(胡静, 林栋梁. 金属学报, 2004; 40: 489)[20] Zhang L W, Lu Y, Deng X H, Pei J B, Zhang G L. J Dalian Univ Technol, 2008; 48: 351(张立文, 卢瑜, 邓小虎, 裴继斌, 张国梁. 大连理工大学学报, 2008; 48: 351)[21] Zhang H. PhD Thesis, University of science and Technology Beijing, 2003(张 鸿. 北京科技大学博士学位论文, 2003) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|