ASTM A216 WCA铸钢凝固及冷却过程相变的CA模拟 |
苏斌1), 韩志强1), 赵永让2), 沈丙振2), 张连振2), 柳百成1) |
1) 清华大学机械工程系先进成形制造教育部重点实验室, 北京 100084
2) 中信重工机械股份有限公司, 洛阳 471039 |
|
CA MODELING OF PHASE TRANSFORMATION IN ASTM A216 WCA CAST STEEL DURING SOLIDIFICATION AND COOLING PROCESS |
SU Bin1), HAN Zhiqiang1), ZHAO Yongrang2), SHEN Bingzhen2), ZHANG Lianzhen2), LIU Baicheng1) |
1) Key Laboratory for Advanced Materials Processing Technology, Ministry of Education, Department of Mechanical Engineering, Tsinghua University, Beijing 100084
2) CITIC Heavy Industries Co., Ltd., Luoyang 471039 |
引用本文:
苏斌 韩志强 赵永让 沈丙振 张连振 柳百成. ASTM A216 WCA铸钢凝固及冷却过程相变的CA模拟[J]. 金属学报, 2011, 47(11): 1388-1395.
,
,
,
,
,
.
CA MODELING OF PHASE TRANSFORMATION IN ASTM A216 WCA CAST STEEL DURING SOLIDIFICATION AND COOLING PROCESS[J]. Acta Metall Sin, 2011, 47(11): 1388-1395.
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|