| 外应力对NiTi合金中共格Ni4Ti3沉淀相长大行为影响的相场法模拟 |
| 柯常波,马骁, 张新平 |
| 华南理工大学材料科学与工程学院, 广州 510640 |
|
| PHASE FIELD SIMULATION OF THE EFFECT OF APPLIED EXTERNAL STRESS ON GROWTH KINETICS OF COHERENT Ni4Ti3 PRECIPITATE IN NiTi ALLOY |
| KE Changbo, MA Xiao, ZHANG Xinping |
| School of Materials Science and Engineering, South China University of Technology, Guangzhou 510640 |
引用本文:
柯常波 马骁 张新平. 外应力对NiTi合金中共格Ni4Ti3沉淀相长大行为影响的相场法模拟[J]. 金属学报, 2010, 46(8): 921-929.
,
,
.
PHASE FIELD SIMULATION OF THE EFFECT OF APPLIED EXTERNAL STRESS ON GROWTH KINETICS OF COHERENT Ni4Ti3 PRECIPITATE IN NiTi ALLOY[J]. Acta Metall Sin, 2010, 46(8): 921-929.
| [1] Allafi J K, Dlouhy A, Eggeler G. Acta Mater, 2002; 50: 4255
[2] Michutta J, Somsen C, Yawny A, Dlouhy A, Eggeler G. Acta Mater, 2006; 54: 3525
[3] Moore K T, Howe J M. Acta Mater, 2000; 48: 4083
[4] Bosze W P, Trivedi R. Metall Trans, 1974; 5: 511
[5] Enomoto M, Aaronson H I. Scr Metall, 1989; 23: 55
[6] Enomoto M, Hirth J P. Metall Mater Trans, 1996; 27A: 1491
[7] Ke C B, Ma X, Zhang X P. Acta Metall Sin, 2010; 46:84
(柯常波, 马骁, 张新平. 金属学报. 2010; 46:84)
[8] Dlouhy A, Allafi J K, Eggeler G. Philos Mag, 2003; 83: 339
[9] Michutta J, Carrol M C, Yawny A, Somsen C, Neuking K, Eggeler G. Mater Sci Eng, 2004; A378: 152
[10] Li D Y, Chen L Q. Acta Mater, 1996; 45: 2435
[11] Li D Y, Chen L Q. Acta Mater, 1996; 45: 471
[12] Li D Y, Chen L Q. Acta Mater. 1997; 46: 639
[13] Khachaturyan A G. Theory of structural transformation in solid. New York: Wiley-Interscience, 1983: 213
[14] Wagner M F, Windl W. Acta Mater, 2008; 56: 6232
[15] Wagner M F, Windl W. Acta Mater, 2009; 60: 207
[16] Sharma S K, Macht M P, Naundorf V. Phys Rev, 1994; 49B: 6655
[17] Wang G, Xu D S, Ma N, Zhou N, Payton E J, Yang R, Mills M J, Wang Y. Acta Mater, 2009;57: 316
[18] Shen C, Chen Q, Wen Y H, Simmons J P, Wang Y. Scr Mater, 2004; 50: 1023
[19] Shen C, Chen Q, Wen Y H, Simmons J P, Wang Y. Scr Mater, 2004; 50: 1029
[20] Wang Y, Banerjee D, Su C C, Khachaturyan A G.. Acta Mater, 1998; 46: 2983
[21] Zhou N. PhD Thesis, The Ohio State University, 2008
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|