| 热处理温度对电刷镀Ni-P镀层组织的影响 |
| 李志明, 钱士强, 王伟, 刘继华 |
| 上海工程技术大学材料工程学院, 上海 201620 |
|
| EFFECTS OF HEAT-TREAT TEMPERATURE ON MICROSTRUCTURE OF ELECTRO-BRUSH PLATING Ni-P COATINGS |
| LI Zhiming, QIAN Shiqiang, WANG Wei, LIU Jihua |
| College of Material Engineering, Shanghai University of Engineering Science, Shanghai 201620 |
引用本文:
李志明 钱士强 王伟 刘继华. 热处理温度对电刷镀Ni-P镀层组织的影响[J]. 金属学报, 2010, 46(7): 867-872.
,
,
,
.
EFFECTS OF HEAT-TREAT TEMPERATURE ON MICROSTRUCTURE OF ELECTRO-BRUSH PLATING Ni-P COATINGS[J]. Acta Metall Sin, 2010, 46(7): 867-872.
| [1] Lee H B, Wuu D S, Lee C Y, Lin C S. Tribol Int, 2010; 43: 235
[2] Raju M, Ananth M V, Vijayaraghavan L. J Alloys Compd, 2009; 475: 664
[3] Sharma R, Agarwala R C, Agarwala V. J Alloys Compd,2009; 467: 357
[4] Elansezhian R, Ramamoorthy B, Kesavan Nair P. Surf Coat Technol, 2008; 203: 709
[5] Xu J. Surf Coat Technol, 2003; 168: 156
[6] Wu B, Xu B, Zhang B, Lv Y. Surf Coat Technol, 2007; 201: 6933
[7] Kornosky R, Lindsay J H. Plat Surf Finish, 2006; 93: 24
[8] Hou K H, Jeng M C, Ger M D. J Alloys Compd, 2007; 437: 289
[9] Liu H Z, Hu W B, Gu M Y, Wu R J. J Inorg Mater, 2002; 17: 429
(刘河洲, 胡文彬, 顾明元, 吴人洁. 无机材料学报, 2002; 17: 429)
[10] Tan G T, Chen Z H. Acta Phys Sin, 2007; 56: 1702
(谈国太, 陈正豪. 物理学报, 2007; 56: 1702)
[11] Jiang C H, Cheng F X, Wu J S. Acta Metall Sin, 2005; 41: 487
(姜传海, 程凡雄, 吴建生. 金属学报, 2005; 41: 487)
[12] Hong B, Jiang C H, Wang X J, Wu J S. Acta Metall Sin, 2006; 42: 699
(洪 波, 姜传海, 王新建, 吴建生. 金属学报, 2006; 42: 699)
[13] Keong K G, Sha W, Malinov S. J Alloys Compd, 2002; 334: 192
[14] Lu K, Wang J T, Dong L. Acta Metall Sin, 1991; 27: B31
(卢 柯, 王景唐, 董 林. 金属学报, 1991; 27: B31)
[15] Liu Y H, Liu P A. X–ray diffraction analysis Principles and Applications. Beijing: Chemical Industry Press, 2003: 138
(刘粤惠, 刘平安. XRD分析原理与应用. 北京: 化学工业出版社, 2003: 138)
[16] Malek J. Thermochim Acta, 1995; 267: 61
[17] Henderson D W. J Non–Cryst Solids, 1979; 30: 301
[18] Sui M L. Acta Metall Sin, 1998; 34: 650
(隋曼龄. 金属学报, 1998; 34: 650)
[19] Feng D, Qiu D R. Metal Physics (Vol.1): Structure and Defect. Beijing: Science press, 1987: 221
(冯端, 邱第荣. 金属物理学(第一卷)--结构与缺陷. 北京: 科学出版社, 1987: 221)
[20] Jin Y, Sun X S, Xue Q. X–ray Diffraction Analysis. Beijing: National Defense Industry Press, 2008: 251
(晋 勇, 孙小松, 薛屺. XRD分析技术. 北京: 国防工业出版社, 2008: 251)
[21] Hu L H, Dai J, Liu W Q, Wang K J, Dai S Y. Acta Phys Sin, 2009; 58: 1115
(胡林华, 戴 俊, 刘伟庆, 王孔嘉, 戴松元. 物理学报, 2009; 58: 1115) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|