| 湿H2S环境中L360MCS钢焊接热影响区的应力导向氢致开裂行为 |
| 周成双; 郑树启; 陈长风 |
| 中国石油大学(北京) 机电工程学院; 北京 102249 |
|
| STRESS ORIENTED HYDROGEN INDUCED CRACKING BEHAVIOR OF HEAT AFFECTED ZONE OF L360MCS STEEL IN WET H2S ENVIRONMENT |
| ZHOU Chengshuang; ZHENG Shuqi; CHEN Changfeng |
| Mechanical and Electrical Engineering Faculty; China University of Petroleum; Beijing 102249 |
引用本文:
周成双 郑树启 陈长风. 湿H2S环境中L360MCS钢焊接热影响区的应力导向氢致开裂行为[J]. 金属学报, 2010, 46(5): 547-553.
.
STRESS ORIENTED HYDROGEN INDUCED CRACKING BEHAVIOR OF HEAT AFFECTED ZONE OF L360MCS STEEL IN WET H2S ENVIRONMENT[J]. Acta Metall Sin, 2010, 46(5): 547-553.
| [1] Pargeter R J. In: NACE, ed., Corrosion 2007, Houston, TX: NACE, 2007: 115
[2] Guo H, Li G F, Cai X, Yang W. Acta Metall Sin, 2004; 40: 967
(郭浩, 李光福, 蔡珣 , 杨武. 金属学报, 2004; 40: 967)
[3] Ren X C, Wu M, Chu W Y, Li J X, Jiao L J, Jiang B, Chen G, Cui Y H. Acta Metall Sin, 2007; 43: 149
(任学冲, 武明, 褚武扬, 李金许, 乔利杰, 江波, 陈 刚, 崔银会. 金属学报, 2007; 43: 149)
[4] Liu Z Y, Zhai G L, Dui C W, Li X G. Acta Metall Sin, 2008; 44: 209
(刘智勇, 翟国丽, 杜翠薇, 李晓刚. 金属学报, 2008; 44: 209)
[5] Guo J, Yang S W, Shang C J, Wang Y, He X L. Corros Sci, 2008; 51: 242
[6] Ernesto V, Andrej A. Eng Fail Anal, 2009; 16: 164
[7] Cayard M S, Kane R D, Cooke D L. In: NACE, ed., Corrosion 97, Houston, TX: NACE, 1997: 525
[8] Cayard M S, Kane R D, Horvath R J. In: NACE ed., Corrosion 2002, Houston, TX: NACE, 2002: 554
[9] Orie K E, Fletcher F B. In: NACE, ed., Corrosion 99, Houston, TX: NACE, 1999: 632
[10] NACE International. NACE Standard MR0177–2005, Houston, 2005
[11] ASTM. ASTM Standard G39–99, Philadelphia, 2005
[12] NACE International. NACE Standard MR0284–2003, Houston, 2003
[13] Zhao M C, Shan Y Y, Qu J B, Xiao F R, Zhong Y, Yang K. In: CSM ed., CSM 2001 Annual Meeting Proceedings. Beijing: Metallurgical Industry Press, 2001: 891
(赵明纯, 单以银, 曲锦波, 肖福仁, 仲勇, 杨柯. 见中国金属学会主编, 2001年中国钢铁年会论文集.
北京: 冶金工业出版社, 2001: 891)
[14] Lee H W. Mater Sci Eng, 2007; A445: 328
[15] Sojka J, Jerome M, Sozanska M, Vanova P, Rytirova L, Jonsta P. Mater Sci Eng, 2008; A430: 237
[16] Wan K K, Seong U K, Boo Y Y, Kyoo Y K. Corros Sci, 2008; 50: 3336
[17] Parkins R N. Corrosion, 1987; 43: 130
[18] Chu R, Chen W, Wang S H. Corrosion, 2004; 60: 275
[19] Lynch S P. In: NACE, ed., Corrosion 2007, Houston, TX: NACE, 2007: 493
[20] Maroecic P, Mclellan R B. Acta Metall, 1998; 46: 5593
[21] Zang D, MeLellan R B. Acta Metall, 1999; 47: 1671
[22] Harada S, Ono D, Sugimoto H, Fukai Y. J Alloys Compd, 2007; 446: 474
[23] Rebak R B, Xia Z, Safruddin R, Szklarska S Z. Corrosion, 1996; 52: 396 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|