| 微合金低碳钢高温拉伸实验过程的有限元模拟 |
| 张长利1,Michel Bellet2,Manuel Bobadilla3,沈厚发1,柳百成1 |
1. 清华大学机械工程系先进成形制造教育部重点实验室, 北京 100084
2. Mines-ParisTech, Centre de Mise en Forme des Mat'eriaux (CEMEF), Sophia Antipolis, France 06904
3. ArcelorMittal, Research and Development, Maizi`eres-l`es-Metz, France 57283 |
|
| FINITE ELEMENT MODELLING OF TENSILE TEST FOR MICRO–ALLOYED LOW CARBON STEEL AT HIGH TEMPERATURE |
| ZHANG Changli 1, Michel Bellet 2, Manuel Bobadilla 3, SHEN Houfa 1, LIU Baicheng 1 |
1. Key Laboratory for Advanced Materials Processing Technology, Department of Mechanical Engineering, Tsinghua
University, Beijing 100084
2. Mines–ParisTech, Centre de Mise en Forme des Mat´eriaux (CEMEF), Sophia Antipolis, France 06904
3. ArcelorMittal, Research and Development, Maizi`eres–l`es–Metz, France 57823 |
引用本文:
张长利 Michel Bellet Manuel Bobadilla 沈厚发 柳百成. 微合金低碳钢高温拉伸实验过程的有限元模拟[J]. 金属学报, 2010, 46(10): 1206-1214.
,
,
,
,
.
FINITE ELEMENT MODELLING OF TENSILE TEST FOR MICRO–ALLOYED LOW CARBON STEEL AT HIGH TEMPERATURE[J]. Acta Metall Sin, 2010, 46(10): 1206-1214.
| [1]Eskin D G, Katgerman L.A quest for a new hot tearing criterion[J].Metallurgical and Materials Transactions A,2007,38(7):1511-1519
[2]Won Y M, Yeo T J, Seol D J, Oh K H.A new criterion for internal crack formation in continuously cast steels[J].Metallurgical and Materials Transactions B,2000,31(4):779-794
[3]Bellet M, Cerri O, Bobadilla M, Chastel Y.Modeling Hot Tearing during Solidification of Steels: Assessment and Improvement of Macroscopic Criteria through the Analysis of Two Experimental Tests[J].Metallurgical and Materials Transactions A,2009,40(11):2705-2717
[4]Rappaz M, Drezet J M, Gremaud M.A new hot-tearing criterion[J].Metallurgical and Materials Transactions A,1999,30(2):449-455
[5]Suzuki M, Yu C H, Emi T.In-situ measurement of fracture strength of solidifying steel shells to predict upper limit of casting speed in continuous caster with oscillating mold[J].ISIJ International,1997,37(4):375-382
[6]Bernhard C, Xia G.Influence of alloying elements on the thermal contraction of peritectic steels during initial solidification[J].,2006,33(1):52-56
[7]Kim K, Oh K H, Lee D N.Mechanical behavior of carbon steels during continuous casting[J].Scripta Materialia,1996,34(2):301-307
[8]Seol D J, Won Y M, Yeo T J, Oh K H, Park J K.High temperature deformation behavior of carbon steel in the austenite and delta-ferrite regions[J].ISIJ International,1999,39(1):91-98
[9]Seol D J, Won Y M, Oh K H, Shin Y C, Yim C H.Mechanical behavior of carbon steels in the temperature range of mushy zone[J].ISIJ International,2000,40(4):356-363
[10]Brown S G R, James J D, Spittle J A.A 3D numerical model of the temperature-time characteristics of specimens tested on a Gleeble thermomechanical simulator[J].Modelling and Simulation in Materials Science and Engineering,1997,5(6):539-548
[11]Norris S D, Wilson I.Application of 3D numerical modelling for thermal profile optimization on the Gleeble thermomechanical simulator[J].Modelling and Simulation in Materials Science and Engineering,1999,7(3):297-309
[12]Solek K, Mitura Z, Kuziak R.A numerical model of the resistance heating system for material tests on a Gleeble simulator[J].Proc. 3rd MIT Conference on Computational Fluid and Solid Mechanics, June 14-17,2005, K.J. Bathe (ed.),2005,:1001-1003
[13]Bellet M, Fachinotti V D.ALE method for solidification modelling[J].,2004,193:4355-4381
[14]Thomas B G, Bellet M.Modeling of stress, distrotion and hot tearing[J].ASM Handbook Volume 15, Casting Division 4: Modeling and Analysis of Casting Processes, American Society of Metals,2008,15:449-461
[15]Bellet M, Heinrich A.A two-dimensional finite element thermomechanical approach to a global stress-strain analysis of steel continuous casting[J].ISIJ International,2004,44(10):1686-1695
[16]Bellet M, Decultieux F, Menai M, Bay F, Levaillant C, Chenot J L, Schmidt P, Svensson I L.Thermomechanics of the cooling stage in casting processes: Three-dimensional finite element analysis and experimental validation[J].Metallurgical and Materials Transactions B,1996,27(1):81-99
[17]Wray P J.Plastic deformation of delta-ferritic iron at intermediate strain rates[J].Metallurgical Transactions A,1976,7(11):1621-1627
[18]Ankem S, Margolin H, Greene C A, Neuberger B W, Oberson P G.Mechanical properties of alloys consisting of two ductile phases[J].Progress in Materials Science,2006,51(5):632-709
[19]Wray P J. PLASTIC-FLOW AND FAILURE OF PLAIN CARBON-STEELS IN FERRITE+AUSTENITE REGION[J].Metals Technology,1981,8(12):466-471
[20]Harste K, Schwerdtfeger K.Thermomechanical properties of iron: Viscoplasticity of ferrite and of austenite-ferrite mixtures[J].,1996,12(5):378-384
[21]Kozlowski P F, Thomas B G, Azzi J A, Hao W.Simple constitutive-equations for steel at high-temperature[J].Metallurgical Transactions A,1992,23(3):903-918
[22]Mizukami H, Shirai Y, Yamanaka A.Prediction of tensile strength and elongation of high alloy steels during solidification[J].ISIJ International,2006,46(7):1040-1046
[23]Koric S, Thomas B G.Thermo-mechanical models of steel solidification based on two elastic visco-plastic constitutive laws[J].,2008,197:408-418
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|