引用本文:
黄姝珂 刘建辉 李昌安 周丹晨 李宁 文玉华. 预变形对Fe-Mn合金层错几率和阻尼性能的影响[J]. 金属学报, 2009, 45(8): 937-942.
,
,
,
,
,
.
EFFECT OF PRE-DEFORMATION ON STACKING FAULT PROBABILITY AND DAMPING CAPACITY OF Fe-Mn ALLOY[J]. Acta Metall Sin, 2009, 45(8): 937-942.
| [1] Pulino–Sagradi D, Sagradi M, Karimi A, Martin J L. Scr Mater, 1998; 39: 131
[2] Wu S K, Lin H C. J Alloys Compd, 2003; 355: 72
[3] Liu Y C, Yang G C, Lu L L, Yang L S. J Mater Process Tecnol, 1999; 87: 53
[4] G¨oken J, Riehemann W. Mater Sci Eng, 2004; A370: 417
[5] Baik S H. Nucl Eng Des, 2000; 198: 241
[6] Jun J H, Choi C S. Mater Sci Eng, 1998; A252: 133
[7] Huang S K, Li N, Wen Y H, Teng J, Ding S. Mater Sci Eng, 2008; A479: 223
[8] Lee Y K, Jun J H, Choi C S. ISIJ Int, 1997; 37: 1023
[9] Huang S K, Li N, Wen Y H, Ding S, Teng J. Acta Metall Sin, 2007; 43: 807
(黄姝珂, 李宁, 文玉华, 丁 胜, 滕 劲. 金属学报, 2007; 43: 807)
[10] Jun J H, Choi C S. Metll Mater rans, 1999, 30A: 667
[11] Seo Y S, Lee Y K, Choi C S. Mater Trans, 2005, 46: 1274
[12] Lee Y K, Baik S H, Kim J C, Choi C S. J Alloys Compd, 2003; 355: 10
[13] Warren B E. X–Ray Diffraction. Massachusett Addison: Wesley, 1969: 275
[14] Ramous E. Z Metallkd, 1974; 65: 515
[15] He G, Zhao H B, Rong Y H, Guo Z H, Chen S P, Hsu T Y. J Shanghai Jiaotong Univ, 1999; 33: 765
(何刚, 赵恒北, 戎咏华, 郭正洪, 陈世朴, 徐祖耀. 上海交通大学学报,1999; 33: 765)
[16] Granato A, L¨ucke K. J Appl Phys, 1956; 27: 583
[17] Teutonico L J, Granato A V, L¨ucke K. J Appl Phys, 1964; 35: 220 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|