金属学报  2009, Vol. 45 Issue (7): 820-825    
  论文 本期目录 | 过刊浏览 |
涂覆Ni--Cr--Al--Y涂层的镍基高温合金热机械疲劳行为
陈竹兵1; 黄志伟1; 王中光1;朱世杰2
1) 中国科学院金属研究所沈阳材料科学国家(联合)实验室; 沈阳 110016 2) Department of Intelligent Mechanical Engineering; Fukuoka Institute of Technology; Fukuoka; Japan
THERMO--MECHANICAL FATIGUE BEHAVIOR OF Ni--BASED SUPERALLOY COATED WITH Ni--Cr--Al--Y
CHEN Zhubing1;  HUANG Zhiwei1;  WANG Zhongguang1; ZHU Shijie2
1) Shenyang National Laboratory for Materials Science; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 2) Department of Intelligent Mechanical Engineering; Fukuoka Institute of Technology; Fukuoka; Japan
引用本文:

陈竹兵 黄志伟 王中光 朱世杰. 涂覆Ni--Cr--Al--Y涂层的镍基高温合金热机械疲劳行为[J]. 金属学报, 2009, 45(7): 820-825.
, , , . THERMO--MECHANICAL FATIGUE BEHAVIOR OF Ni--BASED SUPERALLOY COATED WITH Ni--Cr--Al--Y[J]. Acta Metall Sin, 2009, 45(7): 820-825.

全文: PDF(976 KB)  
摘要: 

分别采取大气等离子 (APS) 和高速火焰 (HVOF)工艺制备Ni--Cr--Al--Y涂层. 对涂覆Ni--Cr--Al--Y涂层的高温合金试样的热机械疲劳 (TMF) 行为进行了研究. 结果表明:在相同应变幅下, 2种涂层试样都是反相位热机械疲劳 (OP TMF) 寿命比同相位热机械疲劳 (IP TMF) 寿命短; 在不同应变幅下, 试样的热机械疲劳寿命与涂层的喷涂工艺相关. 通过断口和纵向剖面图的观察分析表明, 裂纹的萌生对试样的寿命有很大的影响.

关键词 : 镍基高温合金,  Ni--Cr--Al--Y涂层,  热机械疲劳,  裂纹萌生与扩展    
Abstract:

Gas turbine engine is widely used in industry, marine and aerospace. Its efficiency can be enhanced by increasing inlet gas temperature and reducing heat transfer. To achieve this goal it is important to develop materials with higher melting points. Ni--based superalloy is suitable for vane and blade materials. The properties of superalloy have been improved by directionally solidified and single crystal in last 50 years. But it is limited to develop superalloy with much higher temperature, because the operating temperature approaches the melting point of superalloy. In this rigorous environment, high temperature oxidation and hot corrosion impair the alloy property. MCrAlY coating is commonly used as oxidation-- and corrosion--resistant material. Hitherto, it is clearly validated that the oxidation-- and corrosion--resistance of hot parts at high temperature can be greatly improved by MCrAlY coating. The difference of materials properties between MCrAlY coating and superalloy may cause interactions which influence the mechanical properties and life of MCrAlY--coated component. A few of studies have conducted on mechanical properties of $M$CrAlY--coated superalloy. The results revealed that the present of coating affected the performance of superalloy. In service, thermo--mechanical fatigue provides a closer simulation of the actual strain--temperature in an engine environment. Only a few studies were published though their results were not consistency; because the experiment is hard to perform and many factors influence the experiment results such as temperature--strain cycle shape, strain range magnitude, the ductility and the strength of the bond between the coating and the substrate. In this paper, thermo--mechanical fatigue (TMF) behaviors of a Ni--based superalloy M963 coated with Ni--Cr--Al--Y have been investigated at 450---900 ℃ in air under mechanical strain control with a strain ratio of -1 and a period of 200 s. The coating was produced either by air plasma spraying (APS) or by high velocity oxyfuel fuel (HVOF). It was shown that under the same mechanical strain, the out of phase (OP) TMF life is shorter than the in phase (IP) TMF one in both APS and HVOF coated specimens. The TMF life depends on the coating spraying technology under the same testing conditions. Observations of fracture surfaces and longitudinal sections revealed that crack initiation has great impact on the TMF life.

Key words: Ni--based superalloy    Ni--Cr--Al--Y coating    thermo--mechanical fatigue    crack initiation and propagation
收稿日期: 2009-03-11     
ZTFLH: 

TG146.15

 
基金资助:

沈阳界面材料研究中心海外学者计划项目资助CIM09SJZHU

作者简介: 陈竹兵, 男, 1983年生, 博士生

[1] Brindley W J, Miller R A. Adv Mater Process, 1989; 136: 29
[2] Schulz U, Leyens C, Fritscher K, Peters M, Saruhan– Brings B, Lavigne O, Jean–Marc Dorvaux, Poulain M, M´evrel R, Caliez M. Aerosp Sci Technol, 2003; 7: 73
[3] Hu G F. J Mater Prot, 2007; 40(11): 63
(胡国海. 材料保护, 2007; 40(11): 63)

[4] Wu X M, Li W G, Lu F. Equip Environ Eng, 2006; 3: 116
(吴小梅, 李伟光, 陆峰. 装备环境工程, 2006; 3: 116)

[5] Zhang Y J, Sun X F, Jin T, Guan H R, Hu Z Q. Acta Metall Sin, 2003; 39: 189
(张玉娟, 孙晓峰, 金涛, 管恒荣, 胡壮麒. 金属学报, 2003; 39: 189)

[6] Hanshin C, Byounghyun Y, Hyungjun K, Changhee L. Surf Coat Technol, 2002; 150: 297
[7] Ren X, Wang F H. Surf Coat Technol, 2006; 201: 30
[8] Chen Z X. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, 2008
(陈兆祥. 博士学位论文, 中科院金属研究所, 2008)

[9] Kowalewski R, Mughrabi H. Mater Sci Eng, 1998; A247: 295
[10] Gao R F. Thermal Spraying. Beijing: Chemical Industry Press, 1992: 57
(高荣发. 热喷涂. 北京: 化学工业出版社, 1992: 57)

[11] Sidhu T S, Agrawal R D, Prakash S. Surf Coat Technol, 2005; 198: 441
[12] Helali M, Hashmi M S J. J Mater Process Technol, 1996; 56: 431
[13] Tzimas E, M¨ullejans H, Peteves S D, Bressers J, Stamm W. Acta Mater, 2000; 48: 4699

[1] 王磊, 刘梦雅, 刘杨, 宋秀, 孟凡强. 镍基高温合金表面冲击强化机制及应用研究进展[J]. 金属学报, 2023, 59(9): 1173-1189.
[2] 郑亮, 张强, 李周, 张国庆. 增/降氧过程对高温合金粉末表面特性和合金性能的影响:粉末存储到脱气处理[J]. 金属学报, 2023, 59(9): 1265-1278.
[3] 江河, 佴启亮, 徐超, 赵晓, 姚志浩, 董建新. 镍基高温合金疲劳裂纹急速扩展敏感温度及成因[J]. 金属学报, 2023, 59(9): 1190-1200.
[4] 赵鹏, 谢光, 段慧超, 张健, 杜奎. 两种高代次镍基单晶高温合金热机械疲劳中的再结晶行为[J]. 金属学报, 2023, 59(9): 1221-1229.
[5] 穆亚航, 张雪, 陈梓名, 孙晓峰, 梁静静, 李金国, 周亦胄. 基于热力学计算与机器学习的增材制造镍基高温合金裂纹敏感性预测模型[J]. 金属学报, 2023, 59(8): 1075-1086.
[6] 袁江淮, 王振玉, 马冠水, 周广学, 程晓英, 汪爱英. Cr2AlC涂层相结构演变对力学性能的影响[J]. 金属学报, 2023, 59(7): 961-968.
[7] 张禄, 余志伟, 张磊成, 江荣, 宋迎东. GH4169高温合金热机械疲劳循环损伤机理及数值模拟[J]. 金属学报, 2023, 59(7): 871-883.
[8] 刘来娣, 丁彪, 任维丽, 钟云波, 王晖, 王秋良. DZ445镍基高温合金高温长时间氧化形成的多层膜结构[J]. 金属学报, 2023, 59(3): 387-398.
[9] 于少霞, 王麒, 邓想涛, 王昭东. GH3600镍基高温合金极薄带的制备及尺寸效应[J]. 金属学报, 2023, 59(10): 1365-1375.
[10] 祝国梁, 孔德成, 周文哲, 贺戬, 董安平, 疏达, 孙宝德. 选区激光熔化 γ' 相强化镍基高温合金裂纹形成机理与抗裂纹设计研究进展[J]. 金属学报, 2023, 59(1): 16-30.
[11] 朱玉平, 盛乃成, 谢君, 王振江, 荀淑玲, 于金江, 李金国, 杨林, 侯桂臣, 周亦胄, 孙晓峰. 高钨镍基高温合金K416B富W相的析出行为[J]. 金属学报, 2021, 57(2): 215-223.
[12] 刘超, 姚志浩, 江河, 董建新. GH4720Li合金毫米级粗大晶粒热变形获得均匀等轴晶粒的可行性及工艺控制[J]. 金属学报, 2021, 57(10): 1309-1319.
[13] 张小丽, 冯丽, 杨彦红, 周亦胄, 刘贵群. 二次枝晶取向对镍基高温合金晶粒竞争生长行为的影响[J]. 金属学报, 2020, 56(7): 969-978.
[14] 张北江,黄烁,张文云,田强,陈石富. 变形高温合金盘材及其制备技术研究进展[J]. 金属学报, 2019, 55(9): 1095-1114.
[15] 任维鹏, 李青, 黄强, 肖程波, 何利民. 定向凝固镍基高温合金DZ466表面CoAl涂层的氧化及组织演变[J]. 金属学报, 2018, 54(4): 566-574.