| Ni53.2Mn22.6Ga24.2单晶的磁控形状记忆效应和磁控超弹性特性 |
| 游素琴1;崔玉亭1;2;武亮1;孔春阳1;马勇1;杨晓红1;潘复生2 |
1 重庆师范大学物理与信息技术学院; 重庆 400047
2 重庆大学材料科学与工程学院; 重庆 400044 |
|
| MAGNETIC--FIELD--CONTROLLED SHAPE MEMORY EFFECT AND SUPERELASTICITY OF Ni53.2Mn22.6Ga24.2 SINGLE CRYSTAL |
| YOU Suqin1; CUI Yuting1;2; WU Liang1; KONG Chunyang1; MA Yong1; YANG Xiaohong1;PAN Fusheng2 |
1 College of Physics and Information Technology; Chongqing Normal University; Chongqing 400047
2 Department of Materials Science and Engineering; Chongqing University; Chongqing 400044\par |
引用本文:
游素琴 崔玉亭 武亮 孔春阳 马勇 杨晓红 潘复生. Ni53.2Mn22.6Ga24.2单晶的磁控形状记忆效应和磁控超弹性特性[J]. 金属学报, 2009, 45(3): 351-355.
| [1] Murray S J, Marioni M, Allen S M, OHandley R C, Lograsso T A. Appl Phys Lett, 2000; 77: 886
[2] Wang WH,Wu G H, Chen J L, Yu C H, Gao S X, Zhan W S. Appl Phys Lett, 2000; 77: 3245
[3] Jiang C B, Wang J M, Xu H B. Appl Phys Lett, 2005; 86: 252508
[4] Wang W H, Wu G H, Chen J. L, Gao S X, Zhan W S, Wen G H, Zhang X X. Appl Phys Lett, 2001; 79: 1148
[5] Deng L F, Li Y, Jiang C B, Xu H B. Acta Metall Sin, 2004; 40: 1290
(邓丽芬, 李岩, 蒋成保, 徐惠彬. 金属学报, 2004; 40: 1290)
[6] Zayak A T, Entel P, Enkovaara J, Ayuela A, Nieminen R M. J Phys: Condens Matter, 2003; 15: 159
[7] Jiang C B, Liu J H, Zhang T, Xu H B. Acta Metall Sin, 2004; 40: 975
(蒋成保, 刘敬华, 张涛, 徐惠彬. 金属学报, 2004; 40: 975)
[8] Cui Y T, Yang X H, Kong C Y, Ma Y, Pan F S. Solid State Commun, 2006; 138: 234
[9] Chernenko V A, Segui C, Cesari E, Pons J, Kokorin V V. Phys Rev, 1998; 57B: 2659
[10] Wang W H, Chen J L, Liu Z H, Wu G H, Zhan W S. Phys Rev, 2002; 65B: 12416
[11] Martynov V V, Kokorin V V. J Phys III, 1992; 2: 739
[12] Martynov V V. J Phys Colloq, 1995; 8C: 91
[13] Wang W H, Wu G H, Chen J L, Yu C H,Wang Z, Zheng Y F, Zhao C, Zhan W S. J Phys: Condens Matter, 2000; 12: 6287
[14] Ladislav S, Oleg H. IEEE Trans Magn, 2003; 39: 3402
[15] Cui Y T, Hu H N, Liu G D, Dai X F, Liu Z H, Zhang M, Chen J L, Wu G H, Meng F B, Yan L Q, Qu J P, Li Y X. Acta Phys Sin, 2004; 53: 1450
(崔玉亭, 胡海宁, 刘国栋, 代学芳, 柳祝红, 张铭, 陈京兰, 吴光恒, 孟凡斌, 阎丽琴, 曲静萍,
李养贤. 物理学报, 2004; 53: 1450)
[16] Qu J P, Wang W H, Meng F B, Liu B D, Liu Z H, Chen J L, Li Y X,Wu G H. Chin Phys Lett, 2002; 19: 591
[17] Webster P J, Ziebeck K R A, Town S L, Peak M S. Philos Mag, 1984; 49B: 295 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|