| 抽拉速率对定向凝固Al-4%Cu合金枝晶界面特征的影响 |
| 屈敏;刘林;张卫国;张军;傅恒志 |
| 西北工业大学凝固技术国家重点实验室 |
|
| Effect of withdrawal velocity on dendritic interfacial characteristic for Al-Cu alloy during directional solidification |
| Min Qu;Lin LIU;;; |
| 西北工业大学凝固技术国家重点实验室 |
引用本文:
屈敏; 刘林; 张卫国; 张军; 傅恒志 . 抽拉速率对定向凝固Al-4%Cu合金枝晶界面特征的影响[J]. 金属学报, 2008, 44(9): 1051-1056 .
,
,
,
,
.
Effect of withdrawal velocity on dendritic interfacial characteristic for Al-Cu alloy during directional solidification[J]. Acta Metall Sin, 2008, 44(9): 1051-1056 .
[1]Hunt J D.Solidification and Casting of Metals.London: The Metal Society,1979:3 [2]Kurz W,Fisher D J.Acta Metall,1981;29 :11 [3]Trivedi R.Me,all Trans,1984;15A:977 [4]Hunt J D,Lu S Z.Me,all Mater Trans,1996;27A:611 [5]Hunt J D,Lu S Z.Mater Sci Eng,1993;A173:79 [6]Giindiiz M,Cadirh E.Mater Sci Eng,2002;A327:167 [7]Spencer B J,Huppert H E.J Cryst Growth,1999;200: 287 [8](?)stün E,Cadirh E,Kaya H.J Phys:Condens Matter, 2006;18:7825 [9]Kurz W.Adv Eng Mater,2001;3:443 [10]Kurz W,Giovanola B,Trivedi R.Acta Metall,1986;34: 823 [11]Trivrdi R,Kurz W.Acta Metall Mater,1994;42:15 [12]Trivedi R,Kurz W.Int Mater Rev,1994;9(2):49 [13]Bottinger W J,Coriell S R,Trivedi R.In:Mehrabian R, Parrish P A,eds.,Proc 4th Conf on Rapid Solidification Processing:Principles and Technologies,Baton Rouge, LA:Claitor's,Publishing Dir(?)sion,1988:13 [14]Aziz M J.Metall Mater Trans,1996;27A:671 [15]Burden M H,Hunt J D.J Cryst Growth,1974;22:109 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|