|
|
|
| Ti-(Cu, Ni)-Sn合金形成金属玻璃的成分优化及其相关联的共晶反应 |
| 刘元帅;徐坚 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室 |
|
| OPTIMIZED COMPOSITIONS OF Ti-(Cu, Ni)-Sn ALLOY FOR METALLIC GLASS FORMATION AND THEIR CORRELATION WITH EUTECTIC REACTION |
| LIU Yuanshuai; XU Jian |
| Shenyang National Laboratory for Materials Science; Institute of Metal Research; Chinese Academy of Sciences |
引用本文:
刘元帅 徐坚. Ti-(Cu, Ni)-Sn合金形成金属玻璃的成分优化及其相关联的共晶反应[J]. 金属学报, 2008, 44(12): 1424-1430.
,
.
OPTIMIZED COMPOSITIONS OF Ti-(Cu, Ni)-Sn ALLOY FOR METALLIC GLASS FORMATION AND THEIR CORRELATION WITH EUTECTIC REACTION[J]. Acta Metall Sin, 2008, 44(12): 1424-1430.
[1]Johnson W L.MRS Bull,1999;24:42 [2]Inoue A.Acta Mater,2000;28:279 [3]Greet A L,Ma E.MRS Bull,2007;32:611 [4]Li Y,Poon S J,Shiflet G J,Xu J,Kim D H,L(?)ffler J F. MRS Bull,2007;32:624 [5]Kim Y C,Kim W T,Kim D H.Mater Sci Eng,2004; A375-377:127 [6]Men H,Pang S,Inoue A,Zhang T.Mater Trans,2005; 46:2218 [7]Kim K B,Das J,Wang X D,Zhang X,Eckert J,Yi S. Philos Mag Lett,2006;86:479 [8]Ohkubo T,Nagahama D,Mukai T,Hono K.J Mater Res, 2007;22:1406 [9]Qin F X,Wang X M,Kawashima A,Zhu S L,Kimura H, Inoue A.Mater Trans,2006;47:1934 [10]Guo F Q,Wang H J,Poon S J,Shiflet G J.Appl Phys Lett,2005;86:091907 [11]Duan G,Wiest A,Lind M L,Kahl A,Johnson W L.Scr Mater,2008:58:465 [12]Zhang Q S,Zhang W,Inoue A.Mater Trans,2007;48: 3031 [13]Jiang Q K,Wang X D,Nie X P,Zhang G Q,Ma H,Feeht H J,Bendnarcik J,Franz H,Lin Y G,Cao Q P,Jiang J Z.Acta Mater,2008;56:1785 [14]Dai C L,Guo H,Shen Y,Li Y,Ma E,Xu J.Scr Mater, 2006;54:1403 [15]Shen Y,Ma E,Xu J.d Mater Sci Technol,2008;24:149 [16]Ma H,Shi L L,Xu J,Li Y,Ma E.Appl Phys Lett,20051 87:181915 [17]Zheng Q,Xu J,Ma E.J Appl Phys,2007;102:113519 [18]Lu Z P,Liu C T,Thompson J R,Porter W D.Phys Rev Lett,2004;92:245503 [19]Ponnambalam V,Poon S J,Shiflet G J.J Mater Res,2004; 19:1320 [20]Shen J,Chen Q J,Sun F J,Fan H B,Wang G.Appl Phys Lett,2005;86:151907 [21]Zhang T,Inoue A.Mater Trans JIM,1998;39:1001 [22]Zhang T,Inoue A.Mater Sci Eng,2001;A304-306:771 [23]Ma C L,Ishihara S,Soejima H,Nishiyama N,Inoue A. Mater Trans,2004;45:1802 [24]Huang Y J,Shen J,Sun J F,Yu X B.J Alloys Compd, 2007;427:171 [25]Wang Y L,Ma E,Xu J.Philos Mag Lett,2008;88:319 [26]Ma H,Shi L L,Xu J,Li Y,Ma E.J Mater Res,2006;21: 2204 [27]Zheng Q,Ma H,Ma E,Xu J.Scr Mater,2006;55:541 [28]Zhang L,Zhuo M J,Xu J.J Mater Res,2008;23:688 [29]Zhang L,Ma E,Xu J.Intermetallics,2008;16:584 [30]Zhang Z X,Dai C L,Xu J.J Mater Sci Technol,2008;in press [31]Lin X H,Johnson W L.J Appl Phys,1995;78:6514 [32]Massalski T B.Binary Alloy Phase Diagrams.2 Ed.,Met- als Park,OH:ASM International,1996:1495 [33]Louzguine D V,Katao H D,Louzguina L V,Inoue A.J Mater Res,2004;19:3600 [34]Chen H S.Acta Metall,1976;24:153 [35]Miracle D B.Nature Mater,2004;3:697 [36]Guo F Q,Poon S J,Shiflet G J.J Appl Phys,2004;97: 013512 [37]Wang A P,Wang J Q.J Mater Res,2007;22:1 [38]Schuster J C,Naka M,Shibayanagi T.J Alloys Compd, 2000;305:L1 [39]Niessen A K,de Boer F R,Boom R,de Chatel P F,Mat- tens W C M,Miedema A R.Calphad,1983;7:51 [40]Wang D,Tan H,Li Y.Acta Mater,2005;53:2969 [41]Dai C L,Deng J W,Zhang Z X,Xu J.J Mater Res,2008; 23:1249 [42]Dai C L,Guo H,Li Y,Xu J.J Non-Cryst Solids,2008; 354:3659 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|