| SiC颗粒增强体对铝基复合材料微弧氧化膜生长的影响 |
| 薛文斌 |
| 北京师范大学低能核物理研究所射线束材料改性开放实验室 |
|
| EFFECT OF REINFORCEMENT PARTICLE ON GROWTH OF MICROARC OXIDATION FILM ON ALUMINUM MATRIX COMPOSITE |
| WenBin Xue |
| 北京师范大学低能核物理研究所射线束材料改性开放实验室 |
引用本文:
薛文斌 . SiC颗粒增强体对铝基复合材料微弧氧化膜生长的影响[J]. 金属学报, 2006, 42(4): 350-354 .
.
EFFECT OF REINFORCEMENT PARTICLE ON GROWTH OF MICROARC OXIDATION FILM ON ALUMINUM MATRIX COMPOSITE[J]. Acta Metall Sin, 2006, 42(4): 350-354 .
[1] Yue T M, Wu Y X, Man H C. Surf Coat Technol, 1999; 114: 13 [2] Greene H J, Mansfeld F. Corrosion, 1997; 53: 920 [3] Yu X W, Cao C N, Lin H C, Zhou Y H, Zhou D R, Yin Z D. Acta Phys-Chem Sin, 2000; 16: 547 (于兴文,曹楚南,林海潮,周育红,周德瑞,尹钟大.物理化 学学报,2000;16:547) [4] Belevantsev V I, Terleeva O P, Markov G A, Shulepko E K, Slonova A I, Utkin V V. Prot Met, 1998; 34: 416 [5] Xue W B, Deng Z W, Lai Y C, Chen R Y. J Am Ceram Soc, 1998; 81: 1365 [6] Yao Z P, Jiang Z H, Sun X T, Xin S G, Li Y P. Thin Solid Films, 2004; 468: 120 [7] Xue W B, Wang C, Chen R Y, Deng Z W. Mater Lett, 2002; 52: 435 [8] Jiang B L, Zhang X-F, Zhu J. Heat Treat Met, 2004; 29: 23 (蒋百灵,张先锋,朱 静.金属热处理, 2004;29:23) [9] Nie X, Meletis E I, Jiang J C, Leyland A, Yerokhin A L, Matthews A. Surf Coat Technol, 2002; 149: 245 [10] Xue W B, Deng Z W, Chen R Y, Zhang T H. Ada Metall Sin, 1999; 35: 638 (薛文斌,邓志威,陈如意,张通和.金属学报,1999;35:638) [11] Wang Y K, Xiong R Z, Sheng L, Li B S. Ordnance Mater Sci Eng, 1998; 21(4): 25 (王永康,熊仁章,盛磊,李炳生.兵器材料科学与工程,1998; 21(4):25) [12] Jin L, Yang Z, Li G H, Ma Y H, Li J P. Ordnance Mater Sci Eng, 2003; 26(3): 31 (金 玲,扬 忠,李高宏,马玉韩,李建平.兵器材料科学与 工程,2003;26(3):31) [13] Xue W B, Wang C, Li Y, Chen R Y, Zhang T H. ISIJ Int, 2002; 42: 1273 [14] Xue W B, Deng Z W, Chen R Y, Zhang T H. Thin Solid Films, 2000, 372: 114 [15] Shahid M. J Mater Sci, 1997; 32: 3775 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|