| Ti50-0.5xNi50-0.5xCux合金的微观组织 |
| 王 剑 金 伟 曹名洲 杨 锐 |
| 中国科学院金属研究所; 沈阳 110016 |
|
| Microstructures of Ti50-0.5xNi50-0.5xCux Alloys |
| WANG Jian; JIN Wei; CAO Mingzhou; YANG Rui |
| Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
王剑; 金伟; 曹名洲; 杨锐 . Ti50-0.5xNi50-0.5xCux合金的微观组织[J]. 金属学报, 2006, 42(11): 1177-1181 .
,
,
,
.
Microstructures of Ti50-0.5xNi50-0.5xCux Alloys[J]. Acta Metall Sin, 2006, 42(11): 1177-1181 .
[1] Mercier O, Melton K N. Metall Trans, 1979; IDA: 387 [2] Zhu M, Guo J F. Rare Met, 1997; 21: 494 (朱明,郭锦芳.稀有金属, 1997;21:494) [3] Nam T H, Saburi T, Shimizu K. Mater Trans, JIM, 1990; 31: 959 [4] Nam T H, Saburi T, Nakata Y, Shimizu K. Mater Trans, JIM, 1990; 31: 1050 [5] Nakata Y, Tadaki T, Shimizu K. Mater Trans JIM, 1991; 32: 580 [6] Xu D S, Song Y, Li D, Hu Z Q. Rare Met, 1997; 21: 501 (徐东生,宋岩,李东,胡壮麒,稀有金属,1997;21:501) [7] Villars P, Prince A, Okamoto H. Handbook of Ternary Alloy Phase Diagrams. Materials Park, OH: ASM Internatioal, 1997: 9846 [8] Miyazaki S, Wayman C M. Acta Metall, 1988; 36: 181 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|