| Ti-60合金双态组织时效过程中碳化物的溶解行为 |
| 张尚洲 王青江 刘羽寅 杨 锐 |
| 烟台大学环境与材料工程学院; 烟台 264005 |
|
| DISSOLUTION BEHAVIOR OF CARBIDE IN Ti-60 TITANIUM ALLOYS WITH BIMODAL MICROSTRUCTURE DURING AGEING |
| ZHANG Shangzhou; WANG Qingjiang; LIU Yuyin; YANG Rui |
| School of Environment and Materials Engineering; Yantai University; Yantai 264005 |
引用本文:
张尚洲; 王青江; 刘羽寅; 杨锐 . Ti-60合金双态组织时效过程中碳化物的溶解行为[J]. 金属学报, 2005, 41(9): 969-973 .
,
,
,
.
DISSOLUTION BEHAVIOR OF CARBIDE IN Ti-60 TITANIUM ALLOYS WITH BIMODAL MICROSTRUCTURE DURING AGEING[J]. Acta Metall Sin, 2005, 41(9): 969-973 .
[1] Riaz S, Flower H M, West D R F. Mater Sci Technol, 2002; 18: 941 [2] Zhang E L,Jin Y X, Zeng S Y. J Mater Sci Lett, 2001; 20: 1063 [3] Jin Y X, Zeng S Y, Wang H W. Rare Met Mater Eng, 2002; 31: 358 (金云学,曾松岩,王宏伟.稀有金属材料与工程,2002;31: 358) [4] Chen L H, Blenkinsop P A, Jones I P. Mater Sci Technol, 2001; 17: 573 [5] Li Y G, Blenkinsop P A, Loretto M H, Rugg D, Voice W. Acta Mater, 1999; 47: 2889 [6] Li Y G, Loretto M H, Rugg D, Voice W. Ada Mater, 2001; 49: 3011 [7] Haasen P. Phase Transformations in Materials.Weinheim, Germany: VCH Verlagsgesellschaft mbH, 1991: 245 [8] Cam G, Flower H M, West D R F. Mater Sci Technol, 1991; 7: 505 [9] Aaron H B, Kolter G R. Metall Trans, 1971; 2: 393 [10] Hewitt P, Butler E P. Acta Metall, 1984; 34: 1163 [11] Zhang S Z, Li G P, Wang Q J, Liu Y Y, Yang R. Mater Sci Technol, 2004; 20: 167 [12] Murry J L. Binary Alloy Phase Diagrams. Materials Park, Ohio: ASM International, 1986: 593 [13] Villars P, Prince A, Okamoto H. Handbook of Ternary Phase Diagrams. Materials Park, Ohio: ASM International, 1997: 2906 [14] Gundel D B, Wawner F E. Scr Metall Mater,1991;25: 437 |
|