| 双相不锈钢中表面浮凸的测量与表征 |
| 邱 冬 张文征 |
| 清华大学材料科学与工程系;北京 100084 |
|
| MEASUREMENT AND CHARACTERIZATION OF THE SURFACE RELIEF IN A DUPLEX STAINLESS STEEL |
| QIU Dong; ZHANG Wenzheng |
| Department of Materials Science and Engineering; Tsinghua University;Beijing 100084 |
引用本文:
邱冬; 张文征 . 双相不锈钢中表面浮凸的测量与表征[J]. 金属学报, 2005, 41(9): 897-904 .
,
.
MEASUREMENT AND CHARACTERIZATION OF THE SURFACE RELIEF IN A DUPLEX STAINLESS STEEL[J]. Acta Metall Sin, 2005, 41(9): 897-904 .
[1] Bain E C. Trans AIME, 1924; 70: 25 [2] Wechsler M S, Lieberman D S, Read T A. Trans AIME, 1953; 197: 1503 [3] Bowles J S, Mackenzie J K. Acta Metall, 1954; 2: 129, 138, 224 [4] Aaronson H I, Laird C, Kinsman K R. Phase Transformations. Metals Park, OH: ASM, 1970: 59 [5] Ko T, Cottrell S A. J Iron Steel Inst, 1952; 172: 307 [6] Tsuya K. J Mech Lab, 1956; 2: 20 [7] Speich G R. In: Aaronson H I ed., Decomposition of Austenite by Diffusional Process, New York: Interscience, 1962: 361 [8] Garwood R D. Special Report No.93, London: Iron and Steel Institute, 1965: 90 [9] Flewitt P E J, Towner J M. J Inst Met, 1967; 95: 273 [10] Smith R, Bowles J S. Acta Metall, 1960; 8: 405 [11] Pawel T E, Cathcart J V, Campbell J J. Acta Metall, 1962; 10: 149 [12] Hall M G, Aaronson H I, Lorimer G W. Scr Metall, 1975; 9: 533 [13] Ohmori Y, Nakai K, Ohtsubo H, Isshiki Y. ISIJ Int, 1995; 35: 969 [14] Lee H J, Aaronson H I. Acta Metall, 1988; 36: 787 [15] Guo H, Enomoto M. Acta Mater, 2002; 50: 929 [16] Zhang W Z. Philos Mag, 1998; 78A: 913 [17] Zhang W Z, Weatherly G C. Acta Mater, 1998; 46: 1837 [18] Efsic E J, Wayman C M. Trans TMS-AIME, 1967; 239: 873 [19] Muddle B C, Krauklis P, Bowles J S. Acta Metall, 1976; 24: 371 [20] Dunne D P, Wayman C M. Acta Metall, 1970; 18: 981 [21] Yamamoto M, Pujuisawa T, Saburi T. Ultramicroscopy, 1992; 42: 1422 [22] Yamamoto M, Pujuisawa T, Saburi T, Kussao K. Surf Sci, 1992; 266: 289 [23] Yamamoto M, Nishikawa K, Noda Y, Saburi T, Hayakawa M, Oka M, Kurumi-zawa T. J Vac Sci Technol, 1994; 12B: 1813 [24] Yang Z G, Fang H S, Wang J J, Li C M, Zheng Y K. Phys Rev, 1995; 52B: 7879 [25] Waitz T, Karnthaler H P. Acta Mater, 1997; 45: 837 [26] Deville S, Guenin G, Chevalier K. Acta Mater, 2004; 52: 5697 [27] Guo H, Okuda K, Enomoto M. Metall Mater Trans, 2000; 31A: 599 [28] Ameyama K, Weatherly G C, Aust K T. Acta Metall Mater, 1992; 40: 1835 [29] Luo Y H. Master's Dissertation, South China University of Technology, Guangzhou, 1992 (罗英辉.华南理工大学硕士学位论文,广州, 1992) [30] Zhang W Z, Purdy G R. Philos Mag, 1993; 68A: 291 [31] Qiu D, Zhang W Z. Philos Mag, 2003; 83: 3093 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|