| 利用纳米压痕加载曲线计算硬度--压入深度关系及弹性模量 |
| 谭孟曦 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室; 沈阳 110016 |
|
引用本文:
谭孟曦 . 利用纳米压痕加载曲线计算硬度--压入深度关系及弹性模量[J]. 金属学报, 2005, 41(10): 1020-1024 .
[1] Oliver W C, Pharr GM. J Mater Res, 1992; 7: 1564 [2] Oliver W C, Pharr G M. J Mater Res, 2004; 19: 3 [3] Poole W J, Ashby M F, Fleck N A. Scr Mater, 1996; 34:559 [4] Nix W D, Gao H. J Mech Phys Solids, 1998; 46: 411 [5] Swadener J G, George E P, Pharr G M. J Mech Phys Solids, 2002; 50: 681 [6] Li X D, Bhushan B. Mater Charact, 2002; 48: 11 [7] Men H, Hu Z Q, Xu J. Scr Mater, 2002; 46: 699 [B1] Malzbender J, de With G, den Toonder J. J Mater Res, 2000;15:1209 |
|