| 定向凝固铁磁形状记忆合金Ni2MnGa的固-液界面形态 |
| 蒋成保 刘敬华 张涛 徐惠彬 |
| 北京航空航天大学材料学院; 北京100083 |
|
| The Solid-Liquid Interface Morphology of the Unidirectionally Solidified Ni2MnGa Magnetic Shape Memory Alloy |
| JIANG Chengbao; LIU Jinghua; ZHANG Tao; XU Huibin |
| School of Materials Science and Engineering; Beijing University of Aeronautics and Astronautics; Beijing 100083 |
引用本文:
蒋成保; 刘敬华; 张涛; 徐惠彬 . 定向凝固铁磁形状记忆合金Ni2MnGa的固-液界面形态[J]. 金属学报, 2004, 40(9): 975-980 .
,
,
,
.
The Solid-Liquid Interface Morphology of the Unidirectionally Solidified Ni2MnGa Magnetic Shape Memory Alloy[J]. Acta Metall Sin, 2004, 40(9): 975-980 .
[1] O'Handley R C. Appl Phys, 1998; 83: 3263 [2] Wu G H, Yu C H, Meng L Q, Chen J L, Yang F M, Qi S R, Zhan W S, Wang Z, Zheng Y F, Zhao L C. Appl PhysLett, 1999; 75: 2990 [3] Jiang C B, Liang T, Xu H B, Zhang M, Wu G H. ApplPhys Lett, 2002; 81: 1818 [4] Murray S J, Marioni M, Allen S M, O'Handley R C. ApplPhys Lett, 2000; 77: 886 [5] Sozinov A, Likhachev A A, Lanska N, Ullakko K. ApplPhys Lett, 2002; 80: 1746 [6] Schlagel D L, Wu Y L, Zhang W, Lograsso T A. J AlloysCompds, 2000; 312: 77 [7] Pons J, Chernenko V A, Sautamarta R, Cesari E. ActaMater, 2000; 48: 3027 [8] Jiang C B, Feng G, Xu H B. Appl Phys Lett, 2002; 80:1619 [9] Albertini F, Pareti L, Paoluzi A, Morellon L, Algarabel PA, Ibarra M R, Righi L. Appl Phys Lett, 2002; 81: 4032 [10] Straka L, Heczko O, Lanska N. IEEE Trans Magn, 2002;38: 2835 [11] Jiang C B, Muhammad Y, Deng L F, Wu W, Xu H B.Acta Mater, 2004; 52: 2779 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|