| 孪晶对多晶铜疲劳行为的影响 |
| 郭小龙;申勇峰;卢磊;李守新 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室; 沈阳 110016 |
|
| EFFECTS OF TWINS ON THE FATIGUE BEHAVIOR OFPOLYCRYSTALLINE COPPER |
| GUO Xiaolong; SHEN Yongfeng; LU Lei; LI Shouxin |
| Shenyang National Laboratory for Materials Science; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
郭小龙; 申勇峰; 卢磊; 李守新 . 孪晶对多晶铜疲劳行为的影响[J]. 金属学报, 2004, 40(12): 1281-1284 .
,
,
,
.
EFFECTS OF TWINS ON THE FATIGUE BEHAVIOR OFPOLYCRYSTALLINE COPPER[J]. Acta Metall Sin, 2004, 40(12): 1281-1284 .
[1] Burgers W G, Meijs J C, Tiedema T J. Acta Metall, 1953;1: 75 [2] Dash S, Brown N. Acta Metall, 1963; 11: 1067 [3] Meyers M A, Murr L E. Acta Metall, 1978; 26: 951 [4] Thompson A W. Metallography, 1972; 1: 366 [5] Mughrabi H. Mater Sci Eng, 1978; 33: 207 [6] Yamakov V, Wolf D, Phillpot S R, Gleiter H. Acta Mater,2002; 50: 5005 [7] Yamakov V, Wolf D, Phillpot S R, Gleiter H. Acta Mater,2003; 51: 4135 [8] Murr L E, Horylev R J, Lin W N. Philos Mag, 1970; 22:515 [9] Llanes L, Laird C. Mater Sci Eng, 1992; A157: 21 [10] Kawazoe H, Yoshida M, Basinski Z S, Niewczas M. ScrMater, 1999; 40: 639 |
|