| 连铸连轧非调质钢的强度计算及其预报 |
| 刘志林;刘伟东;林 成 |
| 辽宁工学院材料与化学工程学院; 锦州 121001 |
|
| STRENGTH CALCULATION AND ITS PREDICTION OF NON QUENCHED-TEMPERED STEEL DURING CONTINUOUS CASTING-ROLLING |
| LIU Zhilin; LIU Weidong; LIN Cheng |
| Department of Materials and Chemical Engineering; Liaoning Institute of Technology; Jinzhou 121001 |
引用本文:
刘志林; 刘伟东; 林成 . 连铸连轧非调质钢的强度计算及其预报[J]. 金属学报, 2004, 40(12): 1248-1252 .
,
,
.
STRENGTH CALCULATION AND ITS PREDICTION OF NON QUENCHED-TEMPERED STEEL DURING CONTINUOUS CASTING-ROLLING[J]. Acta Metall Sin, 2004, 40(12): 1248-1252 .
[1] Yu R H. Chin Sci Bull, 1978; 23: 217 (余瑞璜.科学通报,1978;23:217) [2] Zhang R L. Empirical Electron Theory of Solid andMolecules.Changchun:Jilin Science and TechnologyPublishing House, 1993: 231 (张瑞林.固体与分子经验电子理论.长春:吉林科学技术出版 社,1993:231) [3] Cheng K J, Cheng S Y. Mater Sci Eng, 1998; 16(1):1 (程开甲,程漱玉.材料科学与工程, 1998;16(1):1) [4] Liu Z L, Dai T S, Yang S L, Zhang B G. Sci Chin, 1989; 32A: 1390 [5] Liu Z L. The Valence Electron Structures and Composition Design in Alloys. 2nd ed., Changchun: Jilin Science and Technology Publishing House, 2002: 15 (刘志林.合金价电子结构与成分设计.第2版,长春:吉林科 学技术出版社,2002:15) [6] Liu Z L, Li Z L, Liu W D. Interface Electron Structure and Interface Property. Beijing: Science Press, 2002: 30 (刘志林,李志林,刘伟东,界面电子结构与界面性能.北京: 科学出版社,2002:30) [7] Liu Z L, Li Z L, Liu W D. Sci Chin, 2001; 44E:542 [8] Liu Z L, Li Z L, Sun Z G. Chin Sci Bull, 1996; 41: 367 [9] Liu Z L, Sun Z G, Li Z. Prog Nat Sci, 1998; 8:134 [10] Liu G X. Principle of Metallurgy. Beijing: MetallurgicalIndustry Press, 1983: 137 (刘国勋.金属学原理.北京:冶金工业出版社,1983:137) [11] Cui Z Q. Metallurgy and Heat Treatment. Beijing: ChinaMachine Press, 1992: 112 (崔忠圻.金属学与热处理.北京:机械工业出版社,1992:112)R |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|