| 合金凝固过程的形核模型 |
| 陈忠伟 介万奇 |
| 西北工业大学凝固技术国家重点实验室; 西安 710072 |
|
| Nucleation Model in Solidification Processes of the Alloys |
| CHEN Zhongwei; JIE Wanqi |
| State Key Laboratory of Solidification Processing; Northwestern Polytechnical University; Xi'an 710072 |
引用本文:
陈忠伟; 介万奇 . 合金凝固过程的形核模型[J]. 金属学报, 2004, 40(10): 1027-1031 .
,
.
Nucleation Model in Solidification Processes of the Alloys[J]. Acta Metall Sin, 2004, 40(10): 1027-1031 .
[1] Turnbull D. J Appl Phys, 1950; 21: 1022 [2] Turnbull D. J Chem Phys, 1950; 18: 198 [3] Maxwell I, Hellawell A. Acta Metall, 1975; 23(2) : 229 [4] Wei B B, Yang G C, Zhou Y H. Ada Mater, 1991; 39:1249 [5] Turbull D, Cech R E. J Appl Phys, 1950; 21: 804 [6] Jian Z Y, Chang F E, Ma W H. Sci Chin, 2000; 43E(2) :113 [7] Thompson C V, Spaepen F. Ada Metall, 1983; 31: 2021 [8] Zhang X Z. Ada Mater, 1998; 46: 1135 [9] Uolland-Moritz D, Schroess J, Herlach D M. Ada Mater,1998; 46: 1601 [10] Rappaz M, Gandin C A. Ada Metall Mater, 1993; 41(2) : 345 [11] Thevoz Ph, Desbiolles J L, Rappaz M. Metall Mater TransA, 1989; 20A: 311 [12] Christian J W. The Theory of Transformation in Metalsand Alloys. Pergamon, Oxford, 1975: 418 [13] Turnbull D. In: Seitz F, Turbull D eds, Solid StatePhysics. New York: Academic Press, 1956: 225 [14] Spaepen F, Turnbull D. In: Grant N J, Giessen B C eds,Proc 2nd Int Conf On Rapidly Quenched Metals. Cambridge: MIT Press, 1976: 205 [15] Spaaepen F. Acta Metall, 1975; 23: 729 [16] Spaepen F, Meyer R B. Scr Metall, 1976; 10(1) : 37 [17] Turnbull D. Contemporary Phys, 1969; 10: 473 [18] Mueller B A, Perepezko J H. Metall Mater Trans A, 1987;18A: 1143 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|