| 稀土对B319铝合金组织性能的影响 |
| 吴国华 马春江 王叶双 朱燕萍 丁文江 |
| 上海交通大学金属基复合材料国家重点实验室;上海200030 |
|
引用本文:
吴国华; 马春江; 王叶双; 朱燕萍; 丁文江 . 稀土对B319铝合金组织性能的影响[J]. 金属学报, 2002, 38(7): 703-708 .
[1] Sun Y, Tsai H L. AFS Trans, 1996; 92: 271 [2] Lawrence M D, Ramsay C W. AFS Trons, 1998; 112: 349 [3] Hill M, Vrieze A E. AFS Trans, 1998; 114: 365 [4] Warner M H, Miller B A. AFS Trans, 1998; 161: 777 [5] Kumar P, Gaindhar J L. AFS Trans, 1996; 159: 1143 [6] Wu G H, Luo J R. Foundry, 2000; (3): 134(吴国华,罗吉荣.铸造,2000;(3):134) [7] Wu G H, Luo J R, Xie M. Trans Nonferrous Met SocChin, 2000; 10(5): 645 [8] Wu G H. Ph.D thesis, Study on the Pinhole of AluminumAlloy in Lost Foam Casting. Wuhan: Material School,Huazhong University of Science and Technology,2000(吴国华.消失模铸造铝合金针孔研究.华中理工大学材料学院博士学位论文,2000年) [9] Tang D G. Special Casting Nonferrous Alloy. 1999; (5):42(唐多光.特种铸造及有色合金,1999;(5):42) [10] Kubschewski O, Alcock C B. Metallurgical thermochem-istry. UK: Pergamor Press, 1979: 326 [11] Lu S Z, Hellawell A. Metall trans A, 1987; 18(10): 1721 [12] Guo J Q, Li Q C. J Chin Rare Earth Soc. 1988; 6(2): 51(郭俊清,李庆春.中国稀土学报,1988;6(2):51) [13] Li H J, Li G H, Tan H X. J Chin Rare Earth Soc, 1998;16(3): 234(李华基,李革胜,谭会辛.中国稀土学报,1998;16(3):234) [14] Du W X, Dang P, Jiang Q. J Chin Rare Earth Soc1988;6(3): 59(杜维玺,党 平,蒋 青.中国稀土学报,1988;6(3):59) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|