AZ91 Mg-Al合金中γ-Mg17Al12析出相的多重位向关系及{112}γ伪孪晶关系 |
罗承萍 肖晓玲 刘江文 聂建峰 B.C.Muddle |
华南理工大学机械工程学院;广州510641 |
|
引用本文:
罗承萍; 肖晓玲; 刘江文; 聂建峰; B.C.Muddle . AZ91 Mg-Al合金中γ-Mg17Al12析出相的多重位向关系及{112}γ伪孪晶关系[J]. 金属学报, 2002, 38(7): 709-714 .
[1] Clark J B. Acta Metall, 1968; 16: 141 [2] Clark J B. Acta Metall, 1965; 13: 1281 [3] Crawley A F, Milliken K S. Acta Metall, 1974; 22: 557 [4] Crawley A F, Lagowski B. Metall Trans, 1974; 5: 949 [5] G(?)jnnes, Ostmoe T. Metkd Z, 1970; 31: 604 [6] Duly D, Simon J P, Brechet Y Y. Acta Metall Mater, 1995;43(1): 101 [7] Celotto S. Acta Metall, 2000; 48: 1775 [8] Xiao X L, Luo C P, Nie J F, Muddle B C. Acta MetallSin. 2001: 37: 1(肖晓玲,罗承萍,聂建峰,B C Muddle.金属学报,2000;37:1) [9] Luo C P, Xu L K, Cha J Z. Acta Metall Sin, 1993; 29:A312(罗承萍,许麟康,查健中.金属学报,1993;29:A312) [10] Douin J, Dahmen U, Westmacott K H, Philos Mag, 1991;B63: 867 |
|